Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.872 g/cc | 0.0315 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Polidan® PNT 0856/35 Polyethylene, Crosslinked (XLPE) POLIDAN® PNT 0856/35 is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction.Features: Crosslinkable; Good Flexibility; Lo.. |
|||
Density | 0.872 g/cc | 0.0315 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Polidiemme® G/450 Thermoset Elastomer (TSE) Polidiemme® XLPO -Cross-linkable Polyolefin. Elastomer based compound crosslinkable by ambient moisture, consisting of a silane pregrafted base compound to be used with a catalyst masterbatch (S.. |
|||
Density | 0.872 - 0.882 g/cc | 0.0315 - 0.0319 lb/in³ | RPC-11002 |
Solvay DURAPHOS® TLP Tri lauryl phosphite Chemical Name: TRIALKYL PHOSPHITECAS: 68610-62-8; 108-95-2 Available in: Asia Pacific, Europe, Latin America and North AmericaWater Solubility: Practically Insoluble Applications: DURAPHOS® TLP i.. |
|||
Density | 0.872 g/cc @Temperature 15.0 °C |
0.0315 lb/in³ @Temperature 59.0 °F |
|
ExxonMobil Mobil 1 10W-40 Motorcycle Oil MX4T 4-Cycle Mobil 1 Motorcycle Oils are formulated with 100 percent synthetic fluids. The unique, synthetic structure of the Mobil 1 Motorcycle formulations enable them to offer advantages well beyond conventio.. |
|||
Density | 0.872 g/cc @Temperature 15.0 °C |
0.0315 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil SAE 40 Mobilgard 1 SHC Mobilgard 1 SHC by ExxonMobil is a supreme performance, synthetic diesel engine oil specifically formulated to address the needs of high power, distillate fueled diesel engines. It provides lubricat.. |
|||
Density | 0.872 g/cc @Temperature 15.0 °C |
0.0315 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil Nuto 32 H Series Exxon Nuto H Series oils are premium quality anti-wear hydraulic oils intended for industrial and mobile service applications where anti-wear lubricants are required. They are formulated with high q.. |
|||
Density | 0.872 g/cc @Temperature 15.0 °C |
0.0315 lb/in³ @Temperature 59.0 °F |
|
ExxonMobil Mobil 1 10W-40 Motorcycle Oil MX4T 4-Cycle Mobil 1 Motorcycle Oils are formulated with 100 percent synthetic fluids. The unique, synthetic structure of the Mobil 1 Motorcycle formulations enable them to offer advantages well beyond conventio.. |
|||
Density | 0.872 g/cc @Temperature 15.0 °C |
0.0315 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil Nuto 32 H Series Exxon Nuto H Series oils are premium quality anti-wear hydraulic oils intended for industrial and mobile service applications where anti-wear lubricants are required. They are formulated with high q.. |
|||
Density | 0.872 g/cc @Temperature 15.0 °C |
0.0315 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil SAE 40 Mobilgard 1 SHC Mobilgard 1 SHC by ExxonMobil is a supreme performance, synthetic diesel engine oil specifically formulated to address the needs of high power, distillate fueled diesel engines. It provides lubricat.. |
|||
Density | 0.872 g/cc | 0.0315 lb/in³ | |
ConocoPhillips Hydroclear® El Mar® Low Ash Heavy Duty SAE 40 Description: Conoco Hydroclear El Mar Low Ash Heavy Duty is a high-quality low ash natural gas engine oil formulated from exclusive Conoco hydrocracked base stock. Hydroclear El Mar Low Ash Heavy Du.. |
|||
Density | 0.872 g/cc | 0.0315 lb/in³ | |
ConocoPhillips Hydroclear® MV68 AW Hydraulic Fluid Description: Conoco Hydroclear AW Hydraulic Fluid is specifically designed for use in high-pressure systems which require greater wear protection and deposit control than that provided by standard a.. |
|||
Density | 0.872 g/cc @Temperature 15.6 °C |
0.0315 lb/in³ @Temperature 60.0 °F |
|
ConocoPhillips Transformer Oil Description: Conoco Transformer Oil, an insulating oil of very high dielectric strength, is suited for oil-filled transformers in both large substations and small pole-mounted transformers. It is al.. |
|||
Density | 0.872 g/cc | 0.0315 lb/in³ | |
ConocoPhillips Hydroclear® 100 Turbine Oil Description: Conoco Hydroclear Turbine Oil is a premium rust- and oxidationinhibited turbine oil formulated from exclusive Conoco hydrocracked base stock. Hydroclear Turbine Oil is specially formula.. |
|||
Density | 0.872 g/cc @Temperature 15.6 °C |
0.0315 lb/in³ @Temperature 60.0 °F |
|
ConocoPhillips Hydroclear® XHP 2-Cycle Engine Oil Description: Conoco Hydroclear XHP 2-Cycle Engine Oil is made with an advanced, high-stability base oil and highly effective additives. This unique combination allows the product to meet full NMMA T.. |
|||
Density | 0.872 g/cc | 0.0315 lb/in³ | |
BASF 3-Methoxypropylamine (MOPA) Formula: C4H11NOCAS: 5332-73-0Description: 3-Methoxypropylamine (MOPA) is a colorless to yellow liquid with an aminelike odor. It is miscible in water.Synonyms: 3-Aminopropyl methyl ether, 3-Methox.. |
|||
Density | 0.872 g/cc @Temperature 0.000 °C |
0.0315 lb/in³ @Temperature 32.0 °F |
|
BorsodChem ONGRONOX EHP 50 D peroxide-type initiator Chemical name: Bis-(2-ethylhexyl)-peroxi-dicarbonate. Mol. wt: 346.5g/mol. Active oxygen content: 4.62 %. Deflegmation material: isododecane. Major decomposition products: carbon-dioxide, 2-ethyl-he.. |
|||
Density | 0.872 - 1.47 g/cc | 0.0315 - 0.0531 lb/in³ | Average value: 0.959 g/cc Grade Count:27 |
Overview of materials for High Density Polyethylene (HDPE), Crosslinkable This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Crosslinkable". Each property range of values reported is minimum and .. |
|||
Density | 0.872 - 1.23 g/cc | 0.0315 - 0.0444 lb/in³ | Average value: 1.02 g/cc Grade Count:19 |
Overview of materials for Polypropylene, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Carbon Fiber 10%". Each property range of values reported is minimum and maximum values o.. |