Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon A3020-R004-12 0.020" (0.508 mm) Cured Fusible Silicone Rubber with Sinusoidal Fiberglass Substrate  

Category Polymer , Thermoset , Silicone , Silicone Rubber , Silicone, Molded, Glass Fiber Filled
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon A3020-R004-12 0.020" (0.508 mm) Cured Fusible Silicone Rubber with Sinusoidal Fiberglass Substrate  .pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
1 inch width and 36 inches long. Design/Construction: Side 1: Cured Fusible Silicone Rubber Substrate: 25% sinusoidal FiberglassSide 2: Cured Fusible Silicone Rubber Interleave: Polyester Film Product Advatages:Flexibility: Silicone rubber resists damage due to vibration, frame movement under load and thermal expansion/contraction in use. Silicone based insulation remains flexible even after many years in extreme service conditions.Thermal Stability: Silicone based insulation remains flexible and resilient to thermal shock, even after years of cold motor starts as low as -54°C and running conditions up to 260°C.Electrical Insulation: Silicone based insulation has excellent dielectric strength, dielectric integrity over a wide temperature range, and resists arc tracking, current leakage, corona damage, and dielectric fatigue.Ozone and Weather Resistance: Unique silicone chemistry resists oxidative embrittlement, damage by ozone and other atmospheric chemicals, and seals against moisture, carbon dust, dirt, and debris.This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 25.4 microns
1.00 mil
Interleave
203 microns
8.00 mil
Substrate; Arlon SQA-TMS-003
508 microns
20.0 mil
Overall; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 55
55
Silicone Property; ASTM D2240
Tensile Strength 7.93 MPa
1150 psi
Silicone Property; ASTM D412
23.1 MPa
3350 psi
Product Property; Arlon SQA-TMS-048
Elongation at Break 25 %
25 %
Tape Property; Arlon SQA-TMS-048
430 %
430 %
Silicone Property; ASTM D412
Tear Strength 15.8 kN/m
90.0 pli
Die B, Silicone Property; ASTM D624
Peel Strength 0.929 kN/m
5.30 pli
Adhesion Strength, Tape Property; Arlon SQA-TMS-047
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Electrical Properties Metric English Comments
Dielectric Strength 26.3 kV/mm
668 kV/in
Tape Property; ASTM D149
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature 21.1 °C
12.0 Month

@Temperature 70.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Red
White
Substrate