Mechanical Properties Metric English Comments
Flexural Modulus 2.20 - 2.60 GPa
319 - 377 ksi
ASTM D790-04
Proto3000 Objet Digital Materials™ DM_7220 Transparent Prototyping Polymer
Primary material: FullCure720Secondary material: TangoBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide ..
Flexural Modulus 1.90 - 2.60 GPa
276 - 377 ksi
Average value: 2.46 GPa Grade Count:4
Overview of materials for Polyphthalamide (PPA), High Impact
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, High Impact". Each property range of values reported is minimum and maximum values of a..
Flexural Modulus 2.40 - 2.60 GPa
348 - 377 ksi
ASTM D790
Loxim 830 02T HB Polypropylene Compound, 30% Talc Filled, Flame Retardant
Information provided by Loxim Industries
Flexural Modulus 0.167 - 2.60 GPa

@Temperature -40.0 - 100 °C
24.2 - 377 ksi

@Temperature -40.0 - 212 °F
Average value: 1.38 GPa Grade Count:1
Overview of materials for High Density Polyethylene (HDPE), Crosslinkable
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Crosslinkable". Each property range of values reported is minimum and ..