Polymer Property : Head Temperature = 200 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Head Temperature 200 - 210 °C
392 - 410 °F
Silon Taborex TA 1109 MD Chemically-Crosslinkable MDPE Compound
TABOREX TA 1110 MD is a crosslinkable compound made by a Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOP..
Head Temperature 200 - 210 °C
392 - 410 °F
Silon Taborex TA 1117HD Chemically-Crosslinkable HDPE Compound
TABOREX TA 1117 HD is a crosslinkable compound made by Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA..
Head Temperature 200 - 210 °C
392 - 410 °F
Silon Taborex TA 1131 HD Chemically-Crosslinkable HDPE Compound
TABOREX TA 1131 HD is a crosslinkable compound made by Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA..
Head Temperature 200 - 210 °C
392 - 410 °F
Silon Taborex TA 1132 HD Chemically-Crosslinkable HDPE Compound
TABOREX TA 1132 HD is a crosslinkable compound made of Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA..
Head Temperature 200 - 210 °C
392 - 410 °F
Silon Taborex TA 1133 HD Chemically-Crosslinkable HDPE Compound
TABOREX TA 1133 HD is a crosslinkable compound made of Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA..
Head Temperature 200 - 210 °C
392 - 410 °F
Silon Taborex TA 1134 HD Chemically-Crosslinkable HDPE Compound
TABOREX TA 1134 HD is a crosslinkable compound made of Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA..
Head Temperature 200 - 210 °C
392 - 410 °F
Silon Taborex TA 1135 HD Chemically-Crosslinkable HDPE Compound
TABOREX TA 1135 HD is a crosslinkable compound made by Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA..
Head Temperature 200 - 210 °C
392 - 410 °F
Silon Taborex TA 1108 HD Chemically-Crosslinkable HDPE Compound
TABOREX TA 1108 HD is a crosslinkable compound according to the “SIOPLAS-SYSTEM”; made by a Silane grafted ethylene copolymer known as the graft and a Masterbatch containing the crosslinki..
Head Temperature 200 - 230 °C
392 - 446 °F
Borealis BB412E Polypropylene Block Copolymer for extrusion and injection
BB412E is a natural, medium molecular weight, medium melt flow rate polypropylene block copolymer with an optimal mechanical properties balance resulting in high stiffness and very good impact stren..
Head Temperature 200 - 230 °C
392 - 446 °F
Borealis BE50-7032 Polypropylene Homopolymer for Non-Pressure pipes and extruded sheets
BE50-7032 is a high molecular weight, low melt flow rate polypropylene homopolymer characterized by high stiffness, high heat distortion temperature and high resistance to thermal aging. The materia..
Head Temperature 200 - 230 °C
392 - 446 °F
Borealis BEC5012 Polypropylene Block Copolymer for Non-Pressure Pipes
BEC5012 is a high molecular weight, low flow rate polypropylene block copolymer with very high impact strength. Applications: BEC5012 is recommended for non-pressure pipes and fittings, structured..
Head Temperature 200 - 230 °C
392 - 446 °F
Borealis Beta (ß)-PP™ BE60-7032 Grey Polypropylene Homopolymer for Pressure Pipes, Fittings and Sheets
Beta(ß)-PP BE60-7032 is a high molecular weight, low melt flow rate polypropylene homopolymer with fine grained ß-modification crystalline structure leading to excellent impact strength even at lo..
Head Temperature 200 - 210 °C
392 - 410 °F
Borealis BorSafe™ HE3494-LS-H HDPE Compound for Pressure Pipes
BorSafe™ HE3494-LS-H is a bimodal polyethylene compound produced by the advanced Borstar® technology. It includes a combination of pigments and stabilizers to ensure excellent long-term thermal s..
Head Temperature 200 - 210 °C
392 - 410 °F
Borealis BorSafe™ ME3420 MDPE Compound for Pressure Pipes
BorSafe™ ME3420 is a bimodal polyethylene compound produced by the advanced Borstar® technology. Well dispersed carbon black gives outstanding UV resistance. Long term stability is ensured by an ..
Head Temperature 200 - 210 °C
392 - 410 °F
Borealis Borstar® HE3410 HDPE for Sewage Pipes
Borstar® HE3410 is a bimodal polyethylene compound produced by the advanced Borstar® technology. Well dispersed carbon black gives outstanding UV resistance. Long term stability is ensured by an ..
Head Temperature 200 - 210 °C
392 - 410 °F
Borealis Borstar® HE3470-LS Black HDPE Compound for Pressure Pipes
Borstar HE3470-LS is a black, high density polyethylene compound classified as an MRS 8.0 material (PE80) produced by the advanced Borstar technology. Well dispersed carbon black gives outstanding ..
Head Temperature 200 - 210 °C
392 - 410 °F
Borealis Borstar® HE3494-LS Dark Blue High Density Polyethylene for Drinking Water Pipes
Borstar HE3494-LS is a yellow-orange, cadmium free, high density polyethylene compound classified as a MRS 10.0 material (PE100) produced with the advanced Borstar technology. It includes a combina..
Head Temperature 200 - 210 °C
392 - 410 °F
Borealis Borstar® ME3440 Black Medium Density Polyethylene for Pressure Pipes
Borstar ME3440 is a black, bimodal medium density polyethylene compound classified as a MRS 8.0 material (PE80), with optimum balance between flexibility and strength, produced with the advanced Bor..
Head Temperature 200 - 210 °C
392 - 410 °F
Borealis Borstar® ME3441 Yellow Medium Density Polyethylene for Natural Gas Pipes
Borstar ME3441 is a yellow, bimodal, cadmium free, medium density polyethylene compound classified as a MRS 8.0 material (PE80) produced with the advanced Borstar technology. It includes a combinat..
Head Temperature 200 - 230 °C
392 - 446 °F
Borealis HA104E Polypropylene Homopolymer
HA104E is a natural high molecular weight, high melt flow rate polypropylene homopolymer characterized by well-balanced stiffness to impact strength ratio at increased processing properties. Applica..
Head Temperature 200 - 210 °C
392 - 410 °F
Borealis BorSafe™ HE3490-LS-H HDPE Compound for Pressure Pipes
BorSafe™ HE3490-LS-H is a bimodal polyethylene compound produced by the advanced Borstar® technology. It includes a combination of pigments and stabilizers to ensure excellent long-term thermal s..
Head Temperature 200 - 210 °C
392 - 410 °F
Borealis Borstar® HE3492-LS Yellow-Orange High Density Polyethylene for Natural Gas Pipes
Borstar HE3492-LS is a yellow-orange, cadmium free, high density polyethylene compound classified as a MRS 10.0 material (PE100) produced with the advanced Borstar technology. It includes a combina..
Head Temperature 200 - 210 °C
392 - 410 °F
Average value: 205 °C Grade Count:6
Overview of materials for High Density Polyethylene (HDPE), Pipe Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Pipe Grade". Each property range of values reported is minimum and max..
Head Temperature 200 - 210 °C
392 - 410 °F
Average value: 204 °C Grade Count:9
Overview of materials for High Density Polyethylene (HDPE), Crosslinkable
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Crosslinkable". Each property range of values reported is minimum and ..
Head Temperature 200 - 210 °C
392 - 410 °F
Borealis Borstar® HE3490-LS Black High Density Polyethylene for Pressure Pipes
Borstar HE3490-LS is a black, bimodal, high density polyethylene classified as an MRS 10.0 material (PE100) produced by the advanced Borstar technology. Well dispersed carbon black gives outstanding..
Head Temperature 200 - 210 °C
392 - 410 °F
Borealis Borstar® ME3444 Blue Medium Density Polyethylene for Drinking Water Pipes
Borstar 3444 is a blue, bimodal, medium density polyethylene classified as a MRS 8.0 material (PE80) produced with the advanced Borstar technology. A combination of pigments and stabilizers is incl..