Mechanical Properties Metric English Comments
Modulus of Elasticity 2.03 - 3.30 GPa
294 - 479 ksi
Average value: 2.64 GPa Grade Count:50
Overview of materials for PVC, High Impact
This property data is a summary of similar materials in the MatWeb database for the category "PVC, High Impact". Each property range of values reported is minimum and maximum values of appropriate M..
Modulus of Elasticity 1.40 - 3.30 GPa
203 - 479 ksi
Average value: 2.46 GPa Grade Count:26
Overview of materials for Polypropylene with 40% Calcium Carbonate (CaCO3) Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be..
Modulus of Elasticity 0.100 - 3.30 GPa
14.5 - 479 ksi
Average value: 1.75 GPa Grade Count:25
Overview of materials for Nylon 6, Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Film Grade". Each property range of values reported is minimum and maximum values of appropriat..
Modulus of Elasticity 0.0000689 - 3.30 GPa
0.0100 - 479 ksi
Average value: 2.45 GPa Grade Count:19
Overview of materials for Acetal Homopolymer, PTFE-Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, PTFE-Filled". Each property range of values reported is minimum and maximum values o..
Modulus of Elasticity 1.80 - 3.30 GPa
261 - 479 ksi
Average value: 2.96 GPa Grade Count:19
Overview of materials for Acrylic, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Extruded". Each property range of values reported is minimum and maximum values of appropriate ..
Modulus of Elasticity 2.80 - 3.30 GPa
406 - 479 ksi
Average value: 3.17 GPa Grade Count:4
Overview of materials for Acrylic, Cast
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW..
Modulus of Elasticity 0.130 - 3.30 GPa

@Temperature -40.0 - 100 °C
18.9 - 479 ksi

@Temperature -40.0 - 212 °F
Average value: 1.72 GPa Grade Count:1
Overview of materials for High Density Polyethylene (HDPE), Crosslinkable
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Crosslinkable". Each property range of values reported is minimum and ..
Modulus of Elasticity 0.145 - 3.30 GPa

@Temperature -40.0 - 150 °C
21.0 - 479 ksi

@Temperature -40.0 - 302 °F
Average value: 0.997 GPa Grade Count:8
Overview of materials for Nylon 6, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Impact Grade". Each property range of values reported is minimum and maximum values of appropri..
Copyright © lookpolymers.com All Rights Reserved