Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

EMS-Grivory Grivory® TSK-30/4 PA666-GB30

Category Polymer , Thermoplastic , Nylon , Nylon 6/66 , Nylon 66/6, 30% Glass Fiber Reinforced
Manufacturer EMS-Grivory (EMS-CHEMIE)
Trade Name Grivory®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Grivory Grivory® TSK-30/4 PA666-GB30.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product description: Grilon TSK-30/4 is a heat stabilized, normal viscosity PA66 +PA6 injection molding grade with 30% glass beads. Grilon TSK-30/4 has the following important properties: Good surface finishHigh abrasion resistanceLow warpage Grilon TSK-30/4 is used typically for low warpage applications such as air ducts, belt pulleys, and housing components.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
ISO 1183
Water Absorption 5.0 %
5.0 %
ISO 62
Moisture Absorption 2.00 %
2.00 %
ISO 62
Linear Mold Shrinkage, Flow 0.0090 cm/cm
0.0090 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0090 cm/cm
0.0090 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Ball Indentation Hardness 85.0 MPa
12300 psi
conditioned; ISO 2039-1
175 MPa
25400 psi
dry; ISO 2039-1
Tensile Strength at Break 45.0 MPa
6530 psi
conditioned; ISO 527-1/-2
75.0 MPa
10900 psi
dry; ISO 527-1/-2
Elongation at Break 10 %
10 %
dry; ISO 527-1/-2
35 %
35 %
conditioned; ISO 527-1/-2
Tensile Modulus 1.80 GPa
261 ksi
conditioned; ISO 527-1/-2
4.10 GPa
595 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched 3.00 J/cm²
14.3 ft-lb/in²
dry; ISO 179/1eU
8.50 J/cm²
40.4 ft-lb/in²
conditioned; ISO 179/1eU
2.50 J/cm²

@Temperature 30.0 °C
11.9 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
2.50 J/cm²

@Temperature 30.0 °C
11.9 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 0.400 J/cm²
1.90 ft-lb/in²
dry; ISO 179/1eA
0.800 J/cm²
3.81 ft-lb/in²
conditioned; ISO 179/1eA
0.200 J/cm²

@Temperature 30.0 °C
0.952 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
0.300 J/cm²

@Temperature 30.0 °C
1.43 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 80.0 µm/m-°C
44.4 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 80.0 µm/m-°C
44.4 µin/in-°F
ISO 11359-1/-2
Melting Point 260 °C
500 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 100 - 120 °C
212 - 248 °F
long term; EMS
220 °C
428 °F
short term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C
158 °F
ISO 75-1/-2
Deflection Temperature at 8.0 MPa 50.0 °C
122 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
conditioned; IEC 60093
1.00e+14 ohm-cm
1.00e+14 ohm-cm
dry; IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Strength 25.0 kV/mm
635 kV/in
conditioned; IEC 60243-1
27.0 kV/mm
686 kV/in
dry; IEC 60243-1
Comparative Tracking Index 500 V
500 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Automotive Interior
Electricals & Electronics Electrical appliances
Lighting
Form Granules
Industry & Consumer goods Housewares
Mechanical Engineering
Sports & Leisure
Tools & Accessories
Processing Injection Molding
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved