Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
ISO 1183-1
Quadrant EPP Techtron® PPS unfilled, extruded (ISO Data)
This unfilled polyphenylene sulfide based material is ideal for structural applications in corrosive environments or as a PEEK replacement at less demanding temperatures. Very good dimensional stabi..
Density 1.35 g/cc
0.0488 lb/in³
Plastcom SLOVASTER® B1 GF 6 PBT, 6% glass fibre
FeaturesPBT for injection moulding, chemically reinforced with 6 % glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending..
Density 1.35 g/cc
0.0488 lb/in³
Average value: 1.35 g/cc Grade Count:7
Overview of materials for Polyvinyl Chloride - Polyvinyl Acetate Copolymer
This property data is a summary of similar materials in the MatWeb database for the category "Polyvinyl Chloride - Polyvinyl Acetate Copolymer". Each property range of values reported is minimum and..
Density 1.35 g/cc
0.0488 lb/in³
ASTM D792
Ensinger Sintimid™ V-HPHT high purity high temp Polyimide (PI)  (discontinued **)
SINTIMID™ V polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an idea choice for the most demanding applications. SINTIMID™ V..
Density 1.35 g/cc
0.0488 lb/in³
ISO 1183
SABIC Innovative Plastics NORYL V02570 PPE+HIPS (Asia Pacific)
Noryl* V02570 is a 25% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t..
Density 1.35 g/cc
0.0488 lb/in³
ISO 1183-A
Solvay Technyl® C 216 Nylon 6, 30% Glass Fiber, EH50
Polyamide PA6, reinforced with 30% of glass fiber, for injection molding.It has good mechanical properties. It is used in all sectors of industry, offering an excellent combination between thermal ..
Density 1.35 g/cc
0.0488 lb/in³
ASTM D792
Solvay Specialty Polymers Radel® R-7159 Polyphenylsulfone (PPSU)
Radel® R-7159 polyphenylsulfone (PPSU) was developed specifically for aircraft interior applications. The product complies with the FAA regulation 14CFR Part 25 Appendix F, offering vertical burn..
Density 1.35 g/cc
0.0488 lb/in³
ASTM D 792
SABIC Innovative Plastics LNP Thermocomp GF003 PSU (Asia Pacific)
LNP* THERMOCOMP* GF003 is a compound based on Polysulfone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region.
Density 1.35 g/cc
0.0488 lb/in³
ISO 1183
Teijin Panlite® G-3120PH For Cameras, Glass Fiber Reinforced Polycarbonate Resin
Reinforced with 30 % of special GF and improved appearance grade.Applications:Precision machinery, electric and electronic components that need dimensional accuracy and good appearance.Information p..
Density 1.35 g/cc
0.0488 lb/in³
ASTM D792
Tipco Tipcolite® THD 321 Phenolic Compound, Wood Flour & Cellulose, having Soft Flow & High Strength
Soft Flow Phenolic Compound, Reinforced with Wood Flour & CelluloseApplications: Switchgear, HRC FusesProcessing: Compression & TransferInformation provided by the Manufacturer, Tipco Industries Lt..
Density 1.35 g/cc
0.0488 lb/in³
ISO 1183
Wolf Kunststoff ZEDEX® ZX-100K A1K Polymer Alloy
Main Characteristics: Hard; Stiff; Tough; High fatigue strength; Good weather resistance; Good machinability; FDA compliant LABS; PTFE and silicone-free; KTW approved; Stress resistantApplications: ..
Density 1.35 g/cc
0.0488 lb/in³
ISO 1183
DSM Akulon® K224-G6 Nylon 6-30% Glass Reinforced (European and Asian Grade) (Dry)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
Density 1.35 g/cc
0.0488 lb/in³
24hr/23°C/50% RH; ISO 1183-A; IEC/EN 60893-2 8.1
Elektro-Isola Etronit IIQ R XX Phenolic, Paper Reinforcement, Yellow, Sheets
Description: Mechanically a good Etronit type with electrical properties adequate for insulation in low-voltage applications. Applications: Used in electrical appliances, bus-bar carriers, partition..
Density 1.35 g/cc
0.0488 lb/in³
24hr/23°C/50% RH; ISO 1183-A; IEC/EN 60893-2 8.1
Elektro-Isola Etronit IS Phenolic, Paper Reinforcement, Dark Brown, Sheets
Description: Very good high-voltage insulation material. Very high breakdown voltage, in particular parallel to the layers. Dimensionally stable.Application: Insulation material in high-voltage tap ..
Density 1.35 g/cc
0.0488 lb/in³
ISO 1183
CP-Polymer-Technik Wellamid® 6000 GS 30 HWUVCP 30% Glass Sphere Filled Nylon 6, UV Stabilized, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
Density 1.35 g/cc
0.0488 lb/in³
ISO 1183
CP-Polymer-Technik Wellamid® 6000 GV 30 HW 30% Glass Fiber Nylon 6, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
Density 1.35 g/cc
0.0488 lb/in³
ISO 1183
EMS-Grivory Grivory® TSG-30/4 H black 9836 PA666-GF30
Information provided by EMS Grivory
Density 1.35 g/cc
0.0488 lb/in³
ISO 1183
Eurostar Star L PA66 30Y D61 PA66, Carbon Fiber Filled, Injection Molded
Star L PA66 30Y D51 is a PTFE/Silicone Oil Lubricated, Carbon Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar.
Density 1.35 g/cc
0.0488 lb/in³
ISO 1183
Eurostar Starflam BFR460B PA6, Glass Fiber Filled, Flame Retardant, Injection Molded
Starflam BFR460B is a Flame Retardant, Glass Fiber Reinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
Density 1.35 g/cc
0.0488 lb/in³
Silicone Property; Arlon SQA-TMS-024
Arlon 55986R028 0.0295" Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: 3 mil PESide 2: Uncured Silicone RubberSubstrate: Style 162 FiberglassSide 1: Cured Silicone RubberThis data represents typical values for the production material..
Density 1.35 g/cc
0.0488 lb/in³
Layer 1 Silicone Property; Arlon SQA-TMS-024
Arlon 56579R028 0.0295" Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: 2.5 mil PELayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 1564 FiberglassThis data represents typical values for the production mate..
Density 1.35 g/cc
0.0488 lb/in³
ISO 1183
BASF Ultramid® 66 H2 G/25-V0KB1 BK 3324 PA66 (Dry)
Description: Ultramid 66 H2 G/25-V0KB1 BK3324 is a 25% glass reinforced, heat stabilized injection molding grade. It's a V-0 self-extinguishing, with phosphorous. It offers good flowability, surface..
Density 1.35 g/cc
0.0488 lb/in³
Silicone Property; Arlon SQA-TMS-024
Arlon 51100R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 7628 FiberglassProduct Use: Flexible heater insulationAppearance: Red silicone gum on fiberglass fabricT..
Density 1.35 g/cc
0.0488 lb/in³
Silicone Property; Arlon SQA-TMS-024
Arlon 51103R015 0.0150" Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: LDPESide 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Cured Silicone RubberInterleave: LDPEThis data represents typical values for the producti..
Density 1.35 g/cc
0.0488 lb/in³
Silicone Property; Arlon SQA-TMS-024
Arlon 55276B028 0.0295" (0.749 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 2: Uncured Silicone Rubber Substrate: Style 162 FiberglassSide 1: Cured Silicone Rubber This data represents typical values for the production mate..
Density 1.35 g/cc
0.0488 lb/in³
Layer 1, Silicone Property; Arlon SQA-TMS-024
Arlon 55279R033 0.033" (0.838 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Product Use: Flexible heater insulationAppearance: Red s..
Density 1.35 g/cc
0.0488 lb/in³
ISO 1183
Pasargad Polymer Peyvand Pasamid 3P-M1130B Nylon 6, 30% Glass Fiber Reinforced
Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Electrical PartsFastenerHousingInformation provided by Pasargad Polymer Peyvand Co
Density 1.35 g/cc
0.0488 lb/in³
DuPont Performance Polymers Sorona® 3030G NC010 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)&
30% Glass Reinforced Polytrimethylene Terephthalate Sorona 3030G NC010 is a 30% glass reinforced PTT resin containing 25% renewably sourced ingredients by weight (37% based on polymer only) with goo..
Density 1.35 g/cc
0.0488 lb/in³
ASTM D792
Kleerdex Kydex® 120 Acrylic/PVC Thermoplastic Sheet  (discontinued **)
USDA approved thermoplastic sheetApplications: High impact resistant wallcovering, push plates and kick plates, equipment housings, splash and safety guardsFeatures: Kydex 120 meets class I/A fire c..
Density 1.35 g/cc
0.0488 lb/in³
Silicone Property; Arlon SQA-TMS-024
Arlon 48271R010 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 1080 FiberglassSide 2: Uncured Silicone RubberInterleave 2: Polyethylene Product Use: Flexible heater ..