Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 8.0 MPa | 50.0 °C | 122 °F | Average value: 50.0 °C Grade Count:3 |
Overview of materials for Nylon 6, 30% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are includ.. |
|||
Deflection Temperature at 8.0 MPa | 50.0 - 204 °C | 122 - 399 °F | Average value: 141 °C Grade Count:20 |
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are incl.. |
|||
Deflection Temperature at 8.0 MPa | 50.0 °C | 122 °F | ISO 75-1/-2 |
Lanxess Durethan® A 30 H2.0 901510 Nylon 66 PA 66 standard injection molding grade, non-reinforced, very easy release, good heat-ageing resistanceApplication Examples: terminal blocks, cable clips, bobbins, gearwheels |
|||
Deflection Temperature at 8.0 MPa | 50.0 °C | 122 °F | ISO 75-1/-2 |
Lanxess Durethan® B 31 SK 000000 Nylon 6 PA 6, injection molding grade, non-reinforced, easy flow, easy-release, rapid solidification, crystallizes somewhat more finely and uniformly than B 30 S |
|||
Deflection Temperature at 8.0 MPa | 50.0 °C | 122 °F | ISO 75-1/-2 |
Lanxess Durethan® DP 1100/30 H2.0 901510 Nylon 6, Micro Glass Balls PA6, molding grade, micro glass balls, good heat-ageing resistance |
|||
Deflection Temperature at 8.0 MPa | 50.0 °C | 122 °F | ISO 75-1/-2 |
Lanxess Durethan® DP 2325 H3.0 000000 Nylon 66 PA 66, injection molding grade, non-reinforced, elastomer-modified, good heat-ageing resistance, extremely high notched impact strength even at dry state and at low temperatures |
|||
Deflection Temperature at 8.0 MPa | 50.0 °C | 122 °F | ISO 75-1/-2 |
Lanxess Durethan® DP BC 500 H2.0 901510 Nylon 6 PA 6, extrusion and blow molding grade, non-reinforced, elastomer-modified, high viscosity, good heat-ageing resistance |
|||
Deflection Temperature at 8.0 MPa | 50.0 °C | 122 °F | ISO 75-1/-2 |
Lanxess Pocan® B 7375 000000 PBT, White Pigment PBT, 25% white pigments, injection molding, improved light reflection, low tendency to warp |
|||
Deflection Temperature at 8.0 MPa | 50.0 °C | 122 °F | ISO 75-1/-2 |
Lanxess Pocan® B 7425 000000 PBT, 20% Glass Spheres PBT, 20% glass spheres, injection molding, low tendency to warp, improved surface finish |
|||
Deflection Temperature at 8.0 MPa | 50.0 °C | 122 °F | ISO 75-1/-2 |
Lanxess Durethan® A 30 000000 Nylon 66 PA 66, standard injection molding grade, non-reinforced, very easy release, normal solidificationApplication Examples: terminal blocks, cable clips, bobbins, gearwheels |
|||
Deflection Temperature at 8.0 MPa | 50.0 °C | 122 °F | ISO 75-1/-2 |
Lanxess Durethan® BM 240 H2.0 901510 Nylon 6, 40% Mineral PA 6, injection molding grade, 40% mineral, isotopic properties, good heat-ageing resistance |
|||
Deflection Temperature at 8.0 MPa | 50.0 °C | 122 °F | ISO 75-1/-2 |
Lanxess Pocan® BF 4409 000000 PBT, 7% Glass Fiber PBT, 7% glass fibers, injection molding, flame retardant |
|||
Deflection Temperature at 8.0 MPa | 50.0 °C | 122 °F | ISO 75-1/-2 |
Lanxess Pocan® DP 1105 000000 PBT PBT, non-reinforced, injection molding, extrusion, improved flowability |
|||
Deflection Temperature at 8.0 MPa | 50.0 °C | 122 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® BGM-30 X PA6-(GF+MD)30 Product description: Grilon BGM-30 X is a heat stabilized PA 6 injection molding grade with a 30 % reinforcement combination (mineral and glass fiber). Grilon BGM-30 X has the following important pr.. |
|||
Deflection Temperature at 8.0 MPa | 50.0 °C | 122 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® BM-30 FR PA6-MD30 FR Information provided by EMS Grivory |
|||
Deflection Temperature at 8.0 MPa | 50.0 °C | 122 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® EBV-15H black 9697 PA6-GF15 Product description: Grilon EBV-15H black 9697 is a high viscosity, heat stabilized PA6 extrusion blow molding grade with 15% glass fibers. Grilon EBV-15H black 9697 has the following important prop.. |
|||
Deflection Temperature at 8.0 MPa | 50.0 °C | 122 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® TSK-30/4 PA666-GB30 Product description: Grilon TSK-30/4 is a heat stabilized, normal viscosity PA66 +PA6 injection molding grade with 30% glass beads. Grilon TSK-30/4 has the following important properties: Good surfa.. |
|||
Deflection Temperature at 8.0 MPa | 50.0 °C | 122 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® BM-30/2 PA6-MD30 Product description: Grilon BM-30/2 is a 30% mineral reinforced PA6 injection molding grade. Grilon BM-30/2 has the following important properties: Iow warpageImpact resistantIsotropic shrinkage App.. |