Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Total Finathene® 53080 HDPE, blow molding, sheet  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total Finathene® 53080 HDPE, blow molding, sheet  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Finathene E® 53080 is a high density polyethylene produced by the slurry loop low pressure polymerization process. Finathene E® 53080 has been especially developed for the production of containers to be submitted to the regulations for transportation of dangerous goods. Finathene® 53080 is best processed at temperatures between 180 and 220°C.Information provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Density 0.953 g/cc
0.0344 lb/in³
ISO 1183
Environmental Stress Crack Resistance 200 hour
200 hour
ASTM D1693-70
High Load Melt Index 8.0 g/10 min

@Load 21.6 kg
8.0 g/10 min

@Load 47.6 lb
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 38.0 MPa
5510 psi
ISO 527
Tensile Strength, Yield 28.0 MPa
4060 psi
ISO 527
Elongation at Break >= 700 %
>= 700 %
ISO 527
Elongation at Yield 9.0 %
9.0 %
ISO 527
Flexural Modulus 1.30 GPa
189 ksi
ISO 178
Tensile Impact Strength 120 kJ/m²
57.1 ft-lb/in²
Notched, -30°C; ISO 8256
280 kJ/m²
133 ft-lb/in²
Notched, 23°C; ISO 8256
Thermal Properties Metric English Comments
Vicat Softening Point 127 °C
261 °F
ISO 306
Descriptive Properties Value Comments
Food Approval This material complies with the main regulations concerning non-toxicity of plastics materials in contact with food stuffs.
Copyright © lookpolymers.com All Rights Reserved