Material Notes:
Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. Flame retardant.Information provided by Hippe.
Physical Properties Metric English Comments
Specific Gravity 1.70 - 1.90 g/cc
1.70 - 1.90 g/cc
IEC 1212-2 8.1
Mechanical Properties Metric English Comments
Tensile Strength >= 300 MPa
>= 43500 psi
IEC 1212-2 5.7
Flexural Strength >= 340 MPa
>= 49300 psi
Perpendicular to laminations; IEC 1212-2 5.1
Flexural Modulus >= 24.0 GPa
>= 3480 ksi
IEC 1212-2 5.2
Compressive Strength >= 350 MPa
>= 50800 psi
Perpendicular to laminations; IEC 1212-2 5.3
Shear Strength >= 30.0 MPa
>= 4350 psi
Parallel to laminations; IEC 1212-2 5.6
Izod Impact, Unnotched (ISO) >= 34.0 kJ/m²
>= 16.2 ft-lb/in²
Parallel to laminations; IEC 1212-2 5.5.3
Charpy Impact Unnotched >= 3.30 J/cm²
>= 15.7 ft-lb/in²
Parallel to laminations; IEC 1212-2 5.5.2
Thermal Properties Metric English Comments
Flammability, UL94 V-0
V-0
IEC 1212-2 7.2
Electrical Properties Metric English Comments
Insulation Resistance >= 5.00e+10 ohm
>= 5.00e+10 ohm
After immersion in water; IEC 1212-2 6.3
Dielectric Constant <= 5.5

@Frequency 48.0 - 62.0 Hz
<= 5.5

@Frequency 48.0 - 62.0 Hz
IEC 1212-2 6.2
<= 5.5

@Frequency 1.00e+6 Hz
<= 5.5

@Frequency 1.00e+6 Hz
IEC 1212-2 6.2
Dielectric Breakdown >= 35000 V

@Temperature 90.0 °C
>= 35000 V

@Temperature 194 °F
In oil, parallel to laminations; IEC 1212-2 6.2
Dissipation Factor <= 0.040

@Frequency 48.0 - 62.0 Hz
<= 0.040

@Frequency 48.0 - 62.0 Hz
IEC 1212-2 6.2
<= 0.040

@Frequency 1.00e+6 Hz
<= 0.040

@Frequency 1.00e+6 Hz
IEC 1212-2 6.2
Comparative Tracking Index >= 200 V
>= 200 V
IEC 1212-2 6.4
Descriptive Properties Value Comments
Thermal Endurance 155 T.I.
IEC 1212-2 7.1
Water Absorption < 34 mg
IEC 1212-2 8.2; Test piece 50 x 50 x 10 mm