Electrical Properties | Metric | English | Comments |
---|---|---|---|
Comparative Tracking Index | 500 V | 500 V | STN 34 6468 |
Plastcom SLOVAMID 6 FRC 2 LS Polyamide 6, Halogen Free Flame Retardant, Light Stabilization FeaturesLongterm external use is possible because of the material stabilization with the light stabilizers on the HALS basis. Meets the flammability in accordance with the norm DIN 4102 - B1. PA 6.. |
|||
Comparative Tracking Index | 500 V | 500 V | Solution A; IEC 60112 |
Polimeri Europa Edistir R 850E Polystyrene Super high impact polystyrene with good heat resistance. Designed for sheet extrusion and thermoforming of deep drawn containers even
diluted with high percentage of GP. Suitable for general injecti.. |
|||
Comparative Tracking Index | 500 V | 500 V | Solution A; IEC 60112 |
PolyOne Bergamid™ A70 GK30 H Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Comparative Tracking Index | 500 V | 500 V | CTI 100; IEC 112 |
Nilit FRIANYL B63 W-KV20 Nylon 6 for injection molding, 20% glass ball reinforced Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Comparative Tracking Index | 500 V | 500 V | Solution A, Rating; IEC 60112 |
Lanxess Durethan® BKV 15 H3.0 000000 Nylon 6 Copolymer, 15% Glass Fibers PA 6 Copolymer, 15% glass fibers, injection molding, heat-ageing stabilized |
|||
Comparative Tracking Index | 500 V | 500 V | Solution B; IEC 60112 |
Solvay TECHNYL® A 221 PA66, DRY Description TECHNYL ® A 221 is an unreinforced polyamide 66, medium viscosity, for injection molding, with a special crystallizing agent, for fast cycles. It is available in natural colors. Benef.. |
|||
Comparative Tracking Index | 500 V | 500 V | IEC 60112 |
SABIC Innovative Plastics LNP THERMOCOMP RB00A PA 66 (Europe-Africa-Middle East) 50% glass beads filled Polyamide 66 injection moulding resin. |
|||
Comparative Tracking Index | 500 V | 500 V | UL 746 |
Teknor Apex Chemlon® 104-13 GH Nylon 66, 13% Glass Fiber Reinforced Notes: Impact Modified; Reinforced with 13% Glass Fibers; Synergistic compound exhibiting impact strength and dimensional stability Features: Good Dimensional stability; Good Processability; Heat St.. |
|||
Comparative Tracking Index | 500 V | 500 V | IEC 60112 |
SABIC Innovative Plastics LNP Thermocomp PF006 PA 6 (Europe-Africa-Middle East) 30% glass fibre reinforced Polyamide 6 injection moulding resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Comparative Tracking Index | 500 V | 500 V | DIN IEC 112 / VDE 030 t1 |
DSM Fibre Intermediates Nyrim® 1500 (Conditioned) Conditioned at 23°C and 50% Relative Humidity.Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is proc.. |
|||
Comparative Tracking Index | 500 V | 500 V | conditioned; IEC 60112 |
EMS-Grivory Grivory® HT2V-15H PA6T/66-GF15 Product description: Grivory HT2V-15H is a 15 % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Polymer designation acc. to ISO.. |
|||
Comparative Tracking Index | >= 500 V | >= 500 V | IEC 1212-2 6.4 |
Hippe MF GC 201 Woven Glass Cloth Reinforced Melamine Resin - Sheet Used in mechanical and electrical applications. High mechanical strength. Arc and tracking resistant. Flame retardant. Information provided by Hippe. |
|||
Comparative Tracking Index | 500 V | 500 V | IEC 60112 |
Eurostar Staramide AG5K PA66, 25% Glass Filled, Injection Molded AG5 is a Heat and Hydrolytically Stabilized, 25% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli.. |
|||
Comparative Tracking Index | 500 V | 500 V | IEC 60112 |
Eurostar Staramide BG6H PA6, 30% Glass Filled, Injection Molded BG6 is a Heat Stabilized, 30% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Comparative Tracking Index | 500 V | 500 V | IEC 60112 |
Eurostar Staramide BG7H PA6, 35% Glass Fiber Filled, Heat Stabilized, Injection Molded Staramide BG7H is a Heat Stabilized, 35% Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Comparative Tracking Index | 500 V | 500 V | IEC 60112 |
Eurostar Staramide RB006S PA66, 30% Glass Bead Filled, Injection Molded Staramide RB006S is a 30% Glass Bead Reinforced Polyamide 66 Injection Molding Resin (also known as Staramide 66 30K S3)Information provided by Eurostar. |
|||
Comparative Tracking Index | 500 V | 500 V | IEC 60112 |
Eurotec® Tecodur® PB70 GR30 NL CA 01 PBT/PET 30% glass fiber reinforced Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Comparative Tracking Index | 500 V | 500 V | Solution A; IEC 60112 |
Eurotec® Tecoform® PO20 GR25 NL HS POM, 25% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Comparative Tracking Index | 500 V | 500 V | IEC 60112 |
Eurotec® Tecodur® PB70 GR20 NL CA 01 PBT/PET 20% glass fiber reinforced Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Comparative Tracking Index | 500 V | 500 V | Solution A; IEC 60112 |
Eurotec® Tecoform® PO30 GB20 NL HS POM, 20% glass bead reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Comparative Tracking Index | 500 V | 500 V | IEC 112 |
Azoty Tarnow™ Tarnamid® T-27 GF50 Polyamide 6 - Glass Fiber Reinforced 50% Glass fiber reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High.. |
|||
Comparative Tracking Index | >= 500 V | >= 500 V | |
Bulk Molding Compounds BMC 620X Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 620X molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a high impact material produced in ex.. |
|||
Comparative Tracking Index | >= 500 V | >= 500 V | |
Bulk Molding Compounds BMC T60-6002A-WG Wear Resistant Molding Compound BMC T60-6002A-WG is a wear resistant molding compound specifically formulated for applications that require excellent abrasion resistance. Due to its low specific gravity it has substantial cost pe.. |
|||
Comparative Tracking Index | 500 - 600 V | 500 - 600 V | Average value: 578 V Grade Count:9 |
Overview of materials for Acetal Copolymer, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Glass Bead Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Comparative Tracking Index | 500 V | 500 V | Solution A; IEC 60112 |
Eurotec® Tecomid® NB40 GR25 NL PA6, 25% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Comparative Tracking Index | 500 V | 500 V | Solution B; IEC 60112 |
Solvay TECHNYL® 2411GF6 PA66, 30% glass fiber, Conditioned Description: Polyamid 66, 30% glass fiber reinforce, for injection moldingAvailable in: Asia PacificProduct Applications: TECHNYL® 2411GF6 used in all sectors of industry, offering an excellent com.. |
|||
Comparative Tracking Index | 500 V | 500 V | Solution B; IEC 60112 |
Solvay TECHNYL® A 216 V30 Natural FA PA66, 30% glass fiber, Conditioned Description: Polyamide PA66, reinforced with 30% of glass fiber and modified for enhanced injection molding.Available in: Europe Product Applications: This material offers an excellent combination b.. |
|||
Comparative Tracking Index | 500 V | 500 V | dry; IEC 60112 |
DSM Stanyl® TS200F6 PA46-GF30 30% Glass Reinforced |
|||
Comparative Tracking Index | >= 500 V | >= 500 V | |
Bulk Molding Compounds BMC T40(20) Die Casting Replacement Grade Molding Compound BMC T40(20) was formulated as a direct replacement for aluminum die casting applications. T40(20) is UL recognized. Excellent mechanical properties and dimensional control allow molded parts to ma.. |