Material Notes:
Product description: Grilon TSGZ-15 is a heat stabilized, normal viscosity, and impact modified PA66 + PA6 injection molding grade with 15% glass fibers. Grilon TSGZ-15 has the following important properties: Good impact strength after moldingGood flow behaviorEasy processing Application examples are fictional parts for automotive and mechanical engineering applications such as levers and strips.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183
Water Absorption 8.0 %
8.0 %
ISO 62
Moisture Absorption 3.00 %
3.00 %
ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cm
0.0010 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0070 cm/cm
0.0070 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Ball Indentation Hardness 75.0 MPa
10900 psi
conditioned; ISO 2039-1
160 MPa
23200 psi
dry; ISO 2039-1
Tensile Strength at Break 65.0 MPa
9430 psi
conditioned; ISO 527-1/-2
110 MPa
16000 psi
dry; ISO 527-1/-2
Elongation at Break 4.0 %
4.0 %
dry; ISO 527-1/-2
10 %
10 %
conditioned; ISO 527-1/-2
Tensile Modulus 2.90 GPa
421 ksi
conditioned; ISO 527-1/-2
5.60 GPa
812 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched 7.50 J/cm²
35.7 ft-lb/in²
dry; ISO 179/1eU
9.00 J/cm²
42.8 ft-lb/in²
conditioned; ISO 179/1eU
6.00 J/cm²

@Temperature 30.0 °C
28.6 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
7.00 J/cm²

@Temperature 30.0 °C
33.3 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 1.20 J/cm²
5.71 ft-lb/in²
dry; ISO 179/1eA
1.70 J/cm²
8.09 ft-lb/in²
conditioned; ISO 179/1eA
0.500 J/cm²

@Temperature 30.0 °C
2.38 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
0.500 J/cm²

@Temperature 30.0 °C
2.38 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 20.0 µm/m-°C
11.1 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 110 µm/m-°C
61.1 µin/in-°F
ISO 11359-1/-2
Melting Point 260 °C
500 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 100 - 120 °C
212 - 248 °F
long term; EMS
200 °C
392 °F
short term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 215 °C
419 °F
ISO 75-1/-2
Deflection Temperature at 8.0 MPa 60.0 °C
140 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
conditioned; IEC 60093
1.00e+13 ohm-cm
1.00e+13 ohm-cm
dry; IEC 60093
Surface Resistance 1.00e+10 ohm
1.00e+10 ohm
IEC 60093
Dielectric Strength 27.0 kV/mm
686 kV/in
conditioned; IEC 60243-1
30.0 kV/mm
762 kV/in
dry; IEC 60243-1
Comparative Tracking Index 600 V
600 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Automotive Interior
Powertrain and Chassis
Electricals & Electronics Connectors
Electrical appliances
Form Granules
Industry & Consumer goods Housewares
Mechanical Engineering
Power transmission
Sports & Leisure
Tools & Accessories
Processing Injection Molding
Special Characteristics High impact or impact modified