Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 9.00 J/cm² | 42.8 ft-lb/in² | ISO 179 |
PolyOne OnForce™ LFT AM-60LGF/001 Natural Polyphthalamide (PPA) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Charpy Impact Unnotched | 9.00 J/cm² | 42.8 ft-lb/in² | ISO 179 |
PolyOne OnForce™ LFT NN-60LGF/000 HS Natural Polyamide 66 (Nylon 66) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Charpy Impact Unnotched | 9.00 J/cm² @Temperature 23.0 °C |
42.8 ft-lb/in² @Temperature 73.4 °F |
|
Radici Radilon® A RV330 (cond.) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Charpy Impact Unnotched | 9.00 J/cm² | 42.8 ft-lb/in² | flatwise; ISO 179 1fU |
Lehmann & Voss LUVOCOM® 1105-8135/GN PEEK, unreinforced, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan.. |
|||
Charpy Impact Unnotched | 9.00 J/cm² | 42.8 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 50-8276 Polycarbonate, with PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High dimensionally stable precision parts, even at elevated te.. |
|||
Charpy Impact Unnotched | 9.00 J/cm² @Temperature 23.0 °C |
42.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Grupo Repol Dinalon® B1S25 G35 35% Glass Fiber Reinforced Nylon 6 Mechanical properties are for dry as molded samples.Information provided by Grupo Repol. |
|||
Charpy Impact Unnotched | 9.00 J/cm² | 42.8 ft-lb/in² | cond.; ISO 179-1eU |
Lanxess Durethan® DP BKV 30 XF 000000 Nylon 6, 30% Glass Fiber PA 6, 30% glass fibers, injection molding, improved flowability, improved surface finishInformation provided by LANXESS. |
|||
Charpy Impact Unnotched | 9.00 J/cm² | 42.8 ft-lb/in² | ISO 179/1eU |
Solvay TECHNYL® A 218 V35 Black 21NHFE PA66, 35% glass fiber, Conditioned Description: TECHNYL® A 218 V35 BLACK 21NHFE is polyamide 6.6, high flow, reinforced with 35% glass fiber, heat stabilized, for injection molding. This product is available in black color.Benefit.. |
|||
Charpy Impact Unnotched | 9.00 J/cm² | 42.8 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics LNP THERMOCOMP PF006S PA 6 (Europe-Africa-Middle East) Heat stabilized, 30% glass fibre reinforced Polyamide 6 injection moulding resin. |
|||
Charpy Impact Unnotched | 9.00 J/cm² @Temperature 30.0 °C |
42.8 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® BG-60 FC PA6-GF60 Product description: Grilon BG-60 FC is a heat stabilized PA6 injection molding grade with 60% glass fibers. Grilon BG-60 FC has the following important properties: Short cycle timesExcellent surfac.. |
|||
Charpy Impact Unnotched | 9.00 J/cm² @Temperature 23.0 °C |
42.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6000/52 GV 15 HWUVCP 15% Glass Fiber Nylon 6, Low Temperature Impact Modified, UV Stabilized, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact Unnotched | 9.00 J/cm² | 42.8 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® GV-5H black PA*-GF50 Product description: Grivory GV-5H black 9915 is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||
Charpy Impact Unnotched | 9.00 J/cm² @Temperature 23.0 °C |
42.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6600 MRGV 20/20 HWCP 20% Mineral and 20% Glass Fiber Nylon 66, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact Unnotched | 9.00 J/cm² | 42.8 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® LBV-30H FWA black 9225 PA12-GF30 Product Description: Grilamid LBV-30H FWA black 9225 is a 30% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: Stiffness combined wit.. |
|||
Charpy Impact Unnotched | 9.00 J/cm² @Temperature 30.0 °C |
42.8 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® LV-30H FWA black 9225 PA12-GF30 Product description: Grilamid LV-30H FWA black 9225 is a 30 % glass fiber reinforced, heat stabilized polyamide12 injection molding grade with the following special features: Stiffness combined with.. |
|||
Charpy Impact Unnotched | 9.00 J/cm² | 42.8 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® LV-50H FWA nat PA12-GF50 Product description: Grilamid LV-50H FWA natural is a 50 % glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combined w.. |
|||
Charpy Impact Unnotched | 9.00 J/cm² | 42.8 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® XE 4065 black 9238 PA*-GF50 Product description: Grivory XE 4065 is a 50% glass-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. This Grivory HT product is partia.. |
|||
Charpy Impact Unnotched | 9.00 J/cm² @Temperature -30.0 °C |
42.8 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 179/1eU |
DuPont Performance Polymers Zytel® 73G35HSL BK262 Nylon 6
(Unverified Data**) 35% Glass Reinforced Heat Stabilized Polyamide 6 Zytel 73G35HSL BK262 is a 35% glass fiber reinforced heat stabilized black polyamide 6 resin for injection molding.Information provided by DuPont Per.. |
|||
Charpy Impact Unnotched | 9.00 J/cm² | 42.8 ft-lb/in² | 50%RH; ISO 179/1eU |
DuPont Performance Polymers Zytel® FG70G30HSR3 BK309 Nylon 66
(Unverified Data**) Information provided by DuPont Performance Polymers |
|||
Charpy Impact Unnotched | 9.00 J/cm² @Temperature -30.0 °C |
42.8 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 179/1eU |
DuPont Performance Polymers Zytel® FG70G50HSLA BK309 Nylon 66
(Unverified Data**) 50% Glass Reinforced Heat Stabilized Polyamide 66 with Developed for Food Contact Applications Information provided by DuPont Performance Polymers |
|||
Charpy Impact Unnotched | 9.00 J/cm² | 42.8 ft-lb/in² | 50%RH; ISO 179/1eU |
DuPont Performance Polymers Zytel® HTN 53G50HSLR BK083 Polyphthalamide (PPA)
(Unverified Data**) 50% Glass Reinforced High Performance Polyamide with Improved Impact and Stiffness Zytel HTN53G50HSLR BK083 is a 50% glass reinforced heat stabilized lubricated high performance polyamide resin deve.. |
|||
Charpy Impact Unnotched | 9.00 J/cm² @Temperature -30.0 °C |
42.8 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eU |
DuPont Performance Polymers Zytel® HTN 53G50LWSF BK702A Polyphthalamide (PPA)
(Unverified Data**) 50% Glass Reinforced High Performance Polyamide with Low Warpage and High Stiffness Information provided by DuPont Performance Polymers |
|||
Charpy Impact Unnotched | 9.00 J/cm² | 42.8 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® BG-50 H PA6-GF50 Product description: Grilon BG-50 H is a high heat stabilized PA6 injection molding grade with 50% glass fibers. Grilon BG-50 H has the following important properties: High stiffnessHigh heat resist.. |
|||
Charpy Impact Unnotched | 9.00 J/cm² | 42.8 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® BG-50 S PA6-GF50 Product description: Grilon BG-50 S is a heat stabilized PA6 injection molding grade with 50% glass fibers. Grilon BG-50 S has the following important properties: High stiffnessExcellent surface fin.. |
|||
Charpy Impact Unnotched | 9.00 J/cm² @Temperature 23.0 °C |
42.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
BASF Ultramid® S3WG6 Balance 30% Glass Filled PA 610 (Conditioned) Description: BASF supplies polyamide 610 for processing by injection molding under the trade name Ultramid® Balance which is produced by polycondensation of hexamethylene diamine and sebacic acid. .. |
|||
Charpy Impact Unnotched | 9.00 J/cm² | 42.8 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® GV-5 FWA nat PA*-GF50 Product description: Grivory GV-5 FWA natural is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||
Charpy Impact Unnotched | 9.00 J/cm² @Temperature 30.0 °C |
42.8 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® BM-30/2 PA6-MD30 Product description: Grilon BM-30/2 is a 30% mineral reinforced PA6 injection molding grade. Grilon BM-30/2 has the following important properties: Iow warpageImpact resistantIsotropic shrinkage App.. |
|||
Charpy Impact Unnotched | 9.00 J/cm² @Temperature 30.0 °C |
42.8 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® LBV-50H FWA nat PA12-GF50 Product Description: Grilamid LBV-50H FWA natural is a 50% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combined w.. |
|||
Charpy Impact Unnotched | 9.00 J/cm² - NB @Temperature -30.0 - 30.0 °C |
42.8 ft-lb/in² - NB @Temperature -22.0 - 86.0 °F |
Average value: 18.9 J/cm² Grade Count:19 |
Overview of materials for Acetal Copolymer, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Impact Modified". Each property range of values reported is minimum and maximum values.. |