Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 110 µm/m-°C | 61.1 µin/in-°F | ISO 11359-2 |
Celanese Celanex® 2003HR PBT
(Unverified Data**) Celanex 2003HR is an unfilled polybutylene terephthalate which has an excellent hydrolysis resistance, mechanical properties and processabilityHydrolytically stable / injectionInformation provided b.. |
|||
CTE, linear, Transverse to Flow | 110 - 140 µm/m-°C | 61.1 - 77.8 µin/in-°F | Average value: 118 µm/m-°C Grade Count:19 |
Overview of materials for Acetal Homopolymer, Unreinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced, Impact Grade". Each property range of values reported is minimum and m.. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C | 61.1 µin/in-°F | ISO 11359-2 |
Celanese Celcon® LW25-S2 POM, Tribological
(Unverified Data**) Celcon® LW25-S2 acetal copolymer is a low flow, improved toughness product formulated with a low level of silicone to reduce friction and improved wear resistance.Low wear/friction, silicone, low s.. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C | 61.1 µin/in-°F | ISO 11359-2 |
Celanese Celcon® WR25Z POM, UV Resistant
(Unverified Data**) Celcon® WR25Z is a 2.5 nominal melt flow rate based acetal copolymer stabilized to provide maximum ultraviolet radiation resistance in outdoor applications. Celcon® WR25Z is a lower flow product .. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C | 61.1 µin/in-°F | ISO 11359-1/-2 |
Lanxess Durethan® B 30 S 000000 Nylon 6 PA 6, injection molding-grade, non-reinforced, easy-flow, easy-release, rapid solidification |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C | 61.1 µin/in-°F | ISO 11359-1/-2 |
Lanxess Pocan® KU 2-7209 Z 000000 PBT, 15% Glass Fiber PBT, 15% glass fibers, injection molding, flame retardant, impact modified |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C | 61.1 µin/in-°F | ISO 11359-1/-2 |
Lanxess Pocan® KU 2-7604 000000 PBT+PC PBT+PC, non-reinforced, injection molding, extrusion, flame retardant, impact modified, low tendency to warp |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature 23.0 - 80.0 °C |
61.1 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xenoy® 6370 PBT+PC (Europe-Africa-Middle East) XENOY 6370 is an impact modified semi-crystalline thermoplastic. blend with 30% glass fibre reinforcement offering toughness and ductility. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature 23.0 - 80.0 °C |
61.1 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xenoy® CL200 PBT+PC (Europe-Africa-Middle East) XENOY CL200 is a semi-crystalline thermoplastic blend, specially developed to obtain good low temperature impact strength combined with excellent chemical resistance to occasional solvent and gasoli.. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature 23.0 - 80.0 °C |
61.1 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xenoy® XD1507S PBT+PC (Europe-Africa-Middle East) XENOY XD1507S is an impact modified PBT+PC blend with outstanding chemical resistance, good UV stability and flow properties, designed for self coloured, optiwall bumper facias.This data was supplie.. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature 20.0 °C |
61.1 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Arnitel® EL740-H/A Injection Molding; Other Extrusion Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C | 61.1 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® TSGZ-15/4 PA666-GF15 Information provided by EMS Grivory |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C | 61.1 µin/in-°F | ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® 127UVE NC010 Acetal (POM)
(Unverified Data**) UV Stabilized High Viscosity Acetal Homopolymer with Very Low Emissions Delrin 127UVE NC010 (formerly DE20555) is a high viscosity acetal homopolymer with UV stabilizers with very low VOC emissions .. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C | 61.1 µin/in-°F | DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® FE5382 BK276 Nylon 612
(Unverified Data**) 33% Glass Reinforced Polyamide 612 Developed for Electrical and Electronics Applications Zytel FE5382 BK276 is a 33% glass fiber reinforced heat stabilized black polyamide 612 resin developed for el.. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature 23.0 - 80.0 °C |
61.1 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/2 |
Akro-Plastic Akromid® A3 (2414) PA 6.6 Dry AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C | 61.1 µin/in-°F | ISO 11359-2 |
Celanese CELANEX 2003HR PBT, Unfilled Celanex 2003HR is an unfilled polybutylene terephthalate which has an excellent hydrolysis resistance, mechanical properties and processabilityInformation provided by Celanese |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C | 61.1 µin/in-°F | ISO 11359-2 |
Celanese CELANEX 3200FC PBT, 15% Glass Reinforced Celanex 3200FC is a general purpose, 15% glass reinforced polybutylene terephthalate with a good balance of mechanical properties and processability.Information provided by Celanese |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C | 61.1 µin/in-°F | ISO 11359-2 |
Celanese Celcon® WR90Z POM, UV Resistant Celcon« WR90Z is a standard nominal 9 melt flow rate based acetal copolymer stabilized to provide maximum ultraviolet radiation resistance in outdoor applications while retaining a good balance of .. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C | 61.1 µin/in-°F | ISO 11359-2 |
Celanese Hostaform® C 9021 10/9005 POM, Unfilled Hostaform« C 9021 10/9005 is a nominal 9 melt flow rate acetal copolymer which is capable of being permanently marked by a laser. Parts molded from Hostaform« C 9021 10/9005 can be laser marked wi.. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C | 61.1 µin/in-°F | ISO 11359-2 |
Celanese Hostaform® EC140XF POM, Specialty Hostaform« EC140XF is a conductive ESD grade of acetal copolymer for applications requiring dissipation of static build-up. EC140XF has an improved resistance to aggressive fuel blends.Informatio.. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C | 61.1 µin/in-°F | ISO 11359-2 |
Celanese Hostaform® LM90 POM, Specialty Hostaform« LM90 is a nominal 9 melt flow rate acetal copolymer which is capable of being permanently marked by a laser. Parts molded from Hostaform« LM90 can be laser marked with barcodes, identif.. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C | 61.1 µin/in-°F | ISO 11359-2 |
Celanese Hostaform® S 9364 POM, Impact Modified Hostaform« acetal copolymer grade S 9364 is highly impact modified grade for demanding applications. Hostaform« S 9364 provides a significant improvement in impact strength and flexibility over s.. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C | 61.1 µin/in-°F | ISO 11359-2 |
Celanese Hostaform® C 27021 XAP² ™ LS colored POM, UV Resistant
(Unverified Data**) PolyacetalcopolymerLow Emission UV stabilizedInformation provided by Celanese |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature 23.0 - 55.0 °C |
61.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-2 |
Polyplastics Duracon® NW-02 Acetal Co-polymer (POM), High sliding, Special lubricant, High sliding DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C | 61.1 µin/in-°F | dry; ISO 11359-1/-2 |
DSM Stanyl® TE300 PA46 Heat Stabilized |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C | 61.1 µin/in-°F | DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® 105F BK010 Nylon 66
(Unverified Data**) Unreinforced UV Stabilized Polyamide 66 Zytel 105F BK010 is a lubricated fast cycling weather resistant PA 66 resin. Zytel 105F BK010 contains finely dispersed carbon black.Information provided by D.. |