Thermal Properties Metric English Comments
Deflection Temperature at 8.0 MPa 60.0 - 100 °C
140 - 212 °F
Average value: 78.3 °C Grade Count:6
Overview of materials for Nylon 66/6, 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are incl..
Deflection Temperature at 8.0 MPa 60.0 - 235 °C
140 - 455 °F
Average value: 194 °C Grade Count:27
Overview of materials for Nylon 66/6, 40% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 40% Glass Fiber Reinforced". Specific grades with glass content between 35% and 44% are incl..
Deflection Temperature at 8.0 MPa 60.0 °C
140 °F
ISO 75-1/-2
Lanxess Durethan® BG 30 X 000000 Nylon 6, 30% Glass Fiber
PA 6, injection molding grade, 30% glass fibers/glass spheres, good surface, low warpage
Deflection Temperature at 8.0 MPa 60.0 °C
140 °F
ISO 75-1/-2
Lanxess Durethan® BG 30 X H2.0 901510 Nylon 6, 30% Glass Fiber
PA 6, injection molding grade, 30% glass fibers/glass spheres, good surface, good heat-ageing resistance
Deflection Temperature at 8.0 MPa 60.0 °C
140 °F
ISO 75-1/-2
Lanxess Durethan® BKV 115 H2.0 901510 Copolyamide, 15% Glass Fiber
CoPA, injection molding grade, 15% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 15, even in..
Deflection Temperature at 8.0 MPa 60.0 °C
140 °F
ISO 75-1/-2
Lanxess Durethan® BKV 15 000000 Copolyamide, 15% Glass Fiber
CoPA, injection molding grade, 15% glass fibers
Deflection Temperature at 8.0 MPa 60.0 °C
140 °F
ISO 75-1/-2
Lanxess Durethan® BKV 15 H2.0 901510 Copolyamide, 15% Glass Fiber
CoPA, injection molding grade, 15% glass fibers, good heat-ageing resistance
Deflection Temperature at 8.0 MPa 60.0 °C
140 °F
ISO 75-1, -2
Lanxess Durethan® BKV 215 000000 Nylon 6-Copolymer, Glass Fiber Reinforced, Impact Modified
PA 6-Copolymer, 15% glass fibers, injection molding impact modifiedInformation provided by LANXESS.
Deflection Temperature at 8.0 MPa 60.0 °C
140 °F
ISO 75-1/-2
Lanxess Durethan® BKV 215 901510 Copolyamide, 15% Glass Fiber
CoPA, injection molding grade, 15% glass fibers, elastomer-modified, higher impact and notched impact strength and also higher energy absorption under biaxial impact load than BKV 115, conditioning ..
Deflection Temperature at 8.0 MPa 60.0 °C
140 °F
ISO 75-1/-2
Lanxess Durethan® BKV 215 H2.0 901510 Copolyamide, 15% Glass Fiber
CoPA, injection molding grade, 15% glass fibers, elastomer-modified, higher impact and notched impact strength and also higher energy absorption under biaxial impact load than BKV 115, conditioning ..
Deflection Temperature at 8.0 MPa 60.0 °C
140 °F
ISO 75-1/-2
Lanxess Durethan® BKV 215 W1 902176 Copolyamide, 15% Glass Fiber
CoPA, injection molding grade, 15% glass fibers, elastomer-modified, weather-stabilized
Deflection Temperature at 8.0 MPa 60.0 °C
140 °F
ISO 75-1/-2
Lanxess Durethan® BKV 115 000000 Copolyamide, 15% Glass Fiber
CoPA, injection molding grade, 15% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 15, even in..
Deflection Temperature at 8.0 MPa 60.0 °C
140 °F
ISO 75-1/-2
EMS-Grivory Grivory® BG-15 PA6-GF15
Product description: Grilon BG-15 is a heat stabilized PA 6 injection molding grade with 15% glass fiber reinforcement. Grilon BG-15 has the following important properties: Good surface finishGood b..
Deflection Temperature at 8.0 MPa 60.0 °C
140 °F
ISO 75-1/-2
EMS-Grivory Grivory® BG-15 S PA6-GF15
Product description: Grilon BG-15 S is a heat stabilized PA6 injection molding grade with 15% glass fibers. Grilon BG-15 S has the following important properties: Excellent surface finishEasy flowin..
Deflection Temperature at 8.0 MPa 60.0 °C
140 °F
ISO 75-1/-2
EMS-Grivory Grivory® BG-15/2 PA6-GF15
Product description: Grilon BG-15/2 is a heat stabilized PA6 injection molding grade with 15% glass fibers. Grilon BG-15/2 has the following important properties: Good surface finishEasy processingG..
Deflection Temperature at 8.0 MPa 60.0 °C
140 °F
ISO 75-1/-2
EMS-Grivory Grivory® GM-4H PA*-MD40
Product description: Grivory GM-4H natural is a 40 % mineral reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copolyamide. G..
Deflection Temperature at 8.0 MPa 60.0 °C
140 °F
ISO 75-1/-2
EMS-Grivory Grivory® TSG-30/4 LF 15/1 PA666-(GF+Z)45
Information provided by EMS Grivory
Deflection Temperature at 8.0 MPa 60.0 °C
140 °F
ISO 75-1/-2
EMS-Grivory Grivory® TSGK-30/4 X PA666-(GF+GB)30
Product description: Grilon TSGK-30 X/4 is a heat stabilized PA 66 + PA 6 injection molding grade with a 30% reinforcement combination (glass fibers and glass beads). Grilon TSGK-30/4 X has the foll..
Deflection Temperature at 8.0 MPa 60.0 °C
140 °F
ISO 75-1/-2
EMS-Grivory Grivory® TSGZ-15 PA666-GF15
Product description: Grilon TSGZ-15 is a heat stabilized, normal viscosity, and impact modified PA66 + PA6 injection molding grade with 15% glass fibers. Grilon TSGZ-15 has the following important p..
Deflection Temperature at 8.0 MPa 60.0 °C
140 °F
ISO 75-1/-2
EMS-Grivory Grivory® TSM-30/2 PA666-MD30
Product description: Grilon TSM-30/2 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% mineral filler. Grilon TSM-30/2 has the following important properties: Excell..
Deflection Temperature at 8.0 MPa 60.0 - 70.0 °C
140 - 158 °F
Average value: 65.0 °C Grade Count:3
Overview of materials for Nylon 66/6, Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, Mineral Reinforced". Each property range of values reported is minimum and maximum values of..
Deflection Temperature at 8.0 MPa 60.0 °C
140 °F
ISO 75-1/-2
Lanxess Durethan® DP 2801 000000 Nylon 66
PA 66 injection molding grade, non-reinforced, UL 94V-2 off 0,75 mm (listed), GWFI: 960°C off 0.75 mm, GWIT: 775°C off 0,75 mm, halogen-free
Copyright © lookpolymers.com All Rights Reserved