Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 110 µm/m-°C

@Temperature 20.0 °C
61.1 µin/in-°F

@Temperature 68.0 °F
ISO data
BASF Capron® GR20 20% Glass-Filled Nylon 6 (Dry)  (discontinued **)
Capron GR20 is a 20% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aesthetics. It is also..
CTE, linear, Transverse to Flow 110 µm/m-°C
61.1 µin/in-°F
ISO 11359-2
Celanese Celanex® 2003HR PBT  (Unverified Data**)
Celanex 2003HR is an unfilled polybutylene terephthalate which has an excellent hydrolysis resistance, mechanical properties and processabilityHydrolytically stable / injectionInformation provided b..
CTE, linear, Transverse to Flow 110 µm/m-°C
61.1 µin/in-°F
ISO 11359-2
Celanese Celcon® LW25-S2 POM, Tribological  (Unverified Data**)
Celcon® LW25-S2 acetal copolymer is a low flow, improved toughness product formulated with a low level of silicone to reduce friction and improved wear resistance.Low wear/friction, silicone, low s..
CTE, linear, Transverse to Flow 110 µm/m-°C
61.1 µin/in-°F
ISO 11359-2
Celanese Hostaform® EC140XF POM, Specialty  (Unverified Data**)
Hostaform® EC140XF is a conductive ESD grade of acetal copolymer for applications requiring dissipation of static build-up. EC140XF has an improved resistance to aggressive fuel blends.electrosta..
CTE, linear, Transverse to Flow 110 µm/m-°C

@Temperature 20.0 °C
61.1 µin/in-°F

@Temperature 68.0 °F
ISO 11359-1/-2
DSM Akulon® Ultraflow™ K-FKGS6 Nylon 6-30% Glass Reinforced (European and Asian Grade) (Dry)  (discontinued **
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
CTE, linear, Transverse to Flow 110 µm/m-°C
61.1 µin/in-°F
ISO 11359-1/-2
Lanxess Pocan® S 1506 000000 PBT
PBT, non-reinforced, injection molding extrusion, impact modified
CTE, linear, Transverse to Flow 110 µm/m-°C

@Temperature -30.0 - 30.0 °C
61.1 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP WP004 PBT
LNP* LUBRICOMP* WP004 is a compound based on PBT resin containing 20% PTFE/Silicone. Added feature of this grade is: Wear Resistant.
CTE, linear, Transverse to Flow 110 µm/m-°C

@Temperature 23.0 - 80.0 °C
61.1 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics Xenoy® 6370 PBT+PC (Europe-Africa-Middle East)
XENOY 6370 is an impact modified semi-crystalline thermoplastic. blend with 30% glass fibre reinforcement offering toughness and ductility.
CTE, linear, Transverse to Flow 110 µm/m-°C

@Temperature 23.0 - 80.0 °C
61.1 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics Xenoy® XL1562 PBT+PC (Europe-Africa-Middle East)
XENOY XL1562 is an impact modified PBT+PC blend with outstanding chemical resistance, good UV stability and flow properties.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio..
CTE, linear, Transverse to Flow 110 µm/m-°C

@Temperature 20.0 °C
61.1 µin/in-°F

@Temperature 68.0 °F
ISO 11359-2
Polyplastics Tepcon M270 Acetal-copolymer (POM), High Fluidity, High Cycle
Information provided by PolyPlastics.
CTE, linear, Transverse to Flow 110 µm/m-°C

@Temperature 20.0 °C
61.1 µin/in-°F

@Temperature 68.0 °F
ISO 11359-1/-2
DSM Arnitel® EL740 Polyether Ester Elastomer (European and Asian Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
CTE, linear, Transverse to Flow 110 µm/m-°C

@Temperature 20.0 °C
61.1 µin/in-°F

@Temperature 68.0 °F
ISO 11359-1/-2
DSM Arnitel® EL740-H/A Injection Molding; Other Extrusion Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
CTE, linear, Transverse to Flow 110 µm/m-°C

@Temperature 20.0 °C
61.1 µin/in-°F

@Temperature 68.0 °F
ISO 11359-1/-2
DSM Arnitel® PL581 Polyether Ester Elastomer (European and Asian Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
CTE, linear, Transverse to Flow 110 µm/m-°C
61.1 µin/in-°F
ISO 11359-1/-2
DuPont Performance Polymers Delrin® 100PE BK602 Acetal (POM)  (Unverified Data**)
High Viscosity Acetal Homopolymer with Very Low Emissions Delrin 100PE BK602 (formerly DE20573) is a high viscosity acetal homopolymer an enhanced version of Delrin 100P with very low VOC emissions...
CTE, linear, Transverse to Flow 110 µm/m-°C
61.1 µin/in-°F
ISO 11359-2
Celanese Celcon® WR90Z POM, UV Resistant
Celcon« WR90Z is a standard nominal 9 melt flow rate based acetal copolymer stabilized to provide maximum ultraviolet radiation resistance in outdoor applications while retaining a good balance of ..
CTE, linear, Transverse to Flow 110 µm/m-°C
61.1 µin/in-°F
ISO 11359-2
Celanese Hostaform® C 9021 S1 POM, Tribological
Information provided by Celanese
CTE, linear, Transverse to Flow 110 µm/m-°C
61.1 µin/in-°F
ISO 11359-2
Celanese Hostaform® LGC90-QX POM, 26% Glass Reinforced
Preliminary Data Sheet26% long fiber glass filled, high strengthLong Fiber Reinforced Thermoplastic products may be processed using current standard injection molding machines having screw diameters..
CTE, linear, Transverse to Flow 110 µm/m-°C
61.1 µin/in-°F
ISO 11359-2
Celanese Hostaform® S 9362 XAP2 ™ POM, Impact Modified
Preliminary Data SheetDrying is suggested to help achieve low emission performance and to counter if material has contacted moisture through improper storage and handling.Information provided by Cel..
CTE, linear, Transverse to Flow 110 µm/m-°C
61.1 µin/in-°F
ISO 11359-2
Celanese Hostaform® S 9364LPB POM, Impact Modified
Preliminary Data SheetInformation provided by Celanese
CTE, linear, Transverse to Flow 110 - 220 µm/m-°C
61.1 - 122 µin/in-°F
Average value: 154 µm/m-°C Grade Count:17
Overview of materials for Polyether Ester Elastomer
This property data is a summary of similar materials in the MatWeb database for the category "Polyether Ester Elastomer". Each property range of values reported is minimum and maximum values of appr..
CTE, linear, Transverse to Flow 110 µm/m-°C
61.1 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® TR 55 LZ PA12/MACMI
Product description: Grilamid TR grades are transparent thermoplastic polyamides based on aliphatic and cycloaliphatic blocks. Grilamid TR 55 LZ offers a variety of interesting properties such as: c..
CTE, linear, Transverse to Flow 110 µm/m-°C
61.1 µin/in-°F
ISO 11359-2
Celanese Celcon® WR90Z POM, UV Resistant  (Unverified Data**)
Celcon® WR90Z is a standard nominal 9 melt flow rate based acetal copolymer stabilized to provide maximum ultraviolet radiation resistance in outdoor applications while retaining a good balance of ..
CTE, linear, Transverse to Flow 110 µm/m-°C
61.1 µin/in-°F
ISO 11359-2
Celanese Hostaform® C 9021 POM  (Unverified Data**)
Chemical abbreviation according to ISO 1043-1: POMGeneral purpose injection molding gradeInformation provided by Celanese
CTE, linear, Transverse to Flow 110 µm/m-°C
61.1 µin/in-°F
ISO 11359-2
Celanese Hostaform® S 9362 POM, Impact Modified  (Unverified Data**)
Hostaform® acetal copolymer grade S 9362 is an impact modified grade for applications requiring improved impact. Hostaform® S 9362 provides good impact strength while improving modulus and weld ..
CTE, linear, Transverse to Flow 110 µm/m-°C

@Temperature 23.0 - 55.0 °C
61.1 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-2
Polyplastics Duracon® M140-44/M140S Acetal Co-polymer (POM), Standard, High flow
DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O)..
CTE, linear, Transverse to Flow 110 µm/m-°C

@Temperature 23.0 - 55.0 °C
61.1 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-2
Polyplastics Duracon® NW-02 Acetal Co-polymer (POM), High sliding, Special lubricant, High sliding
DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O)..
CTE, linear, Transverse to Flow 110 µm/m-°C

@Temperature -30.0 - 100 °C
61.1 µin/in-°F

@Temperature -22.0 - 212 °F
ISO 11359-2
SABIC Innovative Plastics SABIC PPCOMPOUND 15T1040 PP
SABIC® PPcompound 15T1040 is a general purpose, talc filled, heat stabilized homopolymer polypropylene compound, suitable for injection molding applications. The IMDS ID is 16487994
CTE, linear, Transverse to Flow 110 - 140 µm/m-°C
61.1 - 77.8 µin/in-°F
Average value: 125 µm/m-°C Grade Count:10
Overview of materials for Acetal Copolymer, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Impact Modified". Each property range of values reported is minimum and maximum values..
CTE, linear, Transverse to Flow 110 µm/m-°C

@Temperature 23.0 - 60.0 °C
61.1 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics Valox® VX3608C PBT (Europe-Africa-Middle East)
VALOX VX3608C is an impact modified, flame retardant PBT+PC injection moulding resin. Application: electrical enclosures. This grade is 3607U with reduced oxygen index.This data was supplied by SABI..
Copyright © lookpolymers.com All Rights Reserved