Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Dielectric Strength = 30.0 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 30.0 kV/mm
762 kV/in
Dry; IEC 60243
Polimeri Europa Sinkral® C 442 ABS Resin
Sinkral C 442 is a heat resistant injection molding grade offering good flow and impact resistance together with excellent thermal stability during processing. Designation: Thermoplastic ISO 2580-AB..
Dielectric Strength 30.0 - 50.0 kV/mm
762 - 1270 kV/in
ASTM D149
Permabond TA439 Toughened Acrylic Adhesive
Permabond® TA439 is a two component structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some plastics. The typical fixture time of is 10-30 seconds. The fast f..
Dielectric Strength 30.0 kV/mm
762 kV/in
LG Chemical AF312A ABS, Flame Retardant
Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical..
Dielectric Strength 30.0 kV/mm
762 kV/in
IEC 60243-1
Menzolit Menzolit® BMC 0160 Unsaturated Polyester UP
BMC 0160 is a general purpose BMC for electrical applications. Typical applications are lamp housings, canopies, covers and similar components.Information Provided by Menzolit
Dielectric Strength 30.0 kV/mm
762 kV/in
IEC 60243-1
Menzolit Menzolit® BMC 1000 Unsaturated Polyester UP
BMC 1000 is a special BMC for hydrolysis resistant applications. The glass content is set to a level that provides sufficient mouldability with high strength and stiffness properties. Typical applic..
Dielectric Strength 30.0 kV/mm
762 kV/in
ASTM D149
Kuraray Genestarâ„¢ G1300H Nylon, 30% Glass Filled
Standard HB grade. Halogen free, following the standards that Br is less than 900ppm, Cl is less than 900ppm, and total of halogen amount (Br and Cl) is less than 1500ppm. It is suitable for use in ..
Dielectric Strength 30.0 kV/mm
762 kV/in
IEC 60243-1
Menzolit Menzolit® BMC 2300 Unsaturated Polyester UP
BMC 2300 is a special BMC with exceptional high fire retardancy. The glass content is set to a level that provides sufficient mouldability with high strength and stiffness properties. Fire retardanc..
Dielectric Strength 30.0 - 40.0 kV/mm
762 - 1020 kV/in
ASTM D149
Guarniflon PFA Perfluoroalkoxy Polymer
Fluorinated thermoplastic material, offers the advantages of being thermo-processed whilst at the same time having the properties of PTFE, with excellent chemical and mechanical resistance for appli..
Dielectric Strength 30.0 kV/mm
762 kV/in
IEC 60243
Teijin Panlite® L-1225Z100 Transparent and Weather Resistant grade Polycarbonate Resin
Conforms to SAE regulations. It is an injection molding grade that has slightly high fluidity, weather resistance and mold release property and is bluish-tinted to exhibit clear colorApplications:Co..
Dielectric Strength 30.0 kV/mm
762 kV/in
IEC 60243
Teijin Panlite® LV-2225L Standard (mold release/ice color grade) Polycarbonate Resin
Flame retardant and mold release grade with high fluidity, while maintaining intrinsic transparency of polycarbonate resin. It is suitable for thin wall injection moldings.Applications:Electric, ele..
Dielectric Strength 30.0 kV/mm
762 kV/in
ASTM D149
Samyang Triloy® 210NHF Polymer Alloy, Flame Retardancy (Non-Halogen)
Excellent impact, formability and weather resistance.210NHF is a flame retardant (non-halogen) grade.Applications: LCD TV Rear Cover (high flow)Information provided by Samyang.
Dielectric Strength 30.0 kV/mm
762 kV/in
ASTM D149
Unitika C300VN
Characteristics: Flame resistant, transparent (flame resistance: UL94 V0, 0.8 mm) High flowInformation provided by Unitika Ltd.
Dielectric Strength 30.0 kV/mm
762 kV/in
IEC 243
Vyncolit 2923 W Novolac Phenolic
Mineral filled phenolic molding compound with excellent heat resistance and dimensional stability.Information provided by Vyncolit, a Sumitomo Bakelite Group
Dielectric Strength 30.0 kV/mm
762 kV/in
IEC 60243-1
Vyncolit Neopreg Kinel® SK61 L5G Glass Fiber Reinforced Molding Compound
Epoxy based molding compound long glass fiber reinforced with excellent long term property retention over a wide temperature range and climate conditions. It is particular suited for over molding..
Dielectric Strength 30.0 kV/mm
762 kV/in
VDE 0303/4
Polyram RamTough PZ300G6 Polycarbonate, 30% Glass Fiber
30% Glass fiber reinforced polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind.
Dielectric Strength 30.0 kV/mm
762 kV/in
VDE 0303/4
Polyram RamTough PZ307G2 Polycarbonate, 10% Glass Fiber
10% glass fiber reinforced, UV stabilized polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind.
Dielectric Strength 30.0 kV/mm
762 kV/in
DIN VDE 0303, Part 2
Evonik Corporation Plexiglas® XT 0A000 (20070) Extruded Acrylic
Description: PLEXIGLAS® XT extruded acrylic has the following properties:absolutely colorless and clearbreak-resistant to impact-resistant (PLEXIGLAS RESIST®)unequalled resistance to weathering an..
Dielectric Strength 30.0 kV/mm
762 kV/in
Covestro Bayblend® FR 3001 Polycarbonate + ABS Blend
Key Features:Flame retarding agentUnfilledFlame retardantSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separat..
Dielectric Strength 30.0 kV/mm
762 kV/in
Covestro Bayblend® T 88-4N Polycarbonate/ABS Blend, 20% Glass Fiber
Contains 20% glass fiber reinforcement, high stiffness.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – ..
Dielectric Strength 30.0 kV/mm
762 kV/in
Covestro Makrolon® 2207 Polycarbonate, Injection Grade
Exceptionally good flow injection molding grade with easy mold release and UV stabilizer, for parts with a low wall thickness and long flow paths.Information provided by Bayer.As of 1 September 2015..
Dielectric Strength 30.0 kV/mm
762 kV/in
Covestro Makrolon® 6385 Polycarbonate, Injection Grade
Low viscosity, flame retardant injection molding grade with easy mold release, not available in transparent colors.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was sep..
Dielectric Strength 30.0 kV/mm
762 kV/in
Covestro Makrolon® 9425 Polycarbonate
High viscosity, flame retardant extrusion and injection molding grade with 20% standard glass fibers and easy mold release agent.Information provided by Bayer.As of 1 September 2015, Bayer MaterialS..
Dielectric Strength 30.0 kV/mm
762 kV/in
conditioned; IEC 60243-1
EMS-Grivory Grivory® ELX 50 HNZ TPA
Product description: Grilon ELX 50 H NZ is a high viscosity, heat stabilized, impact modified, thermoplastic PA6 elastomer for extrusion blow molding applications. Grilon ELX 50 H NZ has the followi..
Dielectric Strength 30.0 kV/mm
762 kV/in
IEC 243-1
CP-Polymer-Technik Wellamid® 6600 HW Nylon 66, Heat Stabilized, Conditioned
Information provided by CP-Polymer-Technik GmbH & Co. KG
Dielectric Strength 30.0 kV/mm
762 kV/in
IEC 243-1
CP-Polymer-Technik Wellamid® 6600/508 HWUVCP Nylon 66, Impact Modified, UV Stabilized, Heat Stabilized, Conditioned
Information provided by CP-Polymer-Technik GmbH & Co. KG
Dielectric Strength 30.0 kV/mm
762 kV/in
IEC 243-1
Azoty Tarnow™ Tarnamid® T-27 MS Polyamide 6 - Natural
Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.For uncolored parts produced by injection molding, contain including and demo..
Dielectric Strength 30.0 kV/mm
762 kV/in
Conditioned; CEI 60243-1
Addiplast Addinyl B2 ZV20 Nylon 6, 20% Glass Filled
Glass fiber reinforced, increased thermal aging stabilityInformation provided by Addiplast.
Dielectric Strength 30.0 kV/mm
763 kV/in
ASTM D149
Arlon 910-10X##-P1 0.010" (0.254 mm) Cured Self-fusing Silicone Tape
Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1” Wide Rectangular 1 inch wide, 10 mil thick, Gray, Rectangular cross-section, Self-fus..
Dielectric Strength 30.0 kV/mm
762 kV/in
IEC 60243-1
Celanese Celanex® 5202HF PBT, 15% Glass Reinforced
Celanex 5202HF is a 15% glass-filled polyester featuring improved surface gloss and high flow for long flow channels. A typical application is oven handles.Information provided by Celanese Corporat..
Dielectric Strength 30.0 kV/mm
762 kV/in
Conditioned; CEI 60243-1