Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 160 MPa | 23200 psi | ISO 2039-1 |
Murtfeldt Murinit® SP Polyphenylene Sulfide Thanks to the low fiber content and integrated solid lubricant, Murinit® SP offers an excellent combination of good slide and wear behavior, high strength, and dimensional stability – even at high.. |
|||
Ball Indentation Hardness | 160 MPa | 23200 psi | ISO 2039-1 |
Nilit FRIANYL A63 W-GV20 Nylon 6.6 for injection molding, 20% glass fiber reinforced Nylon 6.6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 160 MPa | 23200 psi | ISO 2039-1 |
Nilit FRIANYL B63 AL40 Nylon 6.6 for injection molding, 40% aluminum filled Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 160 MPa | 23200 psi | ISO 2039-1 |
Nilit FRIANYL B63 CV20 Nylon 6.6 for injection molding, 20% carbon fiber reinforced Nylon 6.6 for injection molding, good conductive and electrostatic properties.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 160 MPa | 23200 psi | ISO 2039-1 |
Quadrant EPP Ertacetal® H POM-H, extruded (ISO Data) Ertacetal H is Quadrant’s homopolymer acetal grade. It offers a higher mechanical strength, stiffness, hardness and creep resistance as well as a lower thermal expansion rate and often also a bette.. |
|||
Ball Indentation Hardness | 160 MPa | 23200 psi | ISO 2039-1 |
Quadrant EPP Ertalyte® TX PET + solid lubricant, extruded (ISO Data) Ertalyte TX is a polyethylene terephthalate compound incorporating a uniformly dispersed solid lubricant. Its specific formulation makes it a premium internally lubricated bearing-grade. Ertalyte TX.. |
|||
Ball Indentation Hardness | 160 MPa | 23200 psi | ISO 2039-1 |
Quadrant EPP Nylatron® GSM PA 6 + MoS2, cast (ISO Data) Nylatron GSM contains finely divided particles of molybdenum disulphide to enhance its bearing and wear behaviour without impairing the impact and fatigue resistance inherent to unmodified cast nylo.. |
|||
Ball Indentation Hardness | 160 MPa | 23200 psi | ISO 2039-1 |
Quadrant EPP Techtron® HPV PPS + solid lubricant, bearing grade, extruded (ISO Data) As a reinforced, internally lubricated PPS grade, Techtron HPV PPS demonstrates an excellent combination of properties including wear resistance, load-bearing capabilities and dimensional stability .. |
|||
Ball Indentation Hardness | 160 MPa | 23200 psi | ISO 2039-1 |
Nilit FRIANYL B63 FK 1020 Nylon 6 for injection molding, 10% glass fiber and 20% glass ball reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 160 MPa | 23200 psi | ISO 2039-1 |
Nilit FRIANYL C73 GV15 Nylon 6.6/6 for injection molding, 15% glass fiber reinforced Nylon 6.6/6 for injection molding, medium viscosity.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 160 MPa | 23200 psi | ISO 2039-1 |
Nilit FRIANYL C73 M-HS3005 Nylon 6.6/6 for injection molding, 30% mineral filled Nylon 6.6/6 for injection molding, medium viscosity, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 160 - 270 MPa | 23200 - 39200 psi | Average value: 223 MPa Grade Count:3 |
Overview of materials for Nylon 66, 20% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Carbon Fiber Filled". Specific grades with carbon fiber content between 15% and 24% are in.. |
|||
Ball Indentation Hardness | 160 MPa | 23200 psi | Hc 30; ISO 2039; partially |
Schwartz Technical Plastics LAMIGAMID® 310 Cast Polyamide 6, Dry Application: sheaves, wheels, rollers, mandrell segments, coupling parts, vibrator parts etc.Information provided by Schwartz Technical Plastics GmbH |
|||
Ball Indentation Hardness | 160 MPa | 23200 psi | Hc 30; ISO 2039; partially |
Schwartz Technical Plastics LAMIGAMID® 319 Cast Polyamide 6, Oil Filled, Dry Application: sheaves and wheels without additional bearings, sliding linersInformation provided by Schwartz Technical Plastics GmbH |
|||
Ball Indentation Hardness | 160 MPa | 23200 psi | DIN 2039 |
Wolf Kunststoff ZEDEX® ZX-750V5KF 055 Polymer Alloy. Fiber Reinforced Main Characteristics: Stiff; High elongation and yield stress; Low thermal expansion; Impact resistantApplications: Textile Machinery; Compressors; Hinges; Handling; Machine Tools; Automitve Technol.. |
|||
Ball Indentation Hardness | 160 MPa | 23200 psi | H 358/30; ISO 2039; DIN 53456 |
Zell-Metall Engineering Plastics Zellamid 250 (PA6.6) Zellamid® 250 is noted for its high temperature resistance and high tensile strength. It is the hardest and most rigid type of extruded Nylon. Main characteristics are high resistance to fuels, oil.. |
|||
Ball Indentation Hardness | 160 MPa | 23200 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® TR 30 nat PA* Product description: Grilamid TR 30 natural is a high purity transparent thermoplastic polyamide, based on aliphatic and cycloaliphatic monomers. Grilamid TR 30 natural offers outstanding properties.. |
|||
Ball Indentation Hardness | 160 MPa | 23200 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® TSG-15/4 PA666-GF15 Information provided by EMS Grivory |
|||
Ball Indentation Hardness | 160 MPa | 23200 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® TSG-50 FA PA666-GF50 Information provided by EMS Grivory |
|||
Ball Indentation Hardness | 160 MPa | 23200 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® TSG-50/4 FA PA666-GF50 Information provided by EMS Grivory |
|||
Ball Indentation Hardness | 160 MPa | 23200 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® TSGZ-15 PA666-GF15 Product description: Grilon TSGZ-15 is a heat stabilized, normal viscosity, and impact modified PA66 + PA6 injection molding grade with 15% glass fibers. Grilon TSGZ-15 has the following important p.. |
|||
Ball Indentation Hardness | 160 MPa | 23200 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® TR XE 4139 black 9231 PA* Product description: Grilamid XE 4139 black 9231 is an amorphous thermoplastic polyamide based on aliphatic, cycloaliphatic and aromatic monomers. Grilamid XE 4139 black 9231 contains a processing a.. |
|||
Ball Indentation Hardness | 160 MPa | 23200 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® TR XE 4139 black 9231 PA* Product description: Grilamid XE 4139 black 9231 is an amorphous thermoplastic polyamide based on aliphatic, cycloaliphatic and aromatic monomers. Grilamid XE 4139 black 9231 contains a processing a.. |
|||
Ball Indentation Hardness | 160 MPa | 23200 psi | value at 30 sec.; ISO 2039-1 |
CENTROPLAST CENTROMID 6.6 FG Polyamide 6.6, Food Grade This material has good hardness, wear resistance, abrasion strength and impact strength.Information provided by CENTROPLAST Engineering Plastics GMBH |
|||
Ball Indentation Hardness | 160 MPa | 23200 psi | value at 30 sec.; ISO 2039-1 |
CENTROPLAST CENTROLYTE ZX Polyethylene terephthalate with lubricant This material's solid lubricant additive has good sliding properties, and is well suited for high load, dry running situations. Possible uses include precision plain bearings, plug connectors, r.. |
|||
Ball Indentation Hardness | 160 MPa | 23200 psi | DAM; H 961/30; ISO 2039-1 |
DuPont Performance Polymers Zytel® 101 NC010 Nylon 66
(Unverified Data**) Unreinforced Polyamide 66Zytel 101 NC010 is a general purpose polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers |
|||
Ball Indentation Hardness | 160 - 170 MPa | 23200 - 24700 psi | Average value: 167 MPa Grade Count:6 |
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Unreinforced". Each property range of values reported is minimum and m.. |
|||
Ball Indentation Hardness | 160 MPa @Load 36.5 kg, Time 30.0 sec |
23200 psi @Load 80.5 lb, Time 0.00833 hour |
ISO 2039-1 |
Styrolution Luran® 348 Q Crystal Clear Transparent 77850 SAN Description: Highly transparent grade with low natural color.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Ball Indentation Hardness | 160 MPa @Load 98.0 kg, Time 30.0 sec |
23200 psi @Load 216 lb, Time 0.00833 hour |
ISO 2039-1 |
BASF Ultradur® B 4300 G2 FC 10% Glass Filled PBT Description: The BASF Ultradur® FC (Food Contact) grades enable the industry to develop products for food contact applications which are in compliance with multiple regional food contact regulation.. |