EMS-Grivory Grivory® BS PA6

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer EMS-Grivory (EMS-CHEMIE)
Trade Name Grivory®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Grivory Grivory® BS PA6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product description: Grilon BS is an unreinforced, heat stabilized standard PA6 injection molding grade with normal melt viscosity. Grilon BS has the following important properties: Good flow behaviorEasy processingLight self-color Grilon BS has wide variety of applications in all market sectors, automotive, electrical, leisure and sport, e. g. suitable for clips, covers, housings.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ISO 1183
Water Absorption 9.0 %
9.0 %
ISO 62
Moisture Absorption 3.00 %
3.00 %
ISO 62
Linear Mold Shrinkage, Flow 0.010 cm/cm
0.010 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.013 cm/cm
0.013 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Ball Indentation Hardness 55.0 MPa
7980 psi
conditioned; ISO 2039-1
120 MPa
17400 psi
dry; ISO 2039-1
Tensile Strength, Yield 40.0 MPa
5800 psi
dry; ISO 527-1/-2
80.0 MPa
11600 psi
dry; ISO 527-1/-2
Elongation at Break 15 %
15 %
dry; ISO 527-1/-2
15 %
15 %
dry; ISO 527-1/-2
>= 50 %
>= 50 %
conditioned; ISO 527-1/-2
Elongation at Yield 4.0 %
4.0 %
dry; ISO 527-1/-2
15 %
15 %
conditioned; ISO 527-1/-2
Tensile Modulus 1.00 GPa
145 ksi
conditioned; ISO 527-1/-2
3.00 GPa
435 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched NB
NB
dry; ISO 179/1eU
NB
NB
conditioned; ISO 179/1eU
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
dry; ISO 179/1eA
3.00 J/cm²
14.3 ft-lb/in²
conditioned; ISO 179/1eA
0.400 J/cm²

@Temperature 30.0 °C
1.90 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
0.500 J/cm²

@Temperature 30.0 °C
2.38 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 80.0 µm/m-°C
44.4 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 80.0 µm/m-°C
44.4 µin/in-°F
ISO 11359-1/-2
Melting Point 222 °C
432 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 70.0 - 90.0 °C
158 - 194 °F
long term; EMS
180 °C
356 °F
short term; EMS
Deflection Temperature at 0.46 MPa (66 psi) 175 °C
347 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
conditioned; IEC 60093
1.00e+13 ohm-cm
1.00e+13 ohm-cm
dry; IEC 60093
Surface Resistance 1.00e+11 ohm
1.00e+11 ohm
IEC 60093
Dielectric Strength 27.0 kV/mm
686 kV/in
conditioned; IEC 60243-1
30.0 kV/mm
762 kV/in
dry; IEC 60243-1
Comparative Tracking Index 600 V
600 V
dry; IEC 60112
600 V
600 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Automotive Interior
Powertrain and Chassis
Electricals & Electronics Electrical appliances
Form Granules
Industry & Consumer goods Housewares
Mechanical Engineering
Sports & Leisure
Processing Injection Molding
Product Attributes Nucleated