Henkel Hysol EA 9395 Paste Adhesive System

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Henkel
Trade Name Hysol
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Henkel Hysol EA 9395 Paste Adhesive System.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Two-part, nonmetallic-filled version of Hysol EA 9394.Applications: Potting Structural Repair Composite Bonding
Physical Properties Metric English Comments
Storage Temperature 25.0 °C
77.0 °F
Mechanical Properties Metric English Comments
Tensile Strength 55.7 MPa
8080 psi
Elongation at Break 2.6 %
2.6 %
Tensile Modulus 4.90 GPa
711 ksi
Compressive Strength 96.6 MPa
14000 psi
Compressive Modulus 2.95 GPa
428 ksi
Adhesive Bond Strength 15.9 MPa

@Temperature -55.0 °C
2310 psi

@Temperature -67.0 °F
Tensile Lap Shear
16.6 MPa

@Temperature 93.0 °C
2410 psi

@Temperature 199 °F
Tensile Lap Shear
27.6 MPa

@Temperature 25.0 °C
4000 psi

@Temperature 77.0 °F
Tensile Lap Shear
Peel Strength 2.80 kN/m
16.0 pli
Bell Peel
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 177 °C
351 °F
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 66.0 °C
1.00 hour

@Temperature 151 °F
7200 - 10100 min

@Temperature 25.0 °C
120 - 168 hour

@Temperature 77.0 °F
Pot Life 100 min
100 min
Descriptive Properties Value Comments
Consistency Thixotropic
Form 2 parts
Mix Ratio, Part A:Part B 100:17
Peel Strength Low