Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 3.00 J/cm² | 14.3 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics Lexan® 943A PC (Europe-Africa-Middle East) LEXAN 943A is a medium viscosity flame retardant, UV-stabilized grade. UL-94 V0 listed and available in transparent and tints. |
|||
Charpy Impact, Notched | 3.00 J/cm² | 14.3 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® CFR9712 PC COPOLYMER (Europe-Africa-Middle East) Lexan* CFR9712 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 2.0 mm and high flow capability. .. |
|||
Charpy Impact, Notched | 3.00 J/cm² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HPX8R PC Copolymer (Asia Pacific) Very high flow specialty polycarbonate with outstanding processability and ductility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 o.. |
|||
Charpy Impact, Notched | 3.00 J/cm² | 14.3 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® SLX2231T PC Copolymer (Asia Pacific) Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors |
|||
Charpy Impact, Notched | 3.00 - 3.00 J/cm² @Temperature -20.0 - -20.0 °C |
14.3 - 14.3 ft-lb/in² @Temperature -4.00 - -4.00 °F |
Average value: 3.00 J/cm² Grade Count:1 |
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Ultra High Molecular Weight". Each property range of values reported i.. |
|||
Charpy Impact, Notched | 3.00 J/cm² | 14.3 ft-lb/in² | ISO 179 |
Menzolit Menzolit® BMC 0390 Unsaturated Polyester UP BMC 0390 is a low profile DMC/BMC. Because of its low shrinkage, the material shows good surface quality as well as very low warpage. The product is suitable for applications if a better surface qua.. |
|||
Charpy Impact, Notched | 3.00 J/cm² | 14.3 ft-lb/in² | ISO 179 |
Menzolit Menzolit® BMC 0900 Unsaturated Polyester UP BMC 0900 is a special BMC used in a chemically aggressive environment. The glass content is set to a level that combines good mould ability with good strength and stiffness properties. Typical appli.. |
|||
Charpy Impact, Notched | 3.00 J/cm² | 14.3 ft-lb/in² | |
LATI Latiblend 5262 PP Homopolymer/PA6 Blend based on Polypropylene homopolymer (PPh) / Polyamide 6 (PA6). Unfilled. High impact resistance. Very good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; No.. |
|||
Charpy Impact, Notched | 3.00 J/cm² | 14.3 ft-lb/in² | |
LATI Latigea B01 I8 Bio-Polymer Bio-Polymer (PLA, PHB, ...). Unfilled. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p... |
|||
Charpy Impact, Notched | 3.00 J/cm² | 14.3 ft-lb/in² | ISO 179/1eA |
Solvay TECHNYL® B 230 PA66/6, Conditioned Description: Unreinforced and modified copolyamide 66/6, with high flexibility and improved impact resistance, for injection molding.Available in: Asia Pacific and EuropeProduct Applications: TECHN.. |
|||
Charpy Impact, Notched | 3.00 J/cm² | 14.3 ft-lb/in² | ISO 179/1eA |
Solvay TECHNYL® B 238 Black 21 N PA66/6, Conditioned Description: Unreinforced and modified copolyamide 66/6, heat stabilized, with improved impact resistance, for injection molding.Available in: EuropeProduct Applications: TECHNYL B 238 is particular.. |
|||
Charpy Impact, Notched | 3.00 J/cm² | 14.3 ft-lb/in² | ISO 179 |
Teijin Panlite® AD-5503 Optical Use Polycarbonate Resin High fluidity grade for optical media that provides low optical distortion moldings. Impurities in pellets are severely controlled, and resulting high quality is obtaining good reputation.Applicatio.. |
|||
Charpy Impact, Notched | 3.00 J/cm² | 14.3 ft-lb/in² | ASTM D256 |
Plenco 08225 Polyester BMC, Compression Molded PLENCO 08225 is a renumber of PlasGlas 20215. PLENCO 08225 is a 15% glass-filled polyester bulk molding compound characterized as a medium strength electrical grade, but has many outstanding propert.. |
|||
Charpy Impact, Notched | 3.00 J/cm² | 14.3 ft-lb/in² | ISO 179 |
Polyram Polytron A60N01 Nylon 6.6, 60% Long Fiber Glass 60% Long fiber glass reinforced natural Nylon 6.6, heat stabilized, for injection molding.Information provided by Polyram. |
|||
Charpy Impact, Notched | 3.00 J/cm² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
ISO 179-1 |
Total XSene® 55060 High Density Polyethylene - Blow Molding HDPE 55060 is a semi high molecular weight (SHMW) high density polyethylene with outstanding Environmental Stress Crack Resistance and rigidity. It has been specifically designed for the manufactur.. |
|||
Charpy Impact, Notched | 3.00 J/cm² @Temperature 23.0 °C |
14.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6600 GV 35 HWCP 35% Glass Fiber Nylon 66, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact, Notched | 3.00 J/cm² | 14.3 ft-lb/in² | ISO 179/1eU |
DSM Stanyl® TW371 (COND) Nylon 46 Heat Stabilized, PTFE Lubricated (North America) Information provided by DSM Engineering Plastics. |
|||
Charpy Impact, Notched | 3.00 J/cm² @Temperature 30.0 °C |
14.3 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® TSGL-40/4 nat PA666-GF40 Product description: Grilon TSGL-40/4 natural is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 40% long glass fibers. Grilon TSGL-40/4 natural is characterized by the following .. |
|||
Charpy Impact, Notched | 3.00 J/cm² | 14.3 ft-lb/in² | dry; ISO 179/1eA |
EMS-Grivory Grivory® XE 5107 (GVL-5H V0) PA*-GF50 Product description: Grivory XE 5107 black 9915 is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide. The product is flame retarded and reinf.. |
|||
Charpy Impact, Notched | 3.00 J/cm² @Temperature 23.0 °C |
14.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
BASF Ultramid® A3XZG5 BK 23187 25% Glass Filled PA66 FR (Conditioned) Description: Impact-modified, 25% glass-fiber reinforced injection-molding grade with improved flame retardance and enhanced long-term stability. Flame retardant based on red phosphorus; for compone.. |
|||
Charpy Impact, Notched | 3.00 - 7.00 J/cm² | 14.3 - 33.3 ft-lb/in² | Average value: 4.84 J/cm² Grade Count:16 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced". Each property range of values reported is mi.. |
|||
Charpy Impact, Notched | 3.00 J/cm² | 14.3 ft-lb/in² | Conditioned; ISO 179/1eA |
Solvay Technyl® A 402 H1 Nylon 66 Unreinforced, very high viscosity, heat stabilized, for extrusion and injection molding. TECHNYL® A 402 H1 offers three main advantages: high impact resistance at low humidity levels, good rigidit.. |