Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 70.0 °C | 158 °F | Recommended continuous use |
Rogers Corporation Poron® 4701-30-15 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h.. |
|||
Maximum Service Temperature, Air | 70.0 °C | 158 °F | Constant use; SAE J-2236 |
Rogers Corporation Poron® 4701-30-20064 P Urethane Foam, Very Soft, Supported with Clear Polyester Film Very soft, easily compressed for use where flexibility is a key requirement. Contains PET film reinforcement. Standard available thickness 0.064"Features and Benefits of PORON Products: Excelle.. |
|||
Maximum Service Temperature, Air | 70.0 °C | 158 °F | Constant use; SAE J-2236 |
Rogers Corporation Poron® 4701-30-25037 P Urethane Foam, Very Soft, Supported with Clear Polyester Film Very soft, easily compressed for use where flexibility is a key requirement. Standard available thickness range from 0.021"Features and Benefits of PORON Products: Excellent compression set resi.. |
|||
Maximum Service Temperature, Air | 70.0 - 85.0 °C | 158 - 185 °F | ISO.75 DN.53461 |
Polimersan Plastics POLIPOLEN® (Polyethylene) HD-PE 300 PE 300: Polyethylene with high density. POLIPOLEN® PE (POLYETHYLENE) is maintained from coke oven gas or from natural gas or from Ethene or Ethane which is produced by cracking of petroleum. Monom.. |
|||
Maximum Service Temperature, Air | <= 70.0 °C | <= 158 °F | |
Pearl Engineering PEPLPET B-109JS PET Sheet Grade Used mainly for 5 to 20 liter mineral water containers |
|||
Maximum Service Temperature, Air | 70.0 °C | 158 °F | |
Abatron 80056 A/B Filled Potting Compound
(discontinued **) Neutral gray liquid epoxy to bond new to old concrete and for wet surfaces. 100/43 ratio.Information provided by Abatron. |
|||
Maximum Service Temperature, Air | 70.0 °C | 158 °F | |
Parker Chomerics SOFT-SHIELD® 4000 Low Closure Force, Foam Core EMI Gasket Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu.. |
|||
Maximum Service Temperature, Air | 70.0 °C | 158 °F | |
LATI Latamid SP1 PA 6.10 Polyamide 6.10 (PA6.10). Unfilled. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici .. |
|||
Maximum Service Temperature, Air | 70.0 °C | 158 °F | Constant use |
Saint-Gobain Korel® K20 Very Soft Micro-cellular Polyurethane Foam Description: The Korel® series micro-cellular polyurethane foams are offered in a broad range of properties, making them ideal for a variety of gasketing and energy absorption needs. Korel® mi.. |
|||
Maximum Service Temperature, Air | 70.0 °C | 158 °F | Continuous use |
Polyram PlusTek PA801 Nylon 6.6 Copolymer for Injection Molding, Impact Modified Impact modified Nylon 6.6 copolymer for injection molding application.Information provided by Polyram. |
|||
Maximum Service Temperature, Air | 70.0 °C | 158 °F | Continuous use |
Polyram PlusTek PA804 Nylon 6.6 for Injection Molding, Impact Modified Impact modified Nylon 6.6 for injection molding application.Information provided by Polyram. |
|||
Maximum Service Temperature, Air | 70.0 °C | 158 °F | |
Trelleborg Z800 Commercial SBR Rubber Styrene-butadiene Rubber is a co-polymer of styrene and butadiene.PropertiesIts general properties are similar to those of natural rubber, but it is more resistant to aging and temperature, and like.. |
|||
Maximum Service Temperature, Air | 70.0 °C | 158 °F | ASTM D 3575 |
Eurofoam Evacell EVA 50/S EVA + NR Foam Foamed polyethylene charged with EVA, with extremely fine cells, excellent elasticity, resilience and mechanical resistance. It can be thermoformed several times. It has completely closed cells, di.. |
|||
Maximum Service Temperature, Air | 70.0 °C | 158 °F | ASTM D 3575 |
Eurofoam Polycell PE 30 Polyethylene Foam Closed-cell polyethylene foam. Extruded reticulated pieces. Excellent physical properties both for active and static uses. Adjustable softness, elasticity, thermal deformation, shock absorbing. Use.. |
|||
Maximum Service Temperature, Air | 70.0 °C | 158 °F | |
Abatron AboCoat 8709-2 A/B Carbon-Filled Electrically Conductive Epoxy Compound AboCoat 8709-2 A/B is a high-solid carbon-epoxy coating with various conductivity ranges widely used in silk-screening. |
|||
Maximum Service Temperature, Air | 70.0 °C | 158 °F | |
3M 9416 Repositionable Tape 3M™ Repositionable Tapes are double coated tapes that are ideal for applications where one or both parts need to be repositioned or removed easily.Information provided by 3M |
|||
Maximum Service Temperature, Air | 70.0 °C | 158 °F | |
3M 9449S Repositionable Tape 3M™ Repositionable Tapes are double coated tapes that are ideal for applications where one or both parts need to be repositioned or removed easily.Information provided by 3M |
|||
Maximum Service Temperature, Air | 70.0 °C | 158 °F | |
Abatron AboCast/AboCure 4-4/50-12 Casting Epoxy for Tooling Standard casting compound for molds or patterns of any size, that can be machined with common metal working tools, engraving and reproduction molds.Main Advantages: FastBest rigid, chemical, and hea.. |
|||
Maximum Service Temperature, Air | 70.0 °C | 158 °F | Long Term |
3M 4492W Double Coated Polyethylene Foam Tape 3M™ Double Coated Polyethylene Foam Tapes 4462W, 4462B, 4466W and 4466B combine a conformable closed cell foam with a rubber adhesive that provides high initial adhesion to a variety of surfaces in.. |
|||
Maximum Service Temperature, Air | 70.0 °C | 158 °F | |
Parker Chomerics SOFT-SHIELD® 4005 Low Closure Force EMI Gasket Information provided by Chomerics |
|||
Maximum Service Temperature, Air | 70.0 °C | 158 °F | |
Trelleborg R660 Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Maximum Service Temperature, Air | 70.0 - 90.0 °C | 158 - 194 °F | long term; EMS |
EMS-Grivory Grivory® BR 40 W PA6 Product description: Grilon BR 40 W is a medium viscosity, plasticized PA6 extrusion grade. Grilon BR 40 W has the following important properties: High flexibilityHigh stiffness Grilon BR 40 W is us.. |
|||
Maximum Service Temperature, Air | 70.0 - 149 °C | 158 - 300 °F | Average value: 99.5 °C Grade Count:57 |
Overview of materials for Thermoset Polyurethane Foam, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane Foam, Unreinforced". Each property range of values reported is minimum and maximu.. |