| Category | Polymer , Thermoplastic , Nylon , Nylon 66 |
| Manufacturer | DuPont Performance Polymers |
| Trade Name | Zytel® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | DuPont Performance Polymers Zytel® 101L NC010 Nylon 66
(Unverified Data**).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 0.970 g/cc | 0.0350 lb/in³ | |
| 1.14 g/cc | 0.0412 lb/in³ | DAM; ISO 1183 | |
| Water Absorption | 8.5 % <br>@Thickness 2.00 mm |
8.5 % <br>@Thickness 0.0787 in |
DAM; Sim. to ISO 62 |
| Moisture Absorption | 2.60 % <br>@Thickness 2.00 mm |
2.60 % <br>@Thickness 0.0787 in |
DAM; Sim. to ISO 62 |
| Viscosity | 42820 cP <br>@Shear Rate 5000 1/s,<br> Temperature 300 °C |
42820 cP <br>@Shear Rate 5000 1/s,<br> Temperature 572 °F |
ISO 11403-1 -2 |
| 51190 cP <br>@Shear Rate 5000 1/s,<br> Temperature 290 °C |
51190 cP <br>@Shear Rate 5000 1/s,<br> Temperature 554 °F |
ISO 11403-1 -2 | |
| 61310 cP <br>@Shear Rate 5000 1/s,<br> Temperature 280 °C |
61310 cP <br>@Shear Rate 5000 1/s,<br> Temperature 536 °F |
ISO 11403-1 -2 | |
| 72990 cP <br>@Shear Rate 500 1/s,<br> Temperature 300 °C |
72990 cP <br>@Shear Rate 500 1/s,<br> Temperature 572 °F |
ISO 11403-1 -2 | |
| 95840 cP <br>@Shear Rate 500 1/s,<br> Temperature 290 °C |
95840 cP <br>@Shear Rate 500 1/s,<br> Temperature 554 °F |
ISO 11403-1 -2 | |
| 127400 cP <br>@Shear Rate 500 1/s,<br> Temperature 280 °C |
127400 cP <br>@Shear Rate 500 1/s,<br> Temperature 536 °F |
ISO 11403-1 -2 | |
| Viscosity Test | 150 cm³/g | 150 cm³/g | DAM; ISO 307 1157 1628 |
| Linear Mold Shrinkage, Flow | 0.014 cm/cm | 0.014 in/in | DAM; ISO 294-4 2577 |
| Linear Mold Shrinkage, Transverse | 0.014 cm/cm | 0.014 in/in | DAM; ISO 294-4 2577 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell M | 59 | 59 | 50%RH; ISO 2039-2 |
| 79 | 79 | DAM; ISO 2039-2 | |
| Hardness, Rockwell R | 108 | 108 | 50%RH; ISO 2039-2 |
| 121 | 121 | DAM; ISO 2039-2 | |
| Hardness, H358/30 | 85.0 MPa | 12300 psi | 50%RH; ISO 2039-1 |
| 180 MPa | 26100 psi | DAM; ISO 2039-1 | |
| Tensile Stress | 2.00 MPa <br>@Strain 0.135 %,<br> Time 3600 sec |
290 psi <br>@Strain 0.135 %,<br> Time 1.00 hour |
50%RH; isochronous; ISO 11403-1 -2 |
| 2.00 MPa <br>@Strain 0.157 %,<br> Time 36000 sec |
290 psi <br>@Strain 0.157 %,<br> Time 10.0 hour |
50%RH; isochronous; ISO 11403-1 -2 | |
| 2.00 MPa <br>@Strain 0.192 %,<br> Time 360000 sec |
290 psi <br>@Strain 0.192 %,<br> Time 100 hour |
50%RH; isochronous; ISO 11403-1 -2 | |
| 2.00 MPa <br>@Strain 0.305 %,<br> Time 3.60e+7 sec |
290 psi <br>@Strain 0.305 %,<br> Time 10000 hour |
50%RH; isochronous; ISO 11403-1 -2 | |
| 2.00 MPa <br>@Strain 0.239 %,<br> Time 3.60e+6 sec |
290 psi <br>@Strain 0.239 %,<br> Time 1000 hour |
50%RH; isochronous; ISO 11403-1 -2 | |
| 12.0 MPa <br>@Strain 1.95 %,<br> Time 3.60e+6 sec |
1740 psi <br>@Strain 1.95 %,<br> Time 1000 hour |
50%RH; isochronous; ISO 11403-1 -2 | |
| 12.0 MPa <br>@Strain 2.50 %,<br> Time 3.60e+7 sec |
1740 psi <br>@Strain 2.50 %,<br> Time 10000 hour |
50%RH; isochronous; ISO 11403-1 -2 | |
| 12.0 MPa <br>@Strain 1.52 %,<br> Time 360000 sec |
1740 psi <br>@Strain 1.52 %,<br> Time 100 hour |
50%RH; isochronous; ISO 11403-1 -2 | |
| 12.0 MPa <br>@Strain 1.25 %,<br> Time 36000 sec |
1740 psi <br>@Strain 1.25 %,<br> Time 10.0 hour |
50%RH; isochronous; ISO 11403-1 -2 | |
| 12.0 MPa <br>@Time 3600 sec,<br> Strain 1.02 % |
1740 psi <br>@Time 1.00 hour,<br> Strain 1.02 % |
50%RH; isochronous; ISO 11403-1 -2 | |
| 24.0 MPa <br>@Time 3600 sec,<br> Strain 3.29603 % |
3480 psi <br>@Time 1.00 hour,<br> Strain 3.29603 % |
50%RH; isochronous; ISO 11403-1 -2 | |
| 24.0 MPa <br>@Strain 3.91667 %,<br> Time 36000 sec |
3480 psi <br>@Strain 3.91667 %,<br> Time 10.0 hour |
50%RH; isochronous; ISO 11403-1 -2 | |
| Tensile Strength, Yield | 55.0 MPa | 7980 psi | 50%RH; ISO 527-1/-2 |
| 82.0 MPa | 11900 psi | DAM; ISO 527-1/-2 | |
| Elongation at Break | 25 % | 25 % | DAM; Nominal; ISO 527-1/-2 |
| >= 50 % | >= 50 % | 50%RH; Nominal; ISO 527-1/-2 | |
| Elongation at Yield | 4.5 % | 4.5 % | DAM; ISO 527-1/-2 |
| 4.5 % | 4.5 % | DAM; ISO 527-3 | |
| 25 % | 25 % | 50%RH; ISO 527-1/-2 | |
| Tensile Modulus | 1.40 GPa | 203 ksi | 50%RH; ISO 527-1/-2 |
| 3.10 GPa | 450 ksi | DAM; ISO 527-1/-2 | |
| 0.373 GPa <br>@Temperature 120 °C |
54.1 ksi <br>@Temperature 248 °F |
50%RH; ISO 11403-1 -2 | |
| 0.460 GPa <br>@Temperature 120 °C |
66.7 ksi <br>@Temperature 248 °F |
DAM; ISO 11403-1 -2 | |
| 0.945 GPa <br>@Temperature 40.0 °C |
137 ksi <br>@Temperature 104 °F |
50%RH; ISO 11403-1 -2 | |
| 2.769 GPa <br>@Temperature 40.0 °C |
401.6 ksi <br>@Temperature 104 °F |
DAM; ISO 11403-1 -2 | |
| 3.555 GPa <br>@Temperature -40.0 °C |
515.6 ksi <br>@Temperature -40.0 °F |
DAM; ISO 11403-1 -2 | |
| 4.493 GPa <br>@Temperature -40.0 °C |
651.7 ksi <br>@Temperature -40.0 °F |
50%RH; ISO 11403-1 -2 | |
| Flexural Modulus | 1.20 GPa | 174 ksi | 50%RH; ISO 178 |
| 2.80 GPa | 406 ksi | DAM; ISO 178 | |
| Shear Modulus | 0.154 GPa <br>@Temperature 160 °C |
22.3 ksi <br>@Temperature 320 °F |
50%RH; Dynamic; ISO 11403-1 -2 |
| 0.160 GPa <br>@Temperature 160 °C |
23.2 ksi <br>@Temperature 320 °F |
DAM; Dynamic; ISO 11403-1 -2 | |
| 0.180 GPa <br>@Temperature 120 °C |
26.1 ksi <br>@Temperature 248 °F |
DAM; Dynamic; ISO 11403-1 -2 | |
| 0.180 GPa <br>@Temperature 120 °C |
26.1 ksi <br>@Temperature 248 °F |
50%RH; Dynamic; ISO 11403-1 -2 | |
| 0.240 GPa <br>@Temperature 70.0 °C |
34.8 ksi <br>@Temperature 158 °F |
50%RH; Dynamic; ISO 11403-1 -2 | |
| 0.335 GPa <br>@Temperature 70.0 °C |
48.6 ksi <br>@Temperature 158 °F |
DAM; Dynamic; ISO 11403-1 -2 | |
| 0.880 GPa <br>@Temperature 20.0 °C |
128 ksi <br>@Temperature 68.0 °F |
50%RH; Dynamic; ISO 11403-1 -2 | |
| 0.919 GPa <br>@Temperature 20.0 °C |
133 ksi <br>@Temperature 68.0 °F |
DAM; Dynamic; ISO 11403-1 -2 | |
| 1.02 GPa <br>@Temperature -20.0 °C |
148 ksi <br>@Temperature -4.00 °F |
DAM; Dynamic; ISO 11403-1 -2 | |
| 1.04 GPa <br>@Temperature -20.0 °C |
151 ksi <br>@Temperature -4.00 °F |
50%RH; Dynamic; ISO 11403-1 -2 | |
| 1.11 GPa <br>@Temperature -50.0 °C |
161 ksi <br>@Temperature -58.0 °F |
DAM; Dynamic; ISO 11403-1 -2 | |
| 1.15 GPa <br>@Temperature -50.0 °C |
167 ksi <br>@Temperature -58.0 °F |
50%RH; Dynamic; ISO 11403-1 -2 | |
| Izod Impact, Notched (ISO) | 5.50 kJ/m² | 2.62 ft-lb/in² | DAM; ISO 180/1A |
| 12.0 kJ/m² | 5.71 ft-lb/in² | 50%RH; ISO 180/1A | |
| 3.00 kJ/m² <br>@Temperature -30.0 °C |
1.43 ft-lb/in² <br>@Temperature -22.0 °F |
50%RH; ISO 180/1A | |
| 5.50 kJ/m² <br>@Temperature -40.0 °C |
2.62 ft-lb/in² <br>@Temperature -40.0 °F |
DAM; ISO 180/1A | |
| 5.50 kJ/m² <br>@Temperature -30.0 °C |
2.62 ft-lb/in² <br>@Temperature -22.0 °F |
DAM; ISO 180/1A | |
| Izod Impact, Unnotched (ISO) | NB | NB | DAM; ISO 180/1U |
| NB | NB | 50%RH; ISO 180/1U | |
| 300 kJ/m² <br>@Temperature -30.0 °C |
143 ft-lb/in² <br>@Temperature -22.0 °F |
DAM; ISO 180/1U | |
| Charpy Impact Unnotched | NB | NB | DAM; ISO 179/1eU |
| NB | NB | 50%RH; ISO 179/1eU | |
| 40.0 J/cm² <br>@Temperature -30.0 °C |
190 ft-lb/in² <br>@Temperature -22.0 °F |
DAM; ISO 179/1eU | |
| NB <br>@Temperature -30.0 °C |
NB <br>@Temperature -22.0 °F |
50%RH; ISO 179/1eU |