Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Linear Mold Shrinkage, Transverse = 0.014 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.014 - 0.016 cm/cm
0.014 - 0.016 in/in
ISO 294-4
Celanese Celanex® 4309AR PBT  (Unverified Data**)
Information provided by Celanese
Linear Mold Shrinkage, Transverse 0.014 cm/cm
0.014 in/in
Euronil
Nilit Nilamid B3 H XB Unfilled, Impact Resistant PA6
Description: Nilamid B3 H XB is a high impact NYLON 6. The product has excellent impact properties above 0°C, combined with good maintaining mechanical characteristics. Application areas include au..
Linear Mold Shrinkage, Transverse 0.014 cm/cm

@Thickness 2.00 mm
0.014 in/in

@Thickness 0.0787 in
ISO 294-4
DuPont Performance Polymers Delrin® 510GR NC000 Acetal Homopolymer  (Unverified Data**)
Delrin® 510GR is a 10% glass reinforced acetal homopolymer for injection molding. It has high strength, stiffness, and high deflection temperature and excellent creep resistance.Information provide..
Linear Mold Shrinkage, Transverse 0.014 cm/cm
0.014 in/in
MPC method
Mitsui TPX® MBZ230 Methylpentene Copolymer, Filled, Opaque Grade  (discontinued **)
TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi..
Linear Mold Shrinkage, Transverse 0.014 cm/cm

@Thickness 2.00 mm
0.014 in/in

@Thickness 0.0787 in
DAM; ISO 294-4
DuPont Performance Polymers Zytel® FG42A NC010 Nylon 66  (Unverified Data**)
Zytel® FG42A NC010 is a high viscosity polyamide 66 resin for injection molding and extrusion. It has been developed for consideration into applications such as parts for the food industry.Informat..
Linear Mold Shrinkage, Transverse 0.014 - 0.018 cm/cm
0.014 - 0.018 in/in
LATI Latigray 47/1-01 CX/45 PP Copolymer
Radiopaque compound based on Polypropylene copolymer (PPc). Special mineral filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati ..
Linear Mold Shrinkage, Transverse 0.014 - 0.016 cm/cm

@Time 86400 sec
0.014 - 0.016 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRILOY UA200A PPA
LNP LUBRILOY* UA200A is a compound based on Polyphthalamide resin containing Aramid Fiber, Proprietary Lubricant. Added feature of this material is: Wear Resistant.
Linear Mold Shrinkage, Transverse 0.014 cm/cm

@Time 86400 sec
0.014 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Thermocomp P1000P PA 6 (Asia Pacific)
LNP* Thermocomp* P1000P is a compound based on Nylon 6 resin. Added features of this material include: Exceptional Processing.This data was supplied by SABIC-IP for the Asia Pacific region.
Linear Mold Shrinkage, Transverse 0.014 - 0.016 cm/cm
0.014 - 0.016 in/in
ISO DIS 294-4
Wellman Wellamid® T-731E-BK 10% Reinforced Abrasion Resistant Nylon 6
Description: Abrasion Resistant Nylon 6Information provided by Wellman.
Linear Mold Shrinkage, Transverse 0.014 cm/cm
0.014 in/in
ISO 294-4, 2577
EMS-Grivory Grivory® L 25 NZ ESD PA12
Product Description: Grilamid L 25 NZ ESD is a high viscosity, anti-static extrusion grade of Polyamide 12 (PA12). Grilamid L 25 NZ ESD is impact modified and heat stabilized. The inherent color of ..
Linear Mold Shrinkage, Transverse 0.014 cm/cm
0.014 in/in
ISO 294-4 2577
DuPont Performance Polymers Hytrel® 5553FG NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Linear Mold Shrinkage, Transverse 0.014 cm/cm
0.014 in/in
ISO 294-4 2577
DuPont Performance Polymers Sorona® 3301 NC010 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)&l
Unreinforced Renewably Sourced Polytrimethylene Terephthalate Sorona 3301 NC010 is an unreinforced polytrimethylene terephthalate resin containing 35% renewably sourced ingredients by weight with su..
Linear Mold Shrinkage, Transverse 0.014 cm/cm
0.014 in/in
DAM; ISO 294-4 2577
DuPont Performance Polymers Zytel® 70K20HSL NC010 Nylon 66  (Unverified Data**)
Kevlar® Fiber Reinforced Heat Stabilized Polyamide 66 Zytel 70K20HSL NC010 is a heat stabilized PA66 resin modified with Kevlar aramid fiber for excellent wear resistance.Information provided by Du..
Linear Mold Shrinkage, Transverse 0.014 cm/cm

@Thickness 2.00 mm
0.014 in/in

@Thickness 0.0787 in
DAM; ISO 294-4
DuPont Performance Polymers Zytel® E42A NC010 Nylon 66  (Unverified Data**)
Zytel® E42A is a high viscosity polyamide 66 for injection molding and extrusion. It has improved break resistance for thick-walled parts.Information provided by DuPont Performance Polymers
Linear Mold Shrinkage, Transverse 0.014 cm/cm
0.014 in/in
DAM; ISO 294-4 2577
DuPont Performance Polymers Zytel® FE3734 NC010 Nylon 612  (Unverified Data**)
Unreinforced Polyamide 612 Zytel FE3734 NC010 is an unreinforced lubricated polyamide 612 resin suitable for injection molding.Information provided by DuPont Performance Polymers
Linear Mold Shrinkage, Transverse 0.014 cm/cm
0.014 in/in
Eurotec
Eurotec® Tecodur® PB70 GB20 NL PBT, 20% glass bead reinforced, natural
Information provided by Eurotec®
Linear Mold Shrinkage, Transverse 0.014 cm/cm
0.014 in/in
Eurotec
Eurotec® Tecomid® NA40 MR15 NL IL PA6.6, 15% mineral filled, impact modified, natural
Information provided by Eurotec®
Linear Mold Shrinkage, Transverse 0.014 cm/cm
0.014 in/in
DAM; ISO 294-4 2577
DuPont Performance Polymers Zytel® 151L NC010 Nylon 612  (Unverified Data**)
Unreinforced Polyamide 612Information provided by DuPont Performance Polymers
Linear Mold Shrinkage, Transverse 0.014 cm/cm
0.014 in/in
DAM; ISO 294-4 2577
DuPont Performance Polymers Zytel® 153HSL NC010 Nylon 612  (Unverified Data**)
Unreinforced Heat Stabilized Polyamide 612 Information provided by DuPont Performance Polymers
Linear Mold Shrinkage, Transverse 0.014 cm/cm
0.014 in/in
DAM; ISO 294-4 2577
DuPont Performance Polymers Zytel® ST801 BK010A Nylon 66  (Unverified Data**)
Super Toughened Polyamide 66 Information provided by DuPont Performance Polymers
Linear Mold Shrinkage, Transverse 0.014 cm/cm

@Thickness 4.00 mm,
Time 86400 sec
0.014 in/in

@Thickness 0.157 in,
Time 24.0 hour
Arkema Group Pebax® 6333 SA 01 MED Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 6333 SA 01 MED is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This grade offers the highest quality and it is specially designed to meet t..
Linear Mold Shrinkage, Transverse 0.014 cm/cm

@Thickness 4.00 mm,
Time 86400 sec
0.014 in/in

@Thickness 0.157 in,
Time 24.0 hour
Arkema Group Pebax® 6333 SA 01 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 6333 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SA grade is specially designed to food uses.Information provided by Arkema ..
Linear Mold Shrinkage, Transverse 0.014 cm/cm
0.014 in/in
ISO 294-4
Azoty Tarnow™ Tarnamid® T-27 GF30 I Polyamide 6 - Glass Fiber Reinforced
30% Glass fiber reinforced, impact modified, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following mai..
Linear Mold Shrinkage, Transverse 0.014 cm/cm

@Thickness 2.00 mm
0.014 in/in

@Thickness 0.0787 in
ISO 294-4
Ascend Performance Materials Vydyne® 50BWFS Nylon 66, Conditioned (2.5% Moisture)
Vydyne® 50BWFS is a general purpose Nylon 66 resin. Available in natural. Designed for extrusion applications that do not require use of a highviscosity resin. This resin offers a well-balanced com..
Linear Mold Shrinkage, Transverse 0.014 cm/cm
0.014 in/in
ISO 294-4
Azoty Tarnow™ Tarnamid® T-30 MS Polyamide 6 - Natural
High viscosity extrusion grade for blown and flat films, including biaxial oriented films, also for extrusion of rods, pipes, plates, sheets, low diameter tubes and for injection molding of thick-wa..
Linear Mold Shrinkage, Transverse 0.014 cm/cm

@Thickness 2.00 mm
0.014 in/in

@Thickness 0.0787 in
ISO 294-4
Ascend Performance Materials Vydyne® 50BW Nylon 66, Dry as Molded
Vydyne® 50BW is a general purpose Nylon 66 resin. Available in natural. Designed for extrusion applications that do not require use of a high-viscosity resin. This resin offers a well-balanced comb..
Linear Mold Shrinkage, Transverse 0.014 cm/cm

@Thickness 2.00 mm
0.014 in/in

@Thickness 0.0787 in
ISO 294-4
Ascend Performance Materials Vydyne® ECO-315 Nylon 66/6, non-halogenated, ignition resistant, Conditioned
Vydyne® ECO315 is non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and has an Underwriters Laboratories UL 94 fla..
Linear Mold Shrinkage, Transverse 0.014 cm/cm
0.014 in/in
DAM; ISO 294-4 2577
DuPont Performance Polymers Zytel® 101F NC010 Nylon 66  (Unverified Data**)
Unreinforced Polyamide 66Zytel 101F NC010 is an internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont ..
Copyright © lookpolymers.com All Rights Reserved