Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, H358/30 | 180 MPa | 26100 psi | ISO 2039-1 |
SABIC Innovative Plastics Valox® 457 PBT (Europe-Africa-Middle East) VALOX 457 is a 6.5% glass fibre reinforced flame retarded PBT injection moulding resin. Applications: electrical and appliances industries. |
|||
Hardness, H358/30 | 180 MPa | 26100 psi | DAM; ISO 2039-1 |
DuPont Performance Polymers Zytel® 101L NC010 Nylon 66
(Unverified Data**) Unreinforced Polyamide 66Zytel 101L NC010 is a lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Hardness, H358/30 | 180 MPa | 26100 psi | DAM; ISO 2039-1 |
DuPont Performance Polymers Zytel® 101 NC010 Nylon 66
(Unverified Data**) Unreinforced Polyamide 66Zytel 101 NC010 is a general purpose polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers |
|||
Hardness, H358/30 | 180 MPa | 26100 psi | DAM; DS; ISO 2039-1 |
DuPont Performance Polymers Zytel® 101L BKB080 Nylon 66
(Unverified Data**) Unreinforced Polyamide 66Zytel 101L BKB080 is a lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |