Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.014 - 0.020 cm/cm
0.014 - 0.020 in/in
ASTM D955
PolyOne Versaflex™ HC MT222 Thermoplastic Elastomer (TPE)
Versaflex™ HC MT222 is an exceptionally clear, high performance TPE developed for medical tubing for healthcare. Versaflex™ HC MT222 has been specially formulated without the use of any plasticize..
Linear Mold Shrinkage, Flow 0.014 - 0.020 cm/cm
0.014 - 0.020 in/in
ASTM D955
PolyOne Versaflex™ OM 6258-1 Thermoplastic Elastomer (TPE)
Versaflex™ OM 6258-1 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Except..
Linear Mold Shrinkage, Flow 0.014 cm/cm

@Thickness 2.00 mm
0.014 in/in

@Thickness 0.0787 in
DAM; ISO 294-4
DuPont Performance Polymers Zytel® 101F BKB009 Nylon 66  (Unverified Data**)
Zytel® 101F BKB009 is an internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Performance Polymers
Linear Mold Shrinkage, Flow 0.014 cm/cm

@Thickness 2.00 mm
0.014 in/in

@Thickness 0.0787 in
DAM; ISO 294-4
DuPont Performance Polymers Zytel® 45HSB NC010 Nylon 66  (Unverified Data**)
Zytel® 45HSB NC010 is a high viscosity, heat stabilized polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers
Linear Mold Shrinkage, Flow 0.014 cm/cm

@Thickness 2.00 mm
0.014 in/in

@Thickness 0.0787 in
DAM; ISO 294-4
DuPont Performance Polymers Zytel® FG42A NC010 Nylon 66  (Unverified Data**)
Zytel® FG42A NC010 is a high viscosity polyamide 66 resin for injection molding and extrusion. It has been developed for consideration into applications such as parts for the food industry.Informat..
Linear Mold Shrinkage, Flow 0.014 - 0.018 cm/cm

@Thickness 3.20 mm
0.014 - 0.018 in/in

@Thickness 0.126 in
ASTM D955
LG Chemical KEYFLEX BT 1068D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
Linear Mold Shrinkage, Flow 0.014 - 0.018 cm/cm

@Thickness 3.20 mm
0.014 - 0.018 in/in

@Thickness 0.126 in
ASTM D955
LG Chemical LUPOL HG3200SK2 PP+MF20%, High Gloss
Description: Injection Molding, PP+MF20%, High GlossApplication: Electrical & Electronic PartsCAS: 9003-07-0 and 7727-43-7Information provided by LG Chemical
Linear Mold Shrinkage, Flow 0.014 cm/cm

@Thickness 3.17 mm
0.014 in/in

@Thickness 0.125 in
1/8" Section
Lucent Polymers CPP-310 Polypropylene, 10% Calcium Carbonate Filled, Impact Modified
Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc.
Linear Mold Shrinkage, Flow 0.014 cm/cm

@Thickness 3.17 mm
0.014 in/in

@Thickness 0.125 in
1/8" Section
Lucent Polymers TPP-310 Polypropylene, 10% Talc Filled, Impact Modified
Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc.
Linear Mold Shrinkage, Flow 0.014 - 0.017 cm/cm
0.014 - 0.017 in/in
LATI Latene® 7-V2 PP Homopolymer, Flame Retardant
Polypropylene homopolymer (PPh) based compound. UL94 V-2 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North A..
Linear Mold Shrinkage, Flow 0.014 cm/cm
0.014 in/in
Solvay TECHNYL® A 222 Black 1N PA66, DRY
Description: Unreinforced polyamide PA66, medium viscosity, heat stabilized, for injection molding, fast crystallization, for short cycles .Available in: EuropeProduct Applications: TECHNYL A 222 of..
Linear Mold Shrinkage, Flow 0.014 cm/cm

@Time 86400 sec
0.014 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP ML004S PP (Asia Pacific)
LNP* Lubricomp* ML004S is a compound based on Polypropylene resin containing PTFE. Added features of this material include: Internally Lubricated, Heat Stabilized.
Linear Mold Shrinkage, Flow 0.014 cm/cm

@Thickness 3.17 mm
0.014 in/in

@Thickness 0.125 in
ASTM D955
Techmer ES HiFill FR® PA6 FR IM
Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Flame Retardant and Impact ModifiedInformation provided by TP Composites, Inc.
Linear Mold Shrinkage, Flow 0.014 cm/cm

@Thickness 3.17 mm
0.014 in/in

@Thickness 0.125 in
ASTM D955
Techmer ES HiFill® PA6 X BN071 EL MB Nylon 6
Availability: North AmericaForms: PelletsAdditive: Lubricant and Nucleating AgentFeatures: Fast Molding Cycle, Good Processability, Lubricated and NucleatedTPCI# 1033102Information provided by TP Co..
Linear Mold Shrinkage, Flow 0.014 cm/cm
0.014 in/in
SABIC Method
SABIC Innovative Plastics LNP Thermocomp FX05032 PE (Europe-Africa-Middle East)
LNP* THERMOCOMP* FX05032 is a compound based on Polyethylene resin containing Proprietary Filler(s). Added features include : Foaming Agent for Polyolefins.This data was supplied by SABIC-IP for t..
Linear Mold Shrinkage, Flow 0.014 - 0.016 cm/cm
0.014 - 0.016 in/in
ASTM D955
Shinkong Synthetic Fibers Shinite® PP4410 PP, Fire Retardant
Information from Shinkong Synthetic Fibers Corp.
Linear Mold Shrinkage, Flow 0.014 - 0.017 cm/cm

@Thickness 3.20 mm
0.014 - 0.017 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics NORYL GTX GTX934 PPE+PA (Asia Pacific)
NORYL GTX934 is an unfilled GTX grade with improved processability and heat ageing performance.
Linear Mold Shrinkage, Flow 0.014 cm/cm

@Thickness 3.17 mm
0.014 in/in

@Thickness 0.125 in
ASTM D955
Techmer ES HiFill FR® PP FR-N X BKN001
Availability: North AmericaForms: PelletsFeatures: Flame Retardant Appearance: BlackInformation provided by TP Composites, Inc.
Linear Mold Shrinkage, Flow 0.014 - 0.016 cm/cm
0.014 - 0.016 in/in
ASTM D955
Shinkong Synthetic Fibers Shinite® PP4410 PP, Fire Retardant
Information from Shinkong Synthetic Fibers Corp.
Linear Mold Shrinkage, Flow 0.014 cm/cm

@Thickness 3.17 mm
0.014 in/in

@Thickness 0.125 in
ASTM D955
Techmer ES HiFill® POM 0212B Acetal
Availability: North AmericaForms: PelletsFeatures: Copolymer and High Specific GravityInformation provided by TP Composites, Inc.
Linear Mold Shrinkage, Flow 0.014 cm/cm

@Thickness 2.00 mm
0.014 in/in

@Thickness 0.0787 in
TPE Method
SCG Chemicals EL-Proâ„¢ P750J Polypropylene Injection Molding
Key Characteristics:Excellent clarityHigh productivityGood processability and stiffnessHigh glossOdorlessSafe for food contactRecommended Applications:Food container, utensilMedical parts such as sy..
Linear Mold Shrinkage, Flow 0.014 cm/cm

@Thickness 2.00 mm
0.014 in/in

@Thickness 0.0787 in
TPE Method
SCG Chemicals EL-Proâ„¢ P852J Polypropylene Injection Molding
Key Characteristics:Excellent productivityHigh clarityHigh stiffnessRecommended Applications:Clear food containerClear large size containerHousehold products and other articles that require high tra..
Linear Mold Shrinkage, Flow 0.014 cm/cm
0.014 in/in
ISO 294-4, 2577
EMS-Grivory Grivory® TSM-30/4 PA666-MD30
Information provided by EMS Grivory
Linear Mold Shrinkage, Flow 0.014 cm/cm

@Thickness 2.00 mm
0.014 in/in

@Thickness 0.0787 in
DAM; ISO 294-4
DuPont Performance Polymers Zytel® E42A NC010 Nylon 66  (Unverified Data**)
Zytel® E42A is a high viscosity polyamide 66 for injection molding and extrusion. It has improved break resistance for thick-walled parts.Information provided by DuPont Performance Polymers
Linear Mold Shrinkage, Flow 0.014 cm/cm
0.014 in/in
DAM; ISO 294-4 2577
DuPont Performance Polymers Zytel® FG101L NC010 Nylon 66  (Unverified Data**)
Unreinforced Polyamide 66 with Developed for Food Contact ApplicationsZytel FG101L NC010 is a lubricated polyamide 66 resin for injection molding. It has been developed for consideration into applic..
Linear Mold Shrinkage, Flow 0.014 - 0.018 cm/cm
0.014 - 0.018 in/in
on Tensile Bar; ISO 294
Eurostar Staramide BST42 PA6, Impact Modified, Injection Molded
BST42 is a Low Temperature Impact Modified Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
Linear Mold Shrinkage, Flow 0.014 cm/cm
0.014 in/in
ASTM D955
Clariant Renol PA112 Nylon 66, Nucleated
Data provided by Clariant Masterbatches
Linear Mold Shrinkage, Flow 0.014 cm/cm
0.014 in/in
ISO 294-4
Azoty Tarnow™ Tarnamid® T-29 Polyamide 6 - Natural
Medium-high viscosity extrusion grade for mono or multilayer blown film, including biaxial oriented films, also for production of monofilament; can be used for injection molding and compounding.Tarn..
Linear Mold Shrinkage, Flow 0.014 cm/cm
0.014 in/in
DAM; ISO 294-4 2577
DuPont Performance Polymers Zytel® 101F BKB009 Nylon 66  (Unverified Data**)
Unreinforced Polyamide 66Zytel 101F BKB009 is an internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont..
Linear Mold Shrinkage, Flow 0.014 cm/cm
0.014 in/in
SABIC Method
SABIC Innovative Plastics LNP Thermotuf P1000IX3 PA 6 (Europe-Africa-Middle East)
LNP* THERMOTUF* P1000IX3 is a compound based on PA6 resin containing Impact Modifier. Added features include : High Impact.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio..