Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.10 GPa | 450 ksi | |
Plastcom SLOVAMID 6 NGR PA6, basic type FeaturesPA 6 for injection moulding, modified for general use, with excellent manufacturing properties. Use: automotive, engineering, electrical and consumer-goods industry - electrical tools, faste.. |
|||
Tensile Modulus | 3.10 GPa | 450 ksi | ISO 527-1/-2 |
Quadrant EPP Ertacetal® H-TF POM-H, PTFE-filled, extruded (ISO Data) Ertacetal H-TF is a DELRIN® AF Blend, a combination of TEFLON® fibres evenly dispersed in a DELRIN acetal resin. Much of the strength that is inherent in Ertacetal H is retained. Some properties c.. |
|||
Tensile Modulus | 3.10 GPa | 450 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Edgetek® PF-05GF/000 FR MR Polysulfone (PSU) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Tensile Modulus | 3.10 GPa | 450 ksi | ISO.527 DIN.53455 |
Omnia Plastica Akulon® PET Arnite Omnialite Arnite is a relatively new semi-crystalline polymer developed for technical applications. It is suitable for mechanical parts which require dimensional stability and a low friction coefficient. Omni.. |
|||
Tensile Modulus | 3.10 GPa @Temperature 23.0 °C |
450 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Delrin® 150 NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 150 NC010 is a high viscosity acetal homopolymer for extrusion processes. It has excellent thermal stability, low die deposit, and enhanced crystallization for low porosity.Information pr.. |
|||
Tensile Modulus | 3.10 GPa @Temperature 23.0 °C |
450 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Delrin® 300CP NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 300CP is a medium-high viscosity acetal homopolymer with improved thermal stability and an outstanding balance of ease of processing and part performance.Information provided by DuPont Perf.. |
|||
Tensile Modulus | 3.10 GPa @Temperature 23.0 °C |
450 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Delrin® 500P BK602 Acetal Homopolymer
(Unverified Data**) Delrin® 500P BK602 is a general purpose medium viscosity black acetal homopolymer resin for injection molding. Delrin® 500P has improved processing thermal stability compared to Delrin® 500.Infor.. |
|||
Tensile Modulus | 3.10 GPa | 450 ksi | Dried; ISO 527 |
Manifattura Cattaneo PA 6 G Nylon Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Tensile Modulus | 3.10 GPa | 450 ksi | conditioned, 1 mm/min; ISO 527-1,-2 |
Lanxess Durethan® BKV 15 H.3 DUS008 000000 Nylon 6, 15% Glass Fiber PA 6, 15% glass fibers, injection molding, heat-ageing stabilizedInformation provided by LANXESS. |
|||
Tensile Modulus | 3.10 GPa | 450 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 402 Natural FA PA66, DRY Description: Unreinforced polyamide PA66, very high viscosity, for extrusion.Available in: Europe and North AmericaProduct Applications: TECHNYL® A 402 NATURAL FA offers three main advantages: hi.. |
|||
Tensile Modulus | 3.10 GPa | 450 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 402H1 Natural PA66, DRY Description: TECHNYL® A 402H1 is an unreinforced polyamide 66, very high viscosity, heat stabilized, for extrusion and injection molding. This product is available in natural color.Benefits: The .. |
|||
Tensile Modulus | 3.10 GPa | 450 ksi | |
Master Bond EP46HT-1 Epoxy For Serviceability Up To 600°F Description: Master Bond EP46HT-1 is a two component epoxy system for high performance structural bonding and sealing suitable for applications where resistance to temperatures from -100°F to +550°.. |
|||
Tensile Modulus | 3.10 GPa | 450 ksi | ASTM D638 |
Chevron Phillips MC3700 High Flow Crystal Polystyrene DescriptionChevron polystyrene resin MC3700 crystal is a free-flowing, crystal clear polystyrene injection molding compound, designed specifically for thin- and medium-walled or long-flow, difficult.. |
|||
Tensile Modulus | 3.10 GPa | 450 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Delrin® SC655 NC010 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer Developed for the Healthcare Industry Delrin SC655 is a medium viscosity acetal homopolymer developed for parts requiring high precision molding in the healthcare.. |
|||
Tensile Modulus | 3.10 GPa | 450 ksi | chs 0.2 in/min; ASTM D638 |
Diamond Polymers Centrex® 925 Injection Molding Grade Centrex 925 resin is a soft-flow, high-gloss, molding grade of Polycarbonate / ASA (acrylonitrile-styrene-acrylate) blend. It is an injection molding grade with a good balance of physical properties.. |
|||
Tensile Modulus | 3.10 GPa @Temperature 23.0 °C |
450 ksi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® FE3071 NC010 Nylon 66 Zytel® FE3071 NC010 is an intermediate viscosity polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 3.10 GPa | 450 ksi | ISO 527-1/-2 |
Covestro Makroblend® DP 2-7655 MBS162 Polycarbonate + PET, Mineral Filled Impact Grade Developmental product(PC+PET)-blendsimpact modifiedInjection molding grade 10% mineral filledAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new .. |
|||
Tensile Modulus | 3.10 GPa @Temperature 20.0 °C |
450 ksi @Temperature 68.0 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 103FHS NC010 Nylon 66
(Unverified Data**) Unreinforced Heat Stabilized Polyamide 66 Zytel 103FHS NC010 is a heat stabilized internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivi.. |
|||
Tensile Modulus | 3.10 GPa | 450 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 103HSL NC010 Nylon 66
(Unverified Data**) Unreinforced Heat Stabilized Polyamide 66 Zytel 103HSL NC010 is a heat stabilized lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 3.10 GPa | 450 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 45HSB NC010 Nylon 66
(Unverified Data**) Unreinforced Heat Stabilized Polyamide 66 Zytel 45HSB NC010 is a high viscosity heat stabilized polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Poly.. |
|||
Tensile Modulus | 3.10 GPa | 450 ksi | 1 mm/min; ISO 527 |
Eurostar Starflam BFR330A PA6, Glass Bead Reinforced, Flame Retardant, Injection Molded Starflam BFR330A is a Flame Retardant, Glass Bead Reinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Modulus | 3.10 GPa | 450 ksi | 1mm/min; ISO 527 |
BASF Ultramid® A27 E 01 PA66 (Dry) Ultramid A27 E 01 is a low-viscosity, general-purpose PA66 grade for compounding. It conforms to FDA requirements including, 21 CFR 177.1500,EU Directive 2002/72/EC, the German BfR recommendation ".. |
|||
Tensile Modulus | 3.10 GPa | 450 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® 22HSP Nylon 66, General Purpose, Heat Stabilized, DAM Availability:Asia PacificEuropeNorth America Additive:Lubricant Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood To.. |
|||
Tensile Modulus | 3.10 GPa | 450 ksi | 1 mm/min |
Arkema Group Oroglas® VM Acrylic, Injection Molding Grade
(discontinued **) OROGLAS VM is an injection molding grade with a medium heat resistance and easy flow.OROGLAS VM is particularly suitable to improve mold filling of technical parts.The VM L version has been speciall.. |
|||
Tensile Modulus | 3.10 GPa | 450 ksi | ISO 527-2 |
CENTROPLAST CENTROMID 6.6 Polyamide 6.6 This material has good hardness, wear resistance, abrasion strength and impact strength. It is used for bearing cages, sliding bearings and articulated joint blocks.Information provided by CENTROPL.. |