Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 5.50 kJ/m² @Temperature 23.0 °C |
2.62 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
DuPont Performance Polymers Crastin® LW9020FR BK851 PBT
(Unverified Data**) Crastin® LW9020FR BK851 is a 20% glass fiber reinforced, flame retardant, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional sta.. |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² @Temperature -40.0 °C |
2.62 ft-lb/in² @Temperature -40.0 °F |
ISO 180/1A |
Aardvark Polymers Aarlon® 2000 Rotational Molding Resin, DAM Aarlon® 2000 PA 6/6 is a high performance nylon for rotational molding applications. Aarlon® 2000 offers high heat capabilities with exceptional mechanical properties.Information provided by G.. |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² | 2.62 ft-lb/in² | ISO 180/1eA |
Solvay TECHNYLSTARâ„¢ S 218 MT PA6, 40% mineral filled, DRY Description: TechnylStar Polyamide, 40% mineral filled, heat stabilized, for injection molding. Characterized by a high fluidity of the melt.Available in: Asia Pacific and North AmericaProduct Appli.. |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² | 2.62 ft-lb/in² | ISO 180 |
Polyram PlusTek PA355M6 Nylon 6.6 for Injection Molding, 30% Mineral Filled, Flame Retardant 30% Minerals filled, flame retardant Nylon 6.6 for injection molding applications.Information provided by Polyram. |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² | 2.62 ft-lb/in² | ASTM D256 |
Tipco Tipcolene® FPT 30 PPC - 30% Talc Reinforced Polypropylene Copolymer Compound 30% Talc Reinforced PP CopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² @Temperature -20.0 °C |
2.62 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Total PPC 5660 Propylene, Heterophasic Copolymer ATOFINA Propylene 5660 is heterophasic copolymer. PPC 5660 is characterized by a medium fluidity offering a combination of ease of processing and good manufactured article properties in application.. |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² @Temperature -20.0 °C |
2.62 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Total PPC 9712 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 9712 is heterophasic copolymer. PPC 9712 is characterized by excellent impact resistance and antistatic properties and has been formulated to allow faster cycling through early de.. |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² | 2.62 ft-lb/in² | ISO 179 |
Total PPH 4042 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 4042 is a nucleated homopolymer.ApplicationATOFINA Polypropylene PPH 4042 has been developed for extrusion-thermoforming, providing improved rigidity and impact resistance .. |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² | 2.62 ft-lb/in² | 80x10x4; ISO 180/1A |
Eurostar Star L PA D51 PA6, Injection Molded Star L PA6 D51 is a 15% PTFE Lubricated Unreinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² | 2.62 ft-lb/in² | DAM; ISO 180/1A |
DuPont Performance Polymers Zytel® 103FHS BKB038 Nylon 66
(Unverified Data**) Unreinforced Heat Stabilized Polyamide 66 Zytel 103FHS BKB038 is a heat stabilized lubricated PA 66 resin for fast cycling.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² @Temperature -40.0 °C |
2.62 ft-lb/in² @Temperature -40.0 °F |
DAM; ISO 180/1A |
DuPont Performance Polymers Zytel® 103FHS NC010 Nylon 66
(Unverified Data**) Unreinforced Heat Stabilized Polyamide 66 Zytel 103FHS NC010 is a heat stabilized internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivi.. |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² | 2.62 ft-lb/in² | 80x10x4; ISO 179/1eA |
Eurostar Staramide RFM3353EM PA66/6, Glass/Mineral Fiber Reinforced, Injection Molding Starflam RFM3353EM is a Mineral Filled, Glass Fiber Reinforced Polyamide 66/ Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² @Temperature 23.0 °C |
2.62 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecomid® NA40 AR20 NL HS PA6.6, 20% aramid fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² | 2.62 ft-lb/in² | ISO 180/1A |
Addiplast Addilene H 220 M40 Polypropylene Homopolymer Mineral reinforced, improved rigidityInformation provided by Addiplast. |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² @Temperature -30.0 °C |
2.62 ft-lb/in² @Temperature -22.0 °F |
ISO 180/A |
BASF Ultramid® B3L PA6 (Dry) Ultramid B3L is an impact-modified, easy flowing injection molding PA6 grade for fast processing. |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² | 2.62 ft-lb/in² | ISO 179/1eA |
BLUESTAR BS130 Acetal Copolymer Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² | 2.62 ft-lb/in² | ISO Test |
BASF Ultradur B 4300 G3 BK5110 15% Glass Filled PBT Ultradur B4300 G3 is an easy flowing 15% glass reinforced grade of PBT for injection molding. It is suitable for industrial articles requiring high rigidity, toughness and dimensional stability. |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² | 2.62 ft-lb/in² | ISO Test |
BASF Ultramid® A3EG3 15% Glass Filled PA66 (Dry) Ultramid A3EG3 is a 15% glass fiber reinforced injection molding PA66 grade. It conforms to FDA requirements of 21 CFR 177.1500. |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² @Temperature 23.0 °C |
2.62 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
BASF Ultrason® S 3010 MR UN PSU Description: Unreinforced, higher viscosity injection molding and extrusion grade, tougher, with improved chemical resistance and demolding optimized. Abbreviated designation according to ISO 1043-1.. |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² @Temperature -30.0 °C |
2.62 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 180/1A |
DuPont Performance Polymers Minlon® 12T BKB100 Nylon 66
(Unverified Data**) 36% Mineral Reinforced Toughened Polyamide 66 Minlon 12T BKB100 is a 36% mineral reinforced toughened heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont Pe.. |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² | 2.62 ft-lb/in² | ISO 180/1A |
DuPont Performance Polymers Sorona® FG3015G NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data** 15% Glass Reinforced Renewably Sourced Polytrimethylene Terephthalate Developed for Food Contact Applications Sorona FG3015G NC010 is a 15% glass fiber reinforced polytrimethylene terephthalate resi.. |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² @Temperature -40.0 °C |
2.62 ft-lb/in² @Temperature -40.0 °F |
DAM; ISO 180/1A |
DuPont Performance Polymers Zytel® 101 NC010 Nylon 66
(Unverified Data**) Unreinforced Polyamide 66Zytel 101 NC010 is a general purpose polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² | 2.62 ft-lb/in² | DAM; ISO 180/1A |
DuPont Performance Polymers Zytel® 101F BKB009 Nylon 66
(Unverified Data**) Unreinforced Polyamide 66Zytel 101F BKB009 is an internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont.. |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² | 2.62 ft-lb/in² | ISO 180/1A |
Addiplast Addinyl B2 Nylon 6 Unreinforced, medium viscosityInformation provided by Addiplast. |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² | 2.62 ft-lb/in² | ISO 180/A |
Victrex® PEEK 150FC30 Easy Flow Product Description: High performance thermoplastic material, 30% reinforced with carbon fibre / graphite / PTFE PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding, easy .. |