Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.014 - 0.018 cm/cm | 0.014 - 0.018 in/in | ASTM D955 |
PolyOne Versaflex™ CL2050 Thermoplastic Elastomer (TPE) Versaflex™ CL2050 is an easy processing compound designed for use in applications where clarity and enhanced heat resistance are required. New Product. Commercial specifications have not been estab.. |
|||
Linear Mold Shrinkage, Flow | 0.014 - 0.020 cm/cm | 0.014 - 0.020 in/in | ASTM D955 |
PolyOne Versaflex™ HC MT222 Thermoplastic Elastomer (TPE) Versaflex™ HC MT222 is an exceptionally clear, high performance TPE developed for medical tubing for healthcare. Versaflex™ HC MT222 has been specially formulated without the use of any plasticize.. |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm | 0.014 in/in | Euronil |
Nilit Nilamid A3 H ZB High Impact PA66 Description: Nilamid A3 H ZB is high impact NYLON 66. The product maintains excellent impact properties, even at minus temperatures, whilst maintaining mechanical characteristics. Application areas .. |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm | 0.014 in/in | Euronil |
Nilit Nilamid B3 H ZA Unfilled, Low Temperature Impact Resistant PA6 Description: Nilamid B3 H ZA is a NYLON 6 with a low level of impact modification, allowing parts to be snap fitted in a dry-as-molded condition. It also has improved impact strength and elongation,.. |
|||
Linear Mold Shrinkage, Flow | 0.014 - 0.021 cm/cm | 0.014 - 0.021 in/in | ASTM D955 |
PolyOne Dynaflex™ G2711-1000-00 Thermoplastic Elastomer (TPE) Dynaflex™ G2711-1000-00 is an easy process compound designed for injection molding and extrusion applications that require FDA compliance. - Excellent Colorability - Good Ozone and UV Stability - O.. |
|||
Linear Mold Shrinkage, Flow | 0.014 - 0.015 cm/cm @Thickness 3.20 mm |
0.014 - 0.015 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUMID HI5003A PA6/PO, High Impact, High Flow, Good Paintablility Feature: Injection Molding, PA6/PO, High Impact, High Flow, Good PaintablilityApplication: Automotive Exterior PartsCAS No. 25038-54-4, 9010-79-1, 9003-07-0 and 14807-96-6Information provided by LG .. |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm | 0.014 in/in | ISO 294-4, 2577 |
Kuraray Genestarâ„¢ N1001A-M41 Nylon Low friction unreinforced injection grade. Main Features:Low friction coefficientHigh impact strengthExamples of applications are:Friction and wear applicationGear and wheel |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm | 0.014 in/in | ISO 294-4, 2577 |
Kuraray Genestarâ„¢ N1002A-M41 Nylon Low friction unreinforced injection grade. Main Features:Low friction coefficientLow wearExamples of applications are:Friction and wear applicationGear and wheel |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm @Thickness 3.17 mm |
0.014 in/in @Thickness 0.125 in |
1/8" Section |
Lucent Polymers 66-01 Nylon 66, General Purpose, Injection Grade Add "R" for Added ReleaseAdd "HU" for WeatherableTypical Properties, Dry as MoldedInformation provided by Lucent Polymers, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm @Thickness 3.17 mm |
0.014 in/in @Thickness 0.125 in |
1/8" Section |
Lucent Polymers CPP-110 Polypropylene Homopolymer, 10% Calcium Carbonate Filled Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm @Thickness 3.17 mm |
0.014 in/in @Thickness 0.125 in |
1/8" Section |
Lucent Polymers CPP-310 Polypropylene, 10% Calcium Carbonate Filled, Impact Modified Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm | 0.014 in/in | 60x60x2; 260°C / MT 80°C; 600 bar; ISO 294-4 |
Lanxess Pocan® DP 7102 000000 PBT, 32% Mineral PBT, 32% mineral, injection molding, LDSInformation provided by LANXESS. |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm | 0.014 in/in | |
Solvay TECHNYL® B 216 Natural D PA66/6, DRY Description: Unreinforced copolyamide 66/6, medium viscosity, for injection molding.Available in: EuropeProduct Applications: TECHNYL B 216 offers an excellent combination between impact resistance,.. |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm | 0.014 in/in | |
Solvay TECHNYL® B 218 Black 21 N PA66/6, DRY Description: Unreinforced copolyamide PA 66/6 , heat stabilized , medium viscosity, for injection molding.Available in: EuropeProduct Applications: TECHNYL® B 218 offers all of the primary proper.. |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm @Thickness 3.17 mm |
0.014 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® PA6 X BN071 EL MB Nylon 6 Availability: North AmericaForms: PelletsAdditive: Lubricant and Nucleating AgentFeatures: Fast Molding Cycle, Good Processability, Lubricated and NucleatedTPCI# 1033102Information provided by TP Co.. |
|||
Linear Mold Shrinkage, Flow | 0.014 - 0.020 cm/cm @Thickness 3.20 mm |
0.014 - 0.020 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Xenoy® 6620 PBT+PC (Asia Pacific) Impact modified, highly chemical resistant polyester/polycarbonate alloy.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm @Thickness 3.17 mm |
0.014 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® POM CO GC20 20% Glass Bead Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 20% Filler by WeightFeatures: CopolymerInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm @Thickness 3.17 mm |
0.014 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Luriblend® PA6 TSX10 Nylon 6 Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant (10%)Features: Lubricated and Good Wear ResistanceInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm @Thickness 3.17 mm |
0.014 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Plastiblend® PA6/6,6 L N Nylon 6/66 Availability: North AmericaForms: PelletsAdditive: Nucleating Agent and LubricantFeatures: Copolymer, Fast Molding Cycle, Nucleated and LubricatedProcessing Method: Injection MoldingInformation prov.. |
|||
Linear Mold Shrinkage, Flow | 0.014 - 0.017 cm/cm @Thickness 3.20 mm |
0.014 - 0.017 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX944 PPE+PA NORYL GTX944 is an unfilled GTX grade with improved processability and increased impact performance. |
|||
Linear Mold Shrinkage, Flow | 0.014 - 0.017 cm/cm @Thickness 3.20 mm |
0.014 - 0.017 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX944 PPE+PA (Europe-Africa-Middle East) NORYL GTX944 is an unfilled GTX grade with improved processability and increased impact performance. |
|||
Linear Mold Shrinkage, Flow | 0.014 - 0.018 cm/cm | 0.014 - 0.018 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX963 PPE+PA (Europe-Africa-Middle East) NORYL GTX963 is an unfilled impact modified material with excellent heat properties and good processability. |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm @Thickness 3.17 mm |
0.014 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill FR® PP FR-N X BKN001 Availability: North AmericaForms: PelletsFeatures: Flame Retardant Appearance: BlackInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm | 0.014 in/in | ASTM D955 |
Chase Plastics CP Pryme® NN100M2 (Dry) Nylon 66, Lubricated Features: Good chemical resistanceFast cycleDurableLubricatedSolvent resistantInjection moldingForm: PelletsInformation provided by Chase Plastics. |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm | 0.014 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® TSM-30/4 PA666-MD30 Information provided by EMS Grivory |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm | 0.014 in/in | DAM; ISO 294-4 2577 |
DuPont Performance Polymers Zytel® FG42L NC010 Nylon 66
(Unverified Data**) Unreinforced High Viscosity Polyamide 66 with Developed for Food Contact Applications Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm | 0.014 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Hytrel® RS R4275 BK316 Polyester Elastomer TPC-ET 55 Shore D Renewably Sourced High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm | 0.014 in/in | DAM; ISO 294-4 2577 |
DuPont Performance Polymers Zytel® 45HSB NC010 Nylon 66
(Unverified Data**) Unreinforced Heat Stabilized Polyamide 66 Zytel 45HSB NC010 is a high viscosity heat stabilized polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Poly.. |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm | 0.014 in/in | ISO 294-4 |
Azoty Tarnow™ Tarnamid® T-30 MS Polyamide 6 - Natural High viscosity extrusion grade for blown and flat films, including biaxial oriented films, also for extrusion of rods, pipes, plates, sheets, low diameter tubes and for injection molding of thick-wa.. |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm @Diameter 2.00 mm |
0.014 in/in @Diameter 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 20NSP1 Nylon 66, Conditioned Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 43% Filler by Weight Additive:Nucleating AgentLubricant Features:Fast Molding CycleGeneral PurposeGood Mold Release Good.. |