Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 5.50 kJ/m² @Temperature 23.0 °C |
2.62 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
Victrex® PEEK -HT™ G22 PolyEtherKetone, Unreinforced Product Description:High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact complia.. |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² | 2.62 ft-lb/in² | ISO 180 |
Polyram PlusTek PA355M6 Nylon 6.6 for Injection Molding, 30% Mineral Filled, Flame Retardant 30% Minerals filled, flame retardant Nylon 6.6 for injection molding applications.Information provided by Polyram. |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² | 2.62 ft-lb/in² | ASTM D256 |
Tipco Tipcolene® FPT 30 PPC - 30% Talc Reinforced Polypropylene Copolymer Compound 30% Talc Reinforced PP CopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² | 2.62 ft-lb/in² | ISO 180-93 |
Wellman Wellamid® MRGF25/15 42H-NBK1 40% Mineral/Glass Fiber Reinforced Nylon 6 Description: Mineral/Glass Fiber Reinforced Nylon 6Information provided by Wellman. |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² | 2.62 ft-lb/in² | ISO 180-93 |
Wellman Wellamid® WE1408 13% Glass Fiber Reinforced Engineering Grade Nylon 66 Description: Glass Fiber Reinforced Engineering Grade Nylon 66Information provided by Wellman. |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² @Temperature -20.0 °C |
2.62 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Total PPC 5660 Propylene, Heterophasic Copolymer ATOFINA Propylene 5660 is heterophasic copolymer. PPC 5660 is characterized by a medium fluidity offering a combination of ease of processing and good manufactured article properties in application.. |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² @Temperature -20.0 °C |
2.62 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Total PPC 7650 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 7650 is a nucleated and antistatic heterophasic copolymer. PPC 7642 is characterized by a medium fluidity offering a combination of ease of processing and excellent impact propert.. |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² @Temperature -20.0 °C |
2.62 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Total PPC 4660 Polypropylene, Heterophasic Copolymer ATOFINA Polypropylene PPC 4660 is heterophasic copolymer. |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² | 2.62 ft-lb/in² | ISO 180/1A |
DuPont Performance Polymers Crastin® LW9020FR BK851 PBT+ASA
(Unverified Data**) 20% Glass Reinforced Flame Retardant Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9020FR BK851 is a 20% glass fiber reinforced flame retardant black polybutylene tere.. |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² @Temperature 23.0 °C |
2.62 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecomid® NA40 AR20 NL HS PA6.6, 20% aramid fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² | 2.62 ft-lb/in² | ISO 180/1A |
Addiplast Addilene H 220 M40 Polypropylene Homopolymer Mineral reinforced, improved rigidityInformation provided by Addiplast. |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² | 2.62 ft-lb/in² | ISO 180/1A |
Addiplast Addilene J 520 M40 Polypropylene Copolymer Mineral reinforced, improved rigidityInformation provided by Addiplast. |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² @Temperature -30.0 °C |
2.62 ft-lb/in² @Temperature -22.0 °F |
ISO 180/A |
BASF Ultramid® B3L PA6 (Dry) Ultramid B3L is an impact-modified, easy flowing injection molding PA6 grade for fast processing. |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² | 2.62 ft-lb/in² | ISO Test |
BASF Ultramid® B3WGM24 BK30564 10/20% Glass/Mineral Filled PA6 (Dry) Ultramid B3WGM24 BK30564 is a 30% glass/mineral filled heat stabilized injection molding PA6 grade for industrial articles having medium to high rigidity and high dimensional stability. |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² | 2.62 ft-lb/in² | Conditioned; ISO 180/1A |
Addiplast Addinyl A2 ZV15 Nylon 66, 15% Glass Filled Glass fiber reinforced, increased thermal aging stabilityInformation provided by Addiplast. |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² | 2.62 ft-lb/in² | ISO Test |
BASF Ultramid® A3EG3 15% Glass Filled PA66 (Dry) Ultramid A3EG3 is a 15% glass fiber reinforced injection molding PA66 grade. It conforms to FDA requirements of 21 CFR 177.1500. |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² @Temperature 23.0 °C |
2.62 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
BASF Ultramid® A3WG3 15% Glass Filled PA66 (Dry) Description: 15% Glass-fiber reinforced and heat aging resistant injection-molding grade for machine elements and housings of medium stiffness. For electric insulating parts, preference should be gi.. |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² | 2.62 ft-lb/in² | ISO 180/A |
BASF Ultramid® B3K PA6 (Dry) Ultramid B 3K is an easy flowing, stabilized for fast processing, grade of nylon 6. |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² | 2.62 ft-lb/in² | DAM; ISO 180/1A |
DuPont Performance Polymers Zytel® 101 NC010 Nylon 66
(Unverified Data**) Unreinforced Polyamide 66Zytel 101 NC010 is a general purpose polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² | 2.62 ft-lb/in² | ISO 180 |
Ascend Performance Materials Vydyne® 50BWFS Nylon 66, Dry as Molded Vydyne® 50BWFS is a general purpose Nylon 66 resin. Available in natural. Designed for extrusion applications that do not require use of a highviscosity resin. This resin offers a well-balanced com.. |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² @Temperature -40.0 °C |
2.62 ft-lb/in² @Temperature -40.0 °F |
DAM; ISO 180/1A |
DuPont Performance Polymers Zytel® 101F NC010 Nylon 66
(Unverified Data**) Unreinforced Polyamide 66Zytel 101F NC010 is an internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont .. |
|||
Izod Impact, Notched (ISO) | 5.50 kJ/m² @Temperature 23.0 °C |
2.62 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
BASF Ultramid® A3K Q601 PA66(Dry) Description: Ultramid A3K Q601 is an easy flowing, injection molding grade PA66.Applications: Typical applications include fast processing high stress technical parts or electrically insulating part.. |