Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 42820 cP @Shear Rate 5000 1/s, Temperature 300 °C |
42820 cP @Shear Rate 5000 1/s, Temperature 572 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 101L NC010 Nylon 66
(Unverified Data**) Unreinforced Polyamide 66Zytel 101L NC010 is a lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |