Description/Features:Specialty Thermoplastic ElastomerMarket:IndustrialConsumer GoodsProcessing Method:Injection MoldingPolyOne First ChoiceInformation provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
ASTM D792
Linear Mold Shrinkage 0.0125 cm/cm
0.0125 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 83
83
Instant; ASTM D2240
Tensile Strength, Yield 8.20 MPa
1190 psi
Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412
5.17 MPa

@Strain 300 %
750 psi

@Strain 300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
Elongation at Break 460 %
460 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
Rebound 22 %
22 %
Bayshore; ASTM D2632
Tear Strength 28.0 kN/m
160 pli
Die C (graves), 20 in/min; ASTM D624