Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 12.0 MPa @Strain 5.00 %, Temperature 23.0 °C |
1740 psi @Strain 5.00 %, Temperature 73.4 °F |
ISO 527 (1BA bar) |
DuPont Performance Polymers Hytrel® 6359FG NC010 TPC-ET
(Unverified Data**) Hytrel® 6359FG is a medium modulus Hytrel® grade with nominal durometer hardness of 63D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing t.. |
|||
Tensile Stress | 12.0 MPa @Strain 1.00 %, Temperature 120 °C |
1740 psi @Strain 1.00 %, Temperature 248 °F |
|
Solvay TECHNYL® A 548B2 V15 PA66, 15% glass fiber, DRY Description: TECHNYL® A 548B2 V15 is a polyamide 6.6, reinforced with 15% of glass fiber, heat stabilized, impact modified, for blow molding. This product is available in black color.Benefits: Th.. |
|||
Tensile Stress | 12.0 MPa @Strain 20.0 %, Temperature 150 °C |
1740 psi @Strain 20.0 %, Temperature 302 °F |
|
Solvay TECHNYL® eXten D 437P PA6.10 Description: TECHNYL® eXten D 437P is a high viscosity, unfilled, plasticized, UV and heat stabilized PA6.10 for extrusion applications. Technyl® eXten D 437P is a partially biosourced materia.. |
|||
Tensile Stress | 12.0 MPa @Strain 100 %, Temperature 150 °C |
1740 psi @Strain 100 %, Temperature 302 °F |
|
Solvay TECHNYL® eXten D 437P PA6.10 Description: TECHNYL® eXten D 437P is a high viscosity, unfilled, plasticized, UV and heat stabilized PA6.10 for extrusion applications. Technyl® eXten D 437P is a partially biosourced materia.. |
|||
Tensile Stress | 12.0 MPa @Strain 50.0 % |
1740 psi @Strain 50.0 % |
conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® ELX 50 HNZ TPA Product description: Grilon ELX 50 H NZ is a high viscosity, heat stabilized, impact modified, thermoplastic PA6 elastomer for extrusion blow molding applications. Grilon ELX 50 H NZ has the followi.. |
|||
Tensile Stress | 12.0 MPa @Strain 5.00 % |
1740 psi @Strain 5.00 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® 6356 Polyester Elastomer TPC-ET
(Unverified Data**) 63 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 12.0 MPa @Strain 118.08 %, Temperature 120 °C |
1740 psi @Strain 118.08 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 8238 Polyester Elastomer TPC-ET
(Unverified Data**) 82 Shore D Standard Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 12.0 MPa @Strain 0.528 %, Time 3.60e+6 sec |
1740 psi @Strain 0.528 %, Time 1000 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 80G14A NC010A Nylon 66
(Unverified Data**) 14% Glass Reinforced Toughened Polyamide 66 Zytel 80G14A NC010A is a 14% glass fiber reinforced toughened high flow polyamide 66 resin. It offers outstanding performance in injection molding applica.. |
|||
Tensile Stress | 12.0 MPa @Strain 0.100 %, Temperature 23.0 °C |
1740 psi @Strain 0.100 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 80G43HS1L BK104 Nylon 66
(Unverified Data**) 43% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G43HS1L BK104 is a 43% glass fiber reinforced heat stabilized black polyamide 66 resin with superior impact resistance.Information.. |
|||
Tensile Stress | 12.0 MPa @Strain 0.420 %, Temperature 90.0 °C |
1740 psi @Strain 0.420 %, Temperature 194 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® BM70G20HSLX BK537 Nylon 66
(Unverified Data**) 20% Glass Reinforced Heat Stabilized Polyamide 66 Developed for Blow Molding Zytel BM70G20HSLX BK537 is a 20% glass fiber reinforced polyamide 66 for blow molding.Information provided by DuPont Perf.. |
|||
Tensile Stress | 12.0 MPa @Strain 5.00 %, Temperature 23.0 °C |
1740 psi @Strain 5.00 %, Temperature 73.4 °F |
ISO 527 (1BA bar) |
DuPont Performance Polymers Hytrel® DYM500BK TPC-ET
(Unverified Data**) Hytrel® DYM500BK is a medium modulus polyester alloy suited for injection molding of Air Bag Deployment Doors. It has a nominal durometer hardness of 55D and contains fine particle size carbon blac.. |
|||
Tensile Stress | 12.0 MPa @Strain 5.00 % |
1740 psi @Strain 5.00 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® HTR8163HVBK Polyester Elastomer TPC-ET
(Unverified Data**) 65 Shore D Polyester Elastomer with Heat Ageing Protection Developed for ExtrusionInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 12.0 MPa @Strain 50.0 % |
1740 psi @Strain 50.0 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® HTR8341C BK320 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D Lubricated High Viscosity Polyester Elastomer with Superior Fatigue Resistance Developed for Blow Molding Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 12.0 MPa @Strain 1.52 %, Time 360000 sec |
1740 psi @Strain 1.52 %, Time 100 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 101L NC010 Nylon 66
(Unverified Data**) Unreinforced Polyamide 66Zytel 101L NC010 is a lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 12.0 MPa @Strain 1.25 %, Time 36000 sec |
1740 psi @Strain 1.25 %, Time 10.0 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 101L NC010 Nylon 66
(Unverified Data**) Unreinforced Polyamide 66Zytel 101L NC010 is a lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 12.0 MPa @Strain 1.45 %, Time 3.60e+7 sec |
1740 psi @Strain 1.45 %, Time 10000 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 135F NC010 Nylon 66
(Unverified Data**) Unreinforced Nucleated Polyamide 66 Zytel 135F NC010 is a nucleated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Pe.. |
|||
Tensile Stress | 12.0 MPa @Strain 1.18 %, Time 3.60e+6 sec |
1740 psi @Strain 1.18 %, Time 1000 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 135F NC010 Nylon 66
(Unverified Data**) Unreinforced Nucleated Polyamide 66 Zytel 135F NC010 is a nucleated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Pe.. |
|||
Tensile Stress | 12.0 MPa @Strain 0.947 %, Time 360000 sec |
1740 psi @Strain 0.947 %, Time 100 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 135F NC010 Nylon 66
(Unverified Data**) Unreinforced Nucleated Polyamide 66 Zytel 135F NC010 is a nucleated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Pe.. |
|||
Tensile Stress | 12.0 MPa @Strain 0.772 %, Time 36000 sec |
1740 psi @Strain 0.772 %, Time 10.0 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 135F NC010 Nylon 66
(Unverified Data**) Unreinforced Nucleated Polyamide 66 Zytel 135F NC010 is a nucleated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Pe.. |
|||
Tensile Stress | 12.0 MPa @Strain 1.77333 %, Time 360000 sec |
1740 psi @Strain 1.77333 %, Time 100 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 42A NC010 Nylon 66
(Unverified Data**) Unreinforced High Viscosity Polyamide 66Zytel 42A NC010 is a high viscosity polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 12.0 MPa @Strain 1.45833 %, Time 36000 sec |
1740 psi @Strain 1.45833 %, Time 10.0 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 42A NC010 Nylon 66
(Unverified Data**) Unreinforced High Viscosity Polyamide 66Zytel 42A NC010 is a high viscosity polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 12.0 MPa @Time 3600 sec, Strain 1.19 % |
1740 psi @Time 1.00 hour, Strain 1.19 % |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 42A NC010 Nylon 66
(Unverified Data**) Unreinforced High Viscosity Polyamide 66Zytel 42A NC010 is a high viscosity polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 12.0 MPa @Strain 100 % |
1740 psi @Strain 100 % |
ASTM D412 |
Alliance Polymers Zythane™ 4050D Thermoplastic Polyurethane Elastomer Zythane™ 4050D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Tensile Stress | 12.0 MPa @Strain 100 % |
1740 psi @Strain 100 % |
ASTM D412 |
Alliance Polymers Zythane™ 6070A Thermoplastic Polyurethane Elastomer Zythane™ 6070A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Tensile Stress | 12.0 MPa @Strain 0.200 %, Time 3.60e+6 sec |
1740 psi @Strain 0.200 %, Time 1000 hour |
ISO 899-1 |
BASF Ultraform N 2200 G53 UNC Q600 25% Glass Filled POM Ultraform N2200 G53 UNC Q600 is a 25% glass fiber reinforced POM injection molding grade with enhanced stiffness and toughness. |
|||
Tensile Stress | 12.0 MPa @Strain 100 % |
1740 psi @Strain 100 % |
|
AorTech Biomaterials Elast-Eon™ E2-945 Biomedical Polyurethane Pellets Elast-Eon™ polymers are used in biomedical applications. They have high biostability so they can be used for long term implantation. |
|||
Tensile Stress | >= 12.0 MPa @Strain 300 % |
>= 1740 psi @Strain 300 % |
ISO 37 |
Austin Novel Materials Texalan® 790A PCL TPU Description: Good abrasion resistance, tensile strength, oil resistance and heat resistance which can be used in mechanic parts and various industry parts.Information from Dawnentech |
|||
Tensile Stress | 12.0 MPa @Temperature 240 °C |
1740 psi @Temperature 464 °F |
|
BASF Ultramid® Endure D3G7 Glass-Fiber Reinforced Polyamide Description: Ultramid® Endure is a new, glass-fiber reinforced polyamide that combines excellent heat aging resistance with the good processing properties of PA 66. Ultramid® Endure can withstand .. |
|||
Tensile Stress | 12.0 MPa @Strain 0.100 %, Temperature 23.0 °C |
1740 psi @Strain 0.100 %, Temperature 73.4 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® 80G43HS1L BK104 Nylon 66
(Unverified Data**) Zytel® 80G43HS1L BK104 is a 43% glass fiber reinforced, heat stabilized, black polyamide 66 resin with superior impact resistance.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 12.0 MPa @Strain 10.0 %, Time 3.60e+6 sec |
1740 psi @Strain 10.0 %, Time 1000 hour |
100°C; ISO 527 |
BASF Ultradur B 4520 PBT Ultradur B4520 is a medium viscosity, rapidly freezing injection molding grade. |