Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.40 GPa | 203 ksi | ISO 527 |
Nilit FRIANYL B63 CU90 Nylon 6.6 for injection molding, 90% copper filled Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 1.40 GPa | 203 ksi | 1mm/min |
Eastman Eastar DN101 PCTG Copolyester
(discontinued **) ISO data as provided by the manufacturer, Eastman Chemical |
|||
Tensile Modulus | 1.40 GPa | 203 ksi | 1 mm/min |
Polimeri Europa SINKRAL B813 ABS, Impact Grade
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-04-35-15 Injection moulding grade, providing very high impact resistance, even at low temperatures. Used as.. |
|||
Tensile Modulus | 1.40 GPa | 203 ksi | |
LyondellBasell Lupolen® 6021 D HDPE, Blow Molding Grade Easy flow, blow molding grade for small, rigid, thin-walled containers (up to 5 l), pots (up to 1 l), bottles and canisters (up to 5 l) for packaging mineral oil, antifreeze, brake fluid; drink bott.. |
|||
Tensile Modulus | 1.40 GPa | 203 ksi | |
Aardvark Polymers Aardalloy® 3300 POM Alloy Rotational Molding Resin Aardalloy 3300 is an acetal alloy formulated for enhanced impact resistance and elongation.Aardalloy 3300 maintains the high degree of chemical resistance and low fuel permeation rates of unfilled a.. |
|||
Tensile Modulus | 1.40 GPa | 203 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 230 PA66, Conditioned Description: Unreinforced and modified polyamide 66, with improved impact resistance, for injection molding.Available in: Europe and North AmericaProduct Applications: TECHNYL® A 230 offers excel.. |
|||
Tensile Modulus | 1.40 GPa | 203 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-LOY KX05015 Acetal Copolymer (Europe-Africa-Middle East) LNP* Stat-Loy* KX05015 is a compound based on Acetal Copolymer resin containing Antistat. Added features include permanent Anti-Static. |
|||
Tensile Modulus | 1.40 GPa | 203 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 205F PA66, Conditioned Description: TECHNYL ® A 205F is an unreinforced polyamide 66 for injection molding. It is available in natural color.Benefits: The product offers two main advantages: excellent filling qualities.. |
|||
Tensile Modulus | 1.40 GPa | 203 ksi | At 1 mm/min; ISO 178 |
Borealis Borcoat™ BB700E-7032 Polypropylene Compound for Steel Pipe Coating Applications Borcoat BB700E-7032 is a grey colored high impact polypropylene. This product is especially designed for direct extrusion of syntactic PP with high thermal insulations capacity and high compression.. |
|||
Tensile Modulus | 1.40 GPa | 203 ksi | ISO 527-2 |
Total PPC 9760 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 9760 is heterophasic copolymer. PPC 9760 is characterized by improved stiffness, creep resistance and high impact resistance. |
|||
Tensile Modulus | 1.40 GPa | 203 ksi | ISO 527-2 |
Total PPH 3051 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 3051 is homopolymer.ApplicationATOFINA Polypropylene PPH 3051 is intended for the extrusion of flat bioriented films for food packaging or high strength adhesive tapes. Inf.. |
|||
Tensile Modulus | 1.40 GPa | 203 ksi | ISO 527-2 |
Total PPH 6088 Polypropylene Homopolymer, Cast Film Polypropylene PPH 6088 is a homopolymer polypropylene with a Melt Flow index of 9 g/10 min for the cast extrusion of film with excellent optical properties and good sterilizability.Polypropylene PPH.. |
|||
Tensile Modulus | 1.40 GPa | 203 ksi | ISO 527-1/-2 |
DSM Akulon® K225-KS Nylon 6 (European and Asian Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Tensile Modulus | 1.40 GPa | 203 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® L 20 LM PA12 Product Description: Grilamid L 20 LM is a medium viscosity Polyamide 12 (PA12) extrusion grade. Grilamid L 20 LM is UV and heat stabilized and has been modified with a nucleation agent which result.. |
|||
Tensile Modulus | 1.40 GPa | 203 ksi | Secant; ISO527-2/1 |
ExxonMobil PP4031E2 Polypropylene Impact Copolymer Product Description: An impact copolymer resin for extrusion applications with high melt viscosity and excellent rigidity, shock resistance and dimensional stability. It is designed for corrugated .. |
|||
Tensile Modulus | 1.40 GPa | 203 ksi | ISO 527-2 |
Domo 2348M Polypropylene Copolymer Information provided by Domo. |
|||
Tensile Modulus | 1.40 GPa | 203 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® FG101L NC010 Nylon 66
(Unverified Data**) Unreinforced Polyamide 66 with Developed for Food Contact ApplicationsZytel FG101L NC010 is a lubricated polyamide 66 resin for injection molding. It has been developed for consideration into applic.. |
|||
Tensile Modulus | 1.40 GPa | 203 ksi | 1 mm/min; ISO 527 |
Eurostar Staramide P1000J5 PA6, Impact Modified, Injection Molded Staramide P1000J5 is a Low Temperature Impact Modified, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Modulus | 1.40 GPa @Temperature -20.0 °C |
202 ksi @Temperature -4.00 °F |
50%RH; Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 330 NC010 Nylon
(Unverified Data**) Unreinforced PolyamideZytel 330 NC010 is a transparent polyamide resin with amorphous characteristics.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 1.40 GPa | 203 ksi | ASTM D638 |
Aclo Accutech Polypropylene Homopolymer HP0336T10L1 Talc Reinforced |
|||
Tensile Modulus | 1.40 - 1.45 GPa | 203 - 210 ksi | ASTM D638 |
Adamas Rixon 430 PEEK, 30% Carbon Fiber Information provided by Adamas, HPM |
|||
Tensile Modulus | 1.40 GPa | 203 ksi | |
BASF Novolen® 2348 M Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Tensile Modulus | 1.40 GPa | 203 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® 21SPC1 Nylon 66, Conditioned Vydyne® 21SPC1 is a general-purpose, improved-flow, lubricated PA66 resin available in natural color. 21SPC1 offers a balanced combination of properties characterized by high strength, rigidity, go.. |
|||
Tensile Modulus | 1.40 GPa | 203 ksi | ASTM D638 |
Aclo Accucomp ABS ABS804L High Impact Grade |
|||
Tensile Modulus | 1.40 GPa | 203 ksi | |
BASF Polystyrol® 2712 Impact Grade Polystyrene (Europe) Easy flowing special grade, particularly resistant to stress cracking.Data was collected by ISO methods and provided by BASF. |
|||
Tensile Modulus | 1.40 - 2.20 GPa @Thickness 2.00 mm, Temperature 23.0 °C |
203 - 319 ksi @Thickness 0.0787 in, Temperature 73.4 °F |
Type IV, 1.0 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 9007 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 9007 PVDF homopolymer has low viscosity and is used in film extrusion and injection molding.Information provided by Solvay Specialty Polymers. |
|||
Tensile Modulus | 1.40 GPa | 203 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® L 25 nat PA12 Product Description: Grilamid L 25 is a high viscosity polyamide 12. This product has the following features: Very tasteless High toughness, even at low temperatures Good resistance to weathering Go.. |
|||
Tensile Modulus | 1.40 GPa | 203 ksi | |
Plastcom SLOVALEN PC 92 T 40 PP, 40% mineral filling FeaturesModified homopolymer and copolymer PP for injection moulding with the contenct of 40% microground, chemically modified talc. Increased strength, rigidity and thermal application up to 100°C.. |