Mechanical Properties Metric English Comments
Hardness, H358/30 180 MPa
26100 psi
ISO 2039-1
SABIC Innovative Plastics Valox® 457 PBT (Europe-Africa-Middle East)
VALOX 457 is a 6.5% glass fibre reinforced flame retarded PBT injection moulding resin. Applications: electrical and appliances industries.
Hardness, H358/30 180 MPa
26100 psi
DAM; ISO 2039-1
DuPont Performance Polymers Zytel® 101L NC010 Nylon 66  (Unverified Data**)
Unreinforced Polyamide 66Zytel 101L NC010 is a lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Hardness, H358/30 180 MPa
26100 psi
DAM; ISO 2039-1
DuPont Performance Polymers Zytel® 101 NC010 Nylon 66  (Unverified Data**)
Unreinforced Polyamide 66Zytel 101 NC010 is a general purpose polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers
Hardness, H358/30 180 MPa
26100 psi
DAM; DS; ISO 2039-1
DuPont Performance Polymers Zytel® 101L BKB080 Nylon 66  (Unverified Data**)
Unreinforced Polyamide 66Zytel 101L BKB080 is a lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers