Sibur Phenoplast

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer Sibur
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sibur Phenoplast.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
For production by direct pressing.
Physical Properties Metric English Comments
Density <= 1.50 g/cc
<= 0.0542 lb/in³
Linear Mold Shrinkage 0.0020 - 0.0050 cm/cm
0.0020 - 0.0050 in/in
Collected Volatile Condensable Material <= 9.0 %
<= 9.0 %
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 79.0 MPa
>= 11500 psi
Bending
Charpy Impact Unnotched >= 0.880 J/cm²
>= 4.19 ft-lb/in²
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) >= 150 °C
>= 302 °F
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+9 ohm-cm
>= 1.00e+9 ohm-cm
Descriptive Properties Value Comments
Electric Density, KW/mm >6
Flow, mm 40-140