Material Notes:
Description: Impact-modified and 30% glass fiber reinforced injection-molding grade for technical articles of very high stiffness and toughness, for instance, for vehicle airbag housings and suitcase shells.Information provided by BASF
Physical Properties Metric English Comments
Density 1.33 g/cc
0.0480 lb/in³
ISO 1183
Water Absorption 5.9 - 6.5 %
5.9 - 6.5 %
Saturation; ISO 62
Moisture Absorption at Equilibrium 1.8 - 2.2 %
1.8 - 2.2 %
23°C; 50% RH; ISO 62
Viscosity Measurement 160
160
ISO 307
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
restricted
Melt Flow 33.25 g/10 min

@Load 5.00 kg,
Temperature 275 °C
33.25 g/10 min

@Load 11.0 lb,
Temperature 527 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 100 MPa
14500 psi
50 mm/min; ISO 527-1/-2
Elongation at Yield 10 %
10 %
50 mm/min; ISO 527-1/-2
Modulus of Elasticity 5.30 GPa
769 ksi
ISO 527-1/-2
Flexural Strength 130 MPa
18900 psi
at max force; ISO 178
Flexural Modulus 4.70 GPa
682 ksi
ISO 178
Izod Impact, Notched (ISO) 32.0 kJ/m²

@Temperature 23.0 °C
15.2 ft-lb/in²

@Temperature 73.4 °F
ISO 180/A
Charpy Impact Unnotched 11.0 J/cm²

@Temperature 23.0 °C
52.3 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 3.50 J/cm²

@Temperature 23.0 °C
16.7 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Tensile Creep Modulus, 1000 hours 3000 MPa

@Strain <=0.500 %
435000 psi

@Strain <=0.500 %
ISO 899-1
Thermal Properties Metric English Comments
Thermal Conductivity 0.350 W/m-K
2.43 BTU-in/hr-ft²-°F
DIN 52612
Melting Point 220 °C
428 °F
DIN 53765
Maximum Service Temperature, Air 180 °C
356 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+10 ohm-cm
1.00e+10 ohm-cm
IEC 60093
Surface Resistance 1.00e+10 ohm
1.00e+10 ohm
IEC 60093
Dielectric Constant 6.8

@Frequency 1.00 Hz
6.8

@Frequency 1.00 Hz
IEC 60250
Dissipation Factor 0.20

@Frequency 1.00e+6 Hz
0.20

@Frequency 1.00e+6 Hz
IEC 60250
Comparative Tracking Index 550 V
550 V
Test solution A; IEC 60112
Processing Properties Metric English Comments
Melt Temperature 270 - 290 °C
518 - 554 °F
Injection-molding/Extrusion
Mold Temperature 80.0 - 90.0 °C
176 - 194 °F
Injection-molding
Descriptive Properties Value Comments
Color BK 30564
Commercial Status Europe
Users viewing this material also viewed the following: