Polymer Property : Mold Temperature = 176 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Mold Temperature 80.0 - 120 °C
176 - 248 °F
Lehmann & Voss LUVOCOM® 50-8300 Polycarbonate, with PTFE
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High dimensionally stable precision parts, even at elevated te..
Mold Temperature 80.0 - 120 °C
176 - 248 °F
Lehmann & Voss LUVOCOM® 80-7705 Polyacetal-copolymer, with carbon fiber, aramid reinforcement and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Suitable for discharging of st..
Mold Temperature 80.0 - 120 °C
176 - 248 °F
Lehmann & Voss LUVOCOM® 80-7752 Polyacetal-copolymer, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita..
Mold Temperature 80.0 - 110 °C
176 - 230 °F
Kraiburg TPE THERMOLAST® K TC7HAZ Thermoplastic Elastomer
The AD/POM Series is recommended for applications with excellent adhesion to POM. The compounds are available in natural and black colors. Typical applications: BumpersFunction and design elementsGr..
Mold Temperature 80.0 - 120 °C
176 - 248 °F
ISO 294
Gromax BFG30-FU00B3 Nylon 6 30% Glass Filled (Conditioned)
Information provided by Gromax Enterprises Corp.
Mold Temperature 80.0 - 100 °C
176 - 212 °F
Lanxess Durethan® BKV 130 GIT DUS008 900116 Nylon 6, Impact Modified
PA 6, 30% glass fibers, injection molding, impact modified, GIT/WITInformation provided by LANXESS.
Mold Temperature 80.0 °C
176 °F
for test specimens; ISO 294
Lanxess Durethan® BKV 130 H2.0 DUS008 901510 Nylon 6, Glass Fiber Reinforced, Impact Modified
PA 6, 30% glass fibers, injection molding, impact modified, heat-aging stabilizedInformation provided by LANXESS.
Mold Temperature 80.0 °C
176 °F
Injection Molding; ISO 10724
Lanxess Pocan® DP 4035 000000 PBT + PET, 30% Glass Fiber
PBT+PET, 30% glass fibers, injection molding, halogen free flame retardant
Mold Temperature 80.0 - 120 °C
176 - 248 °F
ISO 294
Gromax BBG30-AN00N1 Nylon 6, Flame Retardant (Dry)
Information provided by Gromax Enterprises Corp.
Mold Temperature 80.0 - 120 °C
176 - 248 °F
ISO 294
Gromax BFG30-AH00B2 Nylon 6 30% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.
Mold Temperature 80.0 - 120 °C
176 - 248 °F
ISO 294
Gromax BTE65-DN001N1 Nylon 6 (Conditioned)
Information provided by Gromax Enterprises Corp.
Mold Temperature 80.0 °C
176 °F
for test specimens; ISO 294
Lanxess Durethan® DP BKV 35 XF 901510 Nylon 6, 35% Glass Fiber
PA 6, 35% glass fibers, injection molding, improved flowability, improved surface finishInformation provided by LANXESS.
Mold Temperature 80.0 °C
176 °F
Injection Molding; ISO 10724
Lanxess Pocan® KU 1-7625 901510 PBT + PC, 20% Glass Fiber
PBT+PC, 20% glass fibers, injection molding, low tendency to warp, improved surface finish
Mold Temperature 80.0 - 90.0 °C
176 - 194 °F
LATI Latiohm 90/13-09 PD01 G/10 PPOm, 10% Glass Fiber Reinforced
Semiconductive/dissipative product based on Modified Polyphenylene Oxide (PPOm). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation prov..
Mold Temperature 80.0 - 100 °C
176 - 212 °F
Solvay TECHNYL® C 218 MZ20 V10 Black Z PA6, 20/10% mineral/glass fiber, DRY
Description: Polyamide PA6, reinforced 20 % mineral filler and 10 % of glass fiber, heat stabilized, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL C 218 MZ20 V10 offe..
Mold Temperature 80.0 - 100 °C
176 - 212 °F
Surface
Solvay Technyl® C218V30 30% Glass Filled, Heat Stabilized Nylon 6
Information provided by Rhodia; Rhodia has been acquired by Solvay.
Mold Temperature 80.0 °C
176 °F
Solvay Technyl Starâ„¢ S 60G1 V30 30% Glass Reinforced Nylon 6, Flame Retardant
This Halogen free flame retardant grade, based on high fluidity Technyl Star, combines excellent all-round mechanical properties with outstanding flame retardancy and electrical performance. This pr..
Mold Temperature 80.0 °C
176 °F
Injection molding; ISO 294
Covestro Bayblend® FR3006 HF PC/ABS Blend
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec..
Mold Temperature 80.0 °C
176 °F
Injection molding; ISO 294
Covestro Bayblend® FR3012 PC/ABS Blend
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec..
Mold Temperature 80.0 °C
176 °F
Injection Molding; ISO 10724
Covestro Makrolon® 2806 Polycarbonate
ISO 7391-PC,M,(,,)-09-9MVR (300 °C/1.2 kg) 9.5 cm3/10 minFood contact qualityMedium viscosityGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CAvailable in transparenttran..
Mold Temperature 80.0 - 120 °C
176 - 248 °F
Covestro Makrolon® 2856 Polycarbonate
ISO 7391-PC,MR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 9.5 cm3/10 minFood contact qualityMedium viscosityEasy releaseGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CAva..
Mold Temperature 80.0 - 130 °C
176 - 266 °F
Covestro Makrolon® 9415 Polycarbonate, 10% Glass Filled
ISO 7391-PC,MFR,(,,)-09-9,GF10Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 min10 % Glass fiber reinforcedChlorine- and bromine-free flame retardantUL 94V-0/1.5 mm and 5VA/3.0 mmHigh viscosityEasy rel..
Mold Temperature 80.0 - 100 °C
176 - 212 °F
E-Polymers Tekaster® F615G30 , 30% Glass Fiber Reinforced PET
30% Glass Fiber reinforced, High strength, Information provided by E-Polymers Co. Ltd.
Mold Temperature 80.0 - 120 °C
176 - 248 °F
Akro-Plastic Akroloy® PA GF 40 (2845) PA 6.6 & PA6I/6T Dry, 40% Glass Filled
One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param..
Mold Temperature 80.0 - 120 °C
176 - 248 °F
Celanese Thermx® CG943 BK010 PCT
Thermx® CG943 BK010 is a 40% glass fiber reinforced, flame retardant, black polycyclohexylenedimethylene terephthalate resin for injection molding.Celenese acquired the Thermx product line from DuP..
Mold Temperature 80.0 - 90.0 °C
176 - 194 °F
Injection molding/Extrusion
BASF Ultramid® S3WG7 Balance 35% Glass Filled PA 610 (Dry)
Description: BASF supplies polyamide 610 for processing by injection molding under the trade name Ultramid® Balance which is produced by polycondensation of hexamethylene diamine and sebacic acid. ..
Mold Temperature 80.0 °C
176 °F
Optimal
BASF Ultramid® A3EG5 25% Glass Filled PA66 (Dry)
Description: Glass fiber reinforced injection molding grade for machinery components and housings of high stiffness and dimensional stability such as coil formers and bearing cages. Also used for el..
Mold Temperature 80.0 - 120 °C
176 - 248 °F
Celanese Hostaform® C 13031 XF POM, Specialty  (Unverified Data**)
Hostaform® acetal copolymer grade C13031 XF is an acetal copolymer modified to resist deterioration from aggressive fuel blends. This material is specially targeted for transportation industry fu..
Mold Temperature 80.0 - 120 °C
176 - 248 °F
Celanese Hostaform® MT12U03 POM, Medical Technology  (Unverified Data**)
Hostaform® MT12U03 is a special grade developed for medical industry applications containing low residual monomers and no animal products. Hostaform® MT12U03 is a moderately high flow grade for fa..
Mold Temperature 80.0 °C
176 °F
Optimal
BASF Ultradur® B 4040 G10 50% Glass Filled BK 15029 PBT + PET
Description: Injection molding grade with 50% glass fibers for industrial parts with excellent surface quality, for example external door handles in vehicles, visible sunroof frames, oven door handl..