Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Precision Polymer Engineering S70U Silicone Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone
Manufacturer Precision Polymer Engineering Limited
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Precision Polymer Engineering S70U Silicone Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Black Silicone Rubber, 66-75 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. Specially formulated for anti-static, semi-conductive applications. ASTM & ISO designation = VMQ.Applications: Low compression set grade, offering excellent heat resistance and low temperature flexibility. Used primarily for dry heat static seals, low physical strength and poor abrasion resistance prevents dynamic sealing.
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
°IRHD; ASTM D1415
Tensile Strength, Yield 4.80 MPa
696 psi
ASTM D412
Elongation at Break 200 %
200 %
ASTM D412
Compression Set 20 %
20 %
70 hours @ 150°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 160 °C
320 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Non-brittle after 3 minutes
-50.0 °C
-58.0 °F
Flash Point >= 300 °C
>= 572 °F