Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Trade Name : Ultramid® Product List

Category Nylon 66, Unreinforced , Nylon 66, 10% Glass Fiber Filled , Nylon 66, 30% Glass Fiber Filled , Nylon 66/6, Unreinforced , Nylon 66, 40% Glass Fiber Filled , Nylon 6, Unreinforced , Nylon 6, Unreinforced, Flame Retardant , Nylon 6, 30% Glass Fiber Filled , Nylon 6, Glass Fiber Filled, Flame Retardant , Nylon 6, 50% Glass Fiber Filled , Nylon 6, 40% Glass Fiber Filled , Nylon 6, Impact Grade , Nylon 6, 40% Mineral Filled , Nylon 6, Glass/Mineral Reinforced , Nylon 66, Unreinforced, Flame Retardant , Nylon 66, 50% Glass Fiber Filled , Nylon 66, 20% Glass Fiber Filled , Nylon 610, Glass Reinforced , Nylon 66, Impact Grade , Nylon 66, Glass/Mineral Filled , Nylon 66, Glass Fiber Filled, Flame Retardant , Nylon 6, Glass Bead Filled , Nylon 6, 30% Mineral Filled , Nylon 6, 20% Glass Fiber Filled , Film , Nylon 66/6, 20% Glass Fiber Reinforced , Nylon 66, 60% Glass Fiber Filled , Nylon 66, 40% Mineral Filled
Manufacturer BASF
Tips: Up to 50 items displayed.
PRODUCT NO. Category
BASF Ultramid® 1403-2 BK ND3007 PA66 (Dry) Nylon 66, 10% Glass Fiber Filled
BASF Ultramid® 8202 L Intermediate PA6 (Conditioned) Nylon 6, Unreinforced
BASF Ultramid® 8202 PA6 (Conditioned) Nylon 6, Unreinforced, Flame Retardant
BASF Ultramid® 8202CQ PA6 (Conditioned) Nylon 6, Unreinforced
BASF Ultramid® 8232G HS FR 25% Glass Fiber Fire Retardant PA6 (Conditioned) Nylon 6, Glass Fiber Filled, Flame Retardant
BASF Ultramid® 8233G HS BK-102 33% Glass Filled PA6 (Dry) Nylon 6, 30% Glass Fiber Filled
BASF Ultramid® 8233G HS BK-106 33% Glass Filled PA6 (Conditioned) Nylon 6, 30% Glass Fiber Filled
BASF Ultramid® 8253 BK-102 PA6 (Dry) Nylon 6, Impact Grade
BASF Ultramid® 8260 40% Mineral Filled PA6 (Dry) Nylon 6, 40% Mineral Filled
BASF Ultramid® 8260 HS BK-102 40% Mineral Filled PA6 (Conditioned) Nylon 6, 40% Mineral Filled
BASF Ultramid® 8266G HS BK-102 15/25% Glass/Mineral Filled PA6 (Dry) Nylon 6, Glass/Mineral Reinforced
BASF Ultramid® 8272G HS BK-102 12% Glass Filled PA6 (Dry) Nylon 6, 10% Glass Fiber Filled
BASF Ultramid® 8281 HS GP PA6 (Dry) Nylon 6, Unreinforced
BASF Ultramid® A24 E 01 PA66 Nylon 66, Unreinforced
BASF Ultramid® A34 01 PA66 (Conditioned) Nylon 66, Unreinforced, Flame Retardant
BASF Ultramid® A3K PA66 (Conditioned) Nylon 66, Unreinforced, Flame Retardant
BASF Ultramid® A3W PA66 (Dry) Nylon 66, Unreinforced
BASF Ultramid® A3WG6 HRX BK 23591 30% Glass Filled PA66 (Dry) Nylon 66, 30% Glass Fiber Filled
BASF Ultramid® A3X4G7 35% Glass Filled PA66 FR (Conditioned) Nylon 66, 40% Glass Fiber Filled
BASF Ultramid® A3ZG6 BK 20591 30% Glass Filled PA66 (Dry) Nylon 66, 30% Glass Fiber Filled
BASF Ultramid® B3EG6 LS BK 23189 30% Glass Filled PA6 (Conditioned) Nylon 6, 30% Glass Fiber Filled
BASF Ultramid® B3EG7 35% Glass Filled PA6 (Conditioned) Nylon 6, 40% Glass Fiber Filled
BASF Ultramid® B3G8 BK00564 40% Glass Filled PA6 (Conditioned) Nylon 6, 40% Glass Fiber Filled
BASF Ultramid® B3GM35 Q643 15/25% Glass/Mineral Filled PA6 (Dry) Nylon 6, Glass/Mineral Reinforced
BASF Ultramid® B3UG4 BK 23215 20% Glass Filled PA66 FR (Conditioned) Nylon 66, 20% Glass Fiber Filled
BASF Ultramid® BU50I BK 106 PA6 (Conditioned) Nylon 6, Unreinforced
BASF Ultramid® C3U10 BK 23079 PA6/66 FR (Dry) Nylon 6/66
BASF Ultramid® C40 LN 01 PA6/66 Nylon 66/6, Unreinforced
BASF Ultramid® FRee A3U40G5 25% Glass Filled PA66 FR (Conditioned) Nylon 66, 30% Glass Fiber Filled
BASF Ultramid® HFX 37 PA6 (Dry) Nylon 6, Unreinforced
BASF Ultramid® HPN 9362 40% Mineral Filled PA6 (Dry) Nylon 6, 40% Mineral Filled
BASF Ultramid® KR 4355 G7 BK 00564 35% Glass Filled PA6/6T (Dry) Nylon 6, 40% Glass Fiber Filled
BASF Ultramid® N-276 BK ND 3007 40% Glass/Mineral Filled PA66 Nylon 66, Glass/Mineral Filled
BASF Ultramid® N-333 NF3001 33% Glass Filled PA66 (Dry) Nylon 66, 30% Glass Fiber Filled
BASF Ultramid® S3EG6 Balance 30% Glass Filled PA 610 (Dry) Nylon 610, Glass Reinforced
BASF Ultramid® S3WG7 Balance 35% Glass Filled PA 610 (Dry) Nylon 610, Glass Reinforced
BASF Ultramid® TG7S BK-102 35% Glass Filled PA6 (Dry) Nylon 6, 40% Glass Fiber Filled
BASF Ultramid® 1003-2 NF2002 PA66 (Dry) Nylon 66, Unreinforced
BASF Ultramid® 1703-2 BK ND3007 25% Glass Filled PA66 (Conditioned) Nylon 66, 30% Glass Fiber Filled
BASF Ultramid® B32 01 PA6 (Dry) Nylon 6, Unreinforced
BASF Ultramid® B36 01 PA6 (Dry) Nylon 6, Unreinforced
BASF Ultramid® B3EG3 BK 00564 15% Glass Filled PA6 (Conditioned) Nylon 6, 20% Glass Fiber Filled
BASF Ultramid® B3EG3 BK00564 15% Glass Filled PA6 (Dry) Nylon 6, 20% Glass Fiber Filled
BASF Ultramid® B3GM35 BK 30564 15/25% Glass/Mineral Filled PA6 (Dry) Nylon 6, Glass/Mineral Reinforced
BASF Ultramid® B3M6 30% Mineral Filled PA6 (Dry) Nylon 6, 30% Mineral Filled
BASF Ultramid® B3ZG3 15% Glass Filled PA6 (Dry) Nylon 6, 20% Glass Fiber Filled
BASF Ultramid® TG3S BK 5966 15% Glass Filled PA6 (Conditioned) Nylon 6, 20% Glass Fiber Filled
BASF Ultramid® B3S BK00464 PA6 (Dry) Nylon 6, Unreinforced
BASF Ultramid® N-265 NF3001 40% Mineral Filled PA66 (Dry) Nylon 66, 40% Mineral Filled
Copyright © lookpolymers.com All Rights Reserved