Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 50.0 - 90.0 °C | 122 - 194 °F | |
PolyOne LubriOne™ NN-25GB/15T Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Mold Temperature | 60.0 - 90.0 °C | 140 - 194 °F | |
Plastcom SLOVAMID 66 GF 20 PA66, 20% glass fibre FeaturesChemically reinforced with 20 % glass fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry. .. |
|||
Mold Temperature | 70.0 - 90.0 °C | 158 - 194 °F | |
Plastcom SLOVAMID 66 GF 25 FRG 5 TS PA66, 25% glass fibre, flame retardant FeaturesPA 66 for injection moulding, chemically reinforced with 25% glass fibre and non-halogen flame retardant, with heat resistance and nonflammability, achieves V 0 in accordance with UL 94. Non.. |
|||
Mold Temperature | 70.0 - 90.0 °C | 158 - 194 °F | |
Plastcom SLOVAMID 66 GF 35 FRI 3 Polyamide 66, 35% Glass Fiber, Halogen Free Flame Retardant FeaturesPA 66 for injection moulding, chemically reinforced with 35% glass fiber and non-halogen flame retardant, with heat and flammability resistance, achieves V-0 in accordance with UL 94. Non-h.. |
|||
Mold Temperature | 80.0 - 90.0 °C | 176 - 194 °F | |
Plastcom SLOVAMID 66 GF 50 TS PA 66 reinforced with 50% glass fibre, thermal stability Features: Chemically reinforced with 50% glass fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry... |
|||
Mold Temperature | 70.0 - 90.0 °C | 158 - 194 °F | |
Plastcom SLOVAMID® 6 GF 40 HI PA6 reinforced with glass fiber, improved impact strength PA 6 for injection molding, reinforced with 40% glass fiber, impact modified. Application: impacted moldings and moldings with higher strength applied in automotive, electrical, engineering and cons.. |
|||
Mold Temperature | 50.0 - 90.0 °C | 122 - 194 °F | DAM |
DuPont Performance Polymers Zytel® 7335F NC010 Nylon 6
(Unverified Data**) Zytel® 7335F NC010 is a nucleated, lubricated polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Mold Temperature | 70.0 - 90.0 °C | 158 - 194 °F | Start Point: 80°C |
Kingfa LONOY 1600 PC/PBT Alloy Features:Excellent balance propertiesGood weather resistanceGood size stabilitySmooth surfaceUniform colorApplications:Injection moldingAutomobile bumperAutomobile interior/exterior trim partsBusine.. |
|||
Mold Temperature | 60.0 - 90.0 °C | 140 - 194 °F | Injection Molding |
LG Chemical LUMAX HR5107 PBT+ABS+GF10%, Heat Resistance Description: Injection Molding Grade, PBT+ABS+GF10%, Heat ResistanceApplication: E&E (CD ROM Tray)CAS: 9003-56-9, 65997-17-3, 24968-12-5, 25038-59-9 and 9003-54-7Information provided by LG Chemical |
|||
Mold Temperature | 60.0 - 90.0 °C | 140 - 194 °F | |
LG Chemical LUPOS GP-2205NB General Purpose SAN, 20% Glass Fiber Reinforced, Dimensional Stability, Anti-Bacteria LUPOS resins are glass fiber reinforced styrene copolymers. LUPOS have improved strength, rigidity and dimensional stability. They offer excellent heat resistance, minimal mold shrinkage and have .. |
|||
Mold Temperature | 70.0 - 90.0 °C | 158 - 194 °F | Start Point: 80°C |
Kingfa LONOY 2200 HT PC/PET Alloy Features:Excellent balance propertiesGood weather resistanceGood size stabilitySmooth surfaceUniform colorApplications:Injection moldingAutomobile bumperAutomobile interior/exterior trim partsBusine.. |
|||
Mold Temperature | 60.0 - 90.0 °C | 140 - 194 °F | Start Point: 60°C |
Kingfa MAC-601 AC PC/ABS Alloy Features:Excellent balance propertiesHigh impact strengthGood processing propertiesApplications:Injection moldingAutomobile instrument panelElectrical and electronic partsComputer and accessoriesHou.. |
|||
Mold Temperature | 40.0 - 90.0 °C | 104 - 194 °F | |
LG Chemical LUPOL TE-5104K Thermoplastic Elastomer Alloy, 10% Polymer Alloy, High Modulus LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive exterior parts.Information Provided by LG Chem |
|||
Mold Temperature | 70.0 - 90.0 °C | 158 - 194 °F | |
LATI Later 4 G/20 PBT, 20% Glass Fiber Reinforced Polybutylene Terephthalate (PBT) based compound. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast.. |
|||
Mold Temperature | 60.0 - 90.0 °C | 140 - 194 °F | |
Sax Polymers SAXATEC 4307 Acrylonitrile Styrene Acrylate SAXATEC 4307 is a high impact resistant, high viscosity and weatherable ASA injection molding grade, characterized by high mechanical strength and good processabilityInformation provided by SAX Poly.. |
|||
Mold Temperature | 50.0 - 90.0 °C | 122 - 194 °F | |
CP-Polymer-Technik Wellamid® 6600 HW Nylon 66, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Mold Temperature | 70.0 - 90.0 °C | 158 - 194 °F | |
CP-Polymer-Technik Wellamid® 6600 PA-66-HWV0CP UL-Licensed Nylon 66, Flame Protection, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Mold Temperature | 50.0 - 90.0 °C | 122 - 194 °F | |
CP-Polymer-Technik Wellamid® 6600 TLWCP Nylon 66, Flame Protection Grade V-2, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Mold Temperature | 50.0 - 90.0 °C | 122 - 194 °F | |
CP-Polymer-Technik Wellamid® 6600/506 HWCP Nylon 66, Impact Modified, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Mold Temperature | 50.0 - 90.0 °C | 122 - 194 °F | |
CP-Polymer-Technik Wellamid® 6600/508 HWUVCP Nylon 66, Impact Modified, UV Stabilized, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Mold Temperature | 50.0 - 90.0 °C | 122 - 194 °F | DAM |
DuPont Performance Polymers Zytel® FE4200 BK136 Nylon 66
(Unverified Data**) Zytel® FE4200 BK136 is a low die deposit polyamide 66 extrusion resin.Information provided by DuPont Performance Polymers |
|||
Mold Temperature | 60.0 - 90.0 °C | 140 - 194 °F | |
Eurostar Staramide RF006SXP PA66, 30% Glass Fiber Filled, Injection Molded Staramide RF006SXP is a 30% Glass Fiber Reinforced Polyamide 66 Injection Molding Resin (also known as RF1006HS)Information provided by Eurostar. |
|||
Mold Temperature | 50.0 - 90.0 °C | 122 - 194 °F | |
Eurostar Starflam BFR430A PA6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam BFR430A is a Flame Retardant, Glass Fiber Reinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Mold Temperature | 60.0 - 90.0 °C | 140 - 194 °F | |
CP-Polymer-Technik Wellamid® 6000 GS 50 HWUVCP 50% Glass Sphere Filled Nylon 6, UV Stabilized Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Mold Temperature | 80.0 - 90.0 °C | 176 - 194 °F | Injection Molding |
BASF Ultramid® B3M6 BK 23213 30% Mineral Filled PA6 (Dry) Description: 30% Mineral-filled injection molding grade for high impact industrial items having very high dimensional stability, such as automobile wheel covers.Information provided by BASF |
|||
Mold Temperature | 80.0 - 90.0 °C | 176 - 194 °F | Injection-molding |
BASF Ultramid® A3HG6 HR BK 23591 30% Glass Filled PA66 (Dry) Description: 30% glass-fiber reinforced injection-molding grade with enhanced hydrolysis resistance, e.g., for applications in vehicle cooling systems.Information provided by BASF |
|||
Mold Temperature | 80.0 - 90.0 °C | 176 - 194 °F | Injection Molding |
BASF Ultramid® B35G3 BK 00564 15% Glass Filled PA6 (Conditioned) Description: 15% glass fiber reinforced injection molding grade e.g. for internal gas pressure applications such as flashing direction switch gears, automobile mirror housings and wheels of mountain.. |
|||
Mold Temperature | 50.0 - 90.0 °C | 122 - 194 °F | DAM; Injection Molding |
DuPont Performance Polymers Zytel® FG7301 NC010 Nylon 6
(Unverified Data**) Zytel® FG7301 NC010 is a general purpose, unlubricated polyamide 6 resin for extrusion applications. It has been developed for consideration into applications such as parts for the food industry.In.. |
|||
Mold Temperature | 80.0 - 90.0 °C | 176 - 194 °F | Injection-molding |
BASF Ultramid® B3M6 BK60564 30% Mineral Filled PA6 (Dry) ultramid B3M6 BK60564 is a 30% mineral reinforced, pigmented black injection molding PA6 grade for industrial items requiring high impact strength and very high dimensional stability, excellent lase.. |
|||
Mold Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Injection Molding |
Arkema Group KYNAR FLEX® 2800-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low.. |