Physical Properties Metric English Comments
Density 1.33 g/cc
0.0480 lb/in³
STN EN ISO 1183-1
Plastcom PLASTAMID® 6 GF 30 031 TS PA6 reinforced with glass fiber, heat stabilized
PA 6 for injection molding, reinforced with 30% glass fiber, heat stabilized, better surface appearance of injection moldings. Decrease in tensile strength by 50 % after 5000 hours at 170°C. Used f..
Density 1.33 g/cc
0.0480 lb/in³
ISO 1183
SABIC Innovative Plastics Lexan® FXE4472L PC (Asia Pacific)
Lexan* FXE4472L is a 20% glass filled, impact modified polycarbonate with excellent light-shield capability. It is designed for high flow, superior surface appearance, enhance release and good impac..
Density 1.33 g/cc
0.0480 lb/in³
ISO 1183
SABIC Innovative Plastics Lexan® ML3042 PC (Europe-Africa-Middle East)
LEXAN ML3042 offers an extremely low light transparency in combination with a very high reflection. This product is ideally suited for lighting reflectors.
Density 1.33 g/cc
0.0480 lb/in³
Eastman Eastapak 7352 PET  (discontinued **)
Unreinforced Low IV. ISO data as provided by the manufacturer, Eastman Chemical.This product is discontinued; 2003.
Density 1.33 g/cc
0.0480 lb/in³
DIN 53479; ASTM D792
Kolon NOPLA® KE911 PEN-PET Copolyester
NOPLA® is an advanced PEN-PET copolyester which can be used for bottle, sheet & injection molding applicationsUV protection & prolonged outdoor durability, enhanced gas barrier, outstanding impac..
Density 1.33 g/cc
0.0480 lb/in³
DIN EN ISO 1183-1
Kraiburg TPE COPEC® CC8OCN Thermoplastic Elastomer, adhesion to ABS, PC and PC/ABS
The VS/AD1 Series is recommended for applications in the consumer electronics section. The compounds feature an exceptionally silky and velvety surface, accompanied by excellent adhesion properties ..
Density 1.33 g/cc
0.0480 lb/in³
ASTM D792
Techmer ES Elastoblend® PA6 GF30 IM HS L 30% Glass Filled (Conditioned)
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Impact Modifier Features: Impact ModifiedProcessing Method: Injection MoldingI..
Density 1.33 g/cc
0.0480 lb/in³
ISO 1183
SABIC Innovative Plastics LNP Lubricomp UL004AS PPA (Europe-Africa-Middle East)
Internally lubricated Polyphthalamide compound, countaining PTFEThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Density 1.33 g/cc
0.0480 lb/in³
ASTM D792
SABIC Innovative Plastics LNP STAT-KON DE0049P PC (Asia Pacific)
LNP* Stat-kon* DE0049P is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Exceptional Processing, Flame Retardant.
Density 1.33 g/cc
0.0480 lb/in³
ISO 1183
SABIC Innovative Plastics LNP STAT-KON DFD02EXC PC (Europe-Africa-Middle East)
LNP* Stat-kon* DFD02EXC is a compound based on Polycarbonate resin containing Glass Fiber, Carbon Powder. Added features of this material include: Electrically Conductive.
Density 1.33 g/cc
0.0480 lb/in³
ASTM D792
SABIC Innovative Plastics LNP STAT-KON DX04489C PC
LNP STAT-KON* DX04489C is a high modulus compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Con..
Density 1.33 g/cc
0.0480 lb/in³
ASTM D792
Techmer ES HiFill® PA4/6 CF40 IM HS 40% Carbon Filled (Dry)
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 40% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedInformation provided by TP Composites..
Density 1.33 g/cc
0.0480 lb/in³
ASTM D792
Techmer ES HiFill® PA6/6 GF10 TL10 BK 10% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by Weight Additive: Heat Stabilizer and PTFE Lubricant(10%)Features: Lubricated and Heat Stabiliz..
Density 1.33 g/cc
0.0480 lb/in³
ISO 1183
SABIC Innovative Plastics LNP THERMOCOMP DC006 PC (Asia Pacific)
LNP THERMOCOMP* DC006 is a compound based on Polycarbonate resin containing Carbon Fiber.This product is also known as Thermocomp* DC-1006.
Density 1.33 g/cc
0.0480 lb/in³
ISO 1183
SABIC Innovative Plastics LNP THERMOCOMP DF004ER PC (Europe-Africa-Middle East)
LNP* Thermocomp* DF004ER is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release.
Density 1.33 g/cc
0.0480 lb/in³
ISO 1183
SABIC Innovative Plastics LNP THERMOCOMP LC003E PEEK
LNP THERMOCOMP* LC003E is a compound based on Polyetheretherketone resin containing 15% Carbon Fiber. Added features of this material include: Easy Molding, Electrically Conductive
Density 1.33 g/cc
0.0480 lb/in³
ISO 1183
SABIC Innovative Plastics LNP THERMOCOMP ZF006 PPE+PS (Europe-Africa-Middle East)
LNP* THERMOCOMP* ZF006 is a compound based on PPE+PS Blend resin containing Glass Fiber
Density 1.33 g/cc
0.0480 lb/in³
ISO 1183
SABIC Innovative Plastics LNP Verton MX03017 PP (Europe-Africa-Middle East)
LNP* VERTON* MX03017 is a compound based on Polypropylene resin containing Glass Fiber, Long Glass Fiber. Added features of this material include: Chemically Coupled.This data was supplied by SABIC..
Density 1.33 g/cc
0.0480 lb/in³
ASTM D792
Techmer ES HiFill FR® PP CO E FR
Availability: North AmericaForms: PelletsFeatures: Flame Retardant and CopolymerProcessing Method: ExtrudedInformation provided by TP Composites, Inc.
Density 1.33 g/cc
0.0480 lb/in³
ASTM D792
SABIC Innovative Plastics LNP THERMOTUF VX00585 PA 66
LNP* Thermotuf* VX00585 is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: High Impact.
Density 1.33 g/cc
0.0480 lb/in³
ASTM D792
SABIC Innovative Plastics LNP THERMOTUF VX00585 PA 66 (Asia Pacific)
LNP* Thermotuf* VX00585 is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: High Impact.
Density 1.33 g/cc
0.0480 lb/in³
ISO 1183
SABIC Innovative Plastics LNP VERTON MV00ASXC PP (Europe-Africa-Middle East)
LNP* VERTON* MV00ASXC is a compound based on PP resin containing Long Glass Fiber. Added features include; Chemically Coupled, Heat Stabilized.
Density 1.33 g/cc
0.0480 lb/in³
Ex-Tech Plastics VersaTech™ APET
Ex-Tech VersaTech™ APET has exceptional properties such as visual transparency high heat distortion and it has good resistance to mineral oils, solvents and acids.Characteristics:TransparentExcepti..
Density 1.33 - 1.37 g/cc
0.0480 - 0.0495 lb/in³
ISO R 1184
Fainplast Compounds KL 84/1 Flexible PVC, Insulation for High Temperatures Lead Free
General purposes flame retardant
Density 1.33 - 1.37 g/cc
0.0480 - 0.0495 lb/in³
ISO R 1183
Fainplast Compounds PK 100 Flexible PVC, Lead Free
Semi-rigid extrusion for handrail
Density 1.33 g/cc
0.0480 lb/in³
Arlon CP-493C Bulk Compound
This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Di..
Density 1.33 g/cc
0.0480 lb/in³
ISO 1183
BASF Ultramid® 1703-2 BK ND3007 25% Glass Filled PA66 (Dry)
Ultramid 1703-2 BK ND3007 is a 25% glass reinforced, heat stabilized injection molding nylon 6/6.
Density 1.33 g/cc
0.0480 lb/in³
ISO 1183
Celanese Hostaform® S 9243 XAP² ™ LS POM, Impact Modified
POM copolymer, modifiedInformation provided by Celanese
Density 1.33 g/cc
0.0480 lb/in³
ISO 1183
Celanese Hostaform® S 9243 XAP2™ LS POM, Impact Modified
POM copolymer, modifiedIt is normally not necessary to dry HOSTAFORM. However, should there be surface moisture (condensate) on the molding compound as a result of incorrect storage, drying is requi..
Density 1.33 g/cc
0.0480 lb/in³
DAM; ISO 1183
DuPont Performance Polymers Zytel® 70G25HSL NC010 Nylon 66  (Unverified Data**)
25% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G25HSL NC010 is a 25% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perform..