SABIC Innovative Plastics LNP Thermotuf P1000J5 PA 6 (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP Thermotuf
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP Thermotuf P1000J5 PA 6 (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* THERMOTUF* P1000J5 is a compound based on PA 6 resin containing Impact Modifier. Added features include: High Impact.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.017 cm/cm
0.017 in/in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 35.0 MPa
5080 psi
5 mm/min; ISO 527
Elongation at Yield 3.7 %
3.7 %
5 mm/min; ISO 527
Tensile Modulus 1.40 GPa
203 ksi
1 mm/min; ISO 527
Flexural Yield Strength 43.0 MPa
6240 psi
2 mm/min; ISO 178
Flexural Modulus 1.20 GPa
174 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 45.0 kJ/m²

@Temperature 23.0 °C
21.4 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C
122 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af