Dow Corning 3-3602 Polymer 80,000 CS

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Dow Corning
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning 3-3602 Polymer 80,000 CS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polydimethylsiloxane polymer with terminated, curable silanol functionality, viscosity= 80,000 cp.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 0.975 g/cc

@Temperature 25.0 °C
0.975 g/cc

@Temperature 77.0 °F
Viscosity 80000 cP
80000 cP
Dynamic
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month