Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | ASTM C518 |
Rogers Corporation XT/duroid™ 8000 Thermoplastic Laminate, Circuit Material XT/duroid™ 8000 thermoplastic circuit materials provide an excellent solution for printed circuit board applications used in demanding environmental conditions. XT/duroid 8000 circuit materials ar.. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | |
Permabond ET510 Epoxy Resin PERMABOND ET510 is a two-part, 1:1 mixable epoxy adhesive. ET510 is a semi-flexible toughened epoxy adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plas.. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | ASTM E1461 |
Park Electrochemical Nelco® N4000-13 BC® Buried Capacitance™, High-Speed Multifunctional Epoxy Laminate and Prepreg The Nelco N4000-13 series is an enhanced epoxy resin system engineered to provide both outstanding thermal and high signal speed / low signal loss properties. The Nelco N4000-13 BC® is offered as a.. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | ASTM E1461 |
Park Electrochemical Nelco® N4000-13 EP™ BC® Buried Capacitance™, High-Speed Multifunctional Epoxy Laminate and Prepreg Nelco N4000-13 EP™ is an enhanced epoxy resin system engineered for today’s leadfree requirements where multiple solder reflow at temperatures approaching 260ºC are required. N4000-13 EP provides.. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | ASTM E1461 |
Park Electrochemical Nelco® N4000-13 High-Speed Multifunctional Epoxy Laminate and Prepreg The Nelco® N4000-13 series is an enhanced epoxy resin system engineered to provide both outstanding thermal and high signal speed / low signal loss properties. N4000-13 SI® is excellent for applic.. |
|||
Thermal Conductivity | 0.350 W/m-K @Temperature 23.0 °C |
2.43 BTU-in/hr-ft²-°F @Temperature 73.4 °F |
Along flow; ISO/CD 22007-4 |
Victrex® PEEK 150GL15 Polyetheretherketone, 15% Glass Fibre Reinforced Product Description:High performance thermoplastic material, 15% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food conta.. |
|||
Thermal Conductivity | 0.350 W/m-K @Temperature 23.0 °C |
2.43 BTU-in/hr-ft²-°F @Temperature 73.4 °F |
Along flow; ISO/CD 22007-4 |
Victrex® PEEK 150GL20 Polyetheretherketone, 20% Glass Fibre Reinforced Product Description:High performance thermoplastic material, 20% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food conta.. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | Along flow; ISO 22007-4 |
Victrex® PEEK 150GL30 30% Glass Fiber Reinforced Product Description: High performance thermoplastic material, 30% glass fibre reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact c.. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | Along flow; ISO 22007-4 |
Victrex® PEEK 450G General Purpose Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, standard flow, FDA food contac.. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | Along flow; ISO 22007-4 |
Victrex® PEEK 450GL20 Polyetheretherketone, 20% Glass Fibre Reinforced Product Description:High performance thermoplastic material, 20% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, .. |
|||
Thermal Conductivity | 0.350 - 0.965 W/m-K | 2.43 - 6.69 BTU-in/hr-ft²-°F | Average value: 0.717 W/m-K Grade Count:8 |
Overview of materials for Polytetrafluoroethylene (PTFE), Bronze Filled This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Bronze Filled". Each property range of values reported is minimum and ma.. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 19/CF/30 Polyamide 46, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 19-7319 Polyamide 46, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive.. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | ASTM D177 |
Manifattura Cattaneo VESPEL® SP1 Polyimide Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 1105/GF/20/EM PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.Dynamic stressed parts at high movement velocity.Ch.. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | ISO 8302 |
Eurostar Starflam AFR682A1 PA66, Mineral Reinforced, Flame Retardant, Injection Molding Starflam AFR682A1 is a Flame Retardant, Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | ISO 8302 |
Eurostar Starflam AFR682B1 PA66, Mineral Reinforced, Flame Retardant, Injection Molding Starflam AFR682B1 is a Flame Retardant, Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | ISO 8302 |
Eurostar Starflam AFR662B1 PA66, Mineral Reinforced, Flame Retardant, Injection Molding Starflam AFR662B1 is a Flame Retardant, Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | DIN 52 612 |
Brandenburger S 5000 Ablation Material for Aeronautics and Space Aviation Information provided by Brandenburger Isoliertechnik GmbH&Co. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | ASTM C 177 |
Adamas Adalon® 406 PTFE, 15% PEEK Information provided by Adamas, HPM |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultramid® B3ZG6 30% Glass Filled PA6 (Conditioned) Ultramid B3ZG6 is an impact-modified, 30% glass fiber reinforced injection molding PA6 grade for industrial items having very high impact strength and rigidity. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultramid® B3ZG6 BK 30564 30% Glass Filled PA6-1 (Conditioned) Description: Impact-modified and 30% glass fiber reinforced injection-molding grade for technical articles of very high stiffness and toughness, for instance, for vehicle airbag housings and suitcas.. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultramid® A3EG6 30% Glass Filled PA66 (Dry) Ultramid A3EG6 is a 30% glass fiber reinforced injection molding PA66 grade for machinery components and housings of high stiffness and dimensional stability. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultramid® A3WG6 BK 00564 30% Glass Filled PA66 (Conditioned) Description: 30% glass-fiber reinforced and heat aging resistant injection-molding grade for machine elements and housings of high stiffness and dimensional stability such as lamp socket housings, f.. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | |
Trelleborg Emerson & Cuming Stycast® 2741-15 Two-Component Epoxy Flexible Encapsulant Emerson & Cuming 2741-15 Stycast® Two-Component Epoxy Flexible EncapsulantDescriptionElectronic embedment and sealing of metals, ceramics, and plastics. Protection of stress sensitive components wh.. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultramid® B3WG5 25% Glass Filled PA6 (Dry) Description: 25% glass-fiber reinforced and heat aging resistant injection-molding grade, for instance, for fan impeller glass-fiber reinforced injection-molding grade for industrial articles and el.. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultramid® B3WG5 BK 00654 PA6 25% Glass Filled BK (Dry) Description: 25% glass-fiber reinforced and heat aging resistant injection-molding grade, for instance, for fan impeller glass-fiber reinforced injection-molding grade for industrial articles and el.. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | Along Flow; ISO 22007-4 |
Victrex® PEEK 150GL30 Black Polyetheretherketone, 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact co.. |