Polymer Property : Linear Mold Shrinkage = 0.0050 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
ASTM D955
Nylene® PA6 Glass Filled 5213 HS Nylon 6
13% Glass Filled; Property data for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
With Flow; ISO 2577
Polykemi AB POLYblend 65CI PC/ABS-Blend
Information provided by Polykemi AB
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ASTM D955
Polymer Resources PC/ABS-GP1-[color]-UV General Purpose PC/ABS Alloy, UV-stabilized
PC/ABS Alloy, General Purpose, UV-stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provide..
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ASTM D955
Polymer Resources PC-GP4-[color]-5 Polycarbonate, FDA-compliant Feedstocks, Easy Flow
Polycarbonate, FDA-compliant Feedstocks, Easy FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr..
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ASTM D955
Polymer Resources PPX-GP4 Modified-PPO, General Purpose
Modified-Polyphenylene Oxide, General Purpose, 210F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati..
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
48 hours after molding; ISO 294-3/4
Mytex Polymers AS319LW-01US Thermoplastic Polyolefin, 19% Talc Filled
AS319LW-01US is a compounded thermoplastic polyolefin (TPO) designed for exterior automotive applications requiring cold temperature impact, processability and paintability. Available in natural, g..
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ASTM D955
Polymer Resources PPX-GP2 Modified PPO, General Purpose with HDT of 250 F  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
Custom Resins Norpex® SE1 PPE (Polyphenylene Ether)  (discontinued **)
High Performance FR. Properties for dry as molded samples.Data provided by the manufacturer
Linear Mold Shrinkage 0.0050 - 0.0080 cm/cm
0.0050 - 0.0080 in/in
0.125 in, DAM; ASTM D955
Ravago Manufacturing Americas Hylon® N1013TL Nylon 6/6 (Cond)  (discontinued **)
Information provided by Ravago.
Linear Mold Shrinkage 0.0050 - 0.010 cm/cm
0.0050 - 0.010 in/in
Lehmann & Voss LUVOCOM® 1105-7336/GY7016 PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
Linear Mold Shrinkage 0.0050 - 0.0080 cm/cm
0.0050 - 0.0080 in/in
ASTM D955
Mitsubishi Iupilon® E2001R 5 MFI FDA Compliant Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ASTM D955
Star Plastics PC1212FRR Molding Grade PC FR
Information provided by Star Plastics, Inc.
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ASTM D955
Star Plastics PC20NBR Molding Grade PC with Release
Information provided by Star Plastics, Inc.
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ASTM D955
Star Plastics PC731 Molding Grade PC
Information provided by Star Plastics, Inc.
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ISO 294-4
Styrolution Novodur® H604 ABS
Novodur H604 is a high heat injection molding grade with enhanced chemical resistance, especially suitable for being painted.Information provided by Styrolution
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
Tisan TISAKRIL® UNR ABS
TISAKRIL has a wide area of application in automotive, electronics, computer, construction, and furniture industries. General Specifications include: High surface luminosityEasy processabilityDimens..
Linear Mold Shrinkage 0.0050 - 0.0090 cm/cm
0.0050 - 0.0090 in/in
ISO 294-4
Wellman Wellamid® GF13-66 22LH-N 13% Glass Fiber Reinforced Nylon 66, Lubricated & Heat Stabilized
Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data ..
Linear Mold Shrinkage 0.0050 - 0.0090 cm/cm
0.0050 - 0.0090 in/in
ISO 294-4
Wellman Wellamid® GF13-66 XE-N 13% Glass Fiber Reinforced Nylon 66, Lubricated & Heat Stabilized
Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data ..
Linear Mold Shrinkage 0.0050 - 0.0080 cm/cm
0.0050 - 0.0080 in/in
ISO 2577
Polyram RamShine PS580 High Impact Polystyrene, Flame Retardant
Flame retardant V-0, high impact polystyrene for injection molding applications.Information provided by Polyram.
Linear Mold Shrinkage 0.0050 - 0.015 cm/cm

@Thickness 3.175 mm
0.0050 - 0.015 in/in

@Thickness 0.1250 in
ASTM D955
A. Schulman SCHULAMID® 66 MK20HI 20% Mineral Reinforced, Impact Modified Nylon 66
Information provided by A. Schulman.
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm

@Thickness 3.17 mm
0.0050 - 0.0070 in/in

@Thickness 0.125 in
ASTM D955
RTP Company RTP 2599 X 87260 C Polycarbonate/ABS Alloy (PC/ABS), Carbon Nanotube - ESD Protection - Electrically Conductive
Linear Mold Shrinkage 0.0050 cm/cm

@Thickness 3.17 mm
0.0050 in/in

@Thickness 0.125 in
ASTM D955
Plastics Group Polifil® 78MRGF Glass Fiber and Mineral Reinforced Nylon 6/6 (DAM)
Polifil® GFN/MRN 6/6 reinforced series of compounds offer superior strength, rigidity and creep resistance. Glass fibers provide excellent thermal and dimensional stability while maintaining good h..
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ASTM D 955
Cossa Polimeri ESTABLEND CR Polycarbonate ABS Blend
Polycarbonate and Acrylonitrile Butadiene Styrene blend for chromium plating, painting and metallizationGood impact resistance, good thermal resistanceInformation provided by Cossa Polimeri S.r.l.
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ASTM D 955
Cossa Polimeri ESTACARB 1060 V0 HF Flame Retardant Polycarbonate
Flame retardant class V0, opaque, antimony, chlorine and bromine free, high impact resistance, high thermal resistance, good melt flow rate, good processability, good light resistanceInformation pro..
Linear Mold Shrinkage 0.0050 cm/cm

@Thickness 4.00 mm
0.0050 in/in

@Thickness 0.157 in
CP-Polymer-Technik Wellamid® 6000 MF 30 HWCP 30% Milled Glass Fiber Nylon 6, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
Linear Mold Shrinkage 0.0050 cm/cm

@Thickness 4.00 mm
0.0050 in/in

@Thickness 0.157 in
CP-Polymer-Technik Wellamid® 6600 MRGV 25/15 HWCP 25% Mineral and 15% Glass Fiber Nylon 66, Heat Stabilized, Conditioned
Information provided by CP-Polymer-Technik GmbH & Co. KG
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ASTM D955
Diamond Polymers PC-1900 Polycarbonate
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ASTM D955
Beijing Chemical Industry KAIFA® M105 MPPO Resin
Flame retardant, Thermal resistantInformation provided by Beijing Chemical Industry Research Institute (Group)
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ASTM D955
Asahi Kasei Xyron® 540Z Modified Polyphenylene Ether
Flame RetardantInformation provided by Asahi Kasei
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
ASTM Data MD (Dry)
BASF Capron® HPN 9315G HS BK-102 Impact Modified, 15% Glass-Filled Nylon 6 (Conditioned)  (discontinued **)<
Capron HPN 9315G HS BK-102 is a 15% glass reinforced impact modified, heat stabilized, pigmented black, nylon 6 injection molding grade resin. It is in the High Productivity Nylon Series developed ..