Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Mold Temperature 80.0 °C
176 °F
optimum; Injection Molding
DuPont Performance Polymers Crastin® S650FR BK851 PBT  (Unverified Data**)
Crastin® S650FR is an unreinforced, black, flame retardant polybutylene terephthalate for injection molding.Information provided by DuPont Performance Polymers
Mold Temperature 80.0 - 120 °C
176 - 248 °F
Lehmann & Voss LUVOCOM® 50-7446 Polycarbonate, with carbon fiber, PTFE, lubricant modified
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi..
Mold Temperature 80.0 - 100 °C
176 - 212 °F
Injection Molding
LG Chemical LUMID HI5001AS PA6/PO, High Barrier Property, CaCl2 Resistance, High Impact
Feature: Injection Molding, PA6/PO, High Barrier Property, CaCl2 Resistance, High ImpactApplication: Automotive (Fuel System Tube)CAS No. 25038-54-4, 9010-79-1, 9002-88-4 and 105-60-2Information pro..
Mold Temperature 80.0 - 100 °C
176 - 212 °F
Injection Molding
LG Chemical LUMID HI5083A(W) PA6/ABS+MF8%, High Impact
Feature: Injection Molding, PA6/ABS+MF8%, High ImpactApplication: Electric/Electronic Components (Shaver Die)CAS No. 25038-54-4, 9003-56-9, 9003-54-7 and 14807-96-6Information provided by LG Chemica..
Mold Temperature 80.0 - 100 °C
176 - 212 °F
Injection Molding
LG Chemical LUMID LW4403A(W) PA66+GF/MF40%, Low Warpage
Feature: Injection Molding, PA66+GF/MF40%, Low WarpageApplication: Automotive (Timing Belt Cover)CAS No. 25038-54-4, 13983-17-0 and 65997-17-3Information provided by LG Chemical
Mold Temperature 80.0 - 120 °C
176 - 248 °F
suitable temperature 90-120°C
Gromax PET 9030-104E 30% Glass/Mineral Filled
Product Description: PET glass 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent mechanic and chemical property Excellent weatherability Excellent wear..
Mold Temperature 80.0 - 120 °C
176 - 248 °F
Lanxess Durethan® BG 30 X W1 000000 Nylon 6, Glass Fiber Reinforced
PA 6, 30% glass fibers/glass spheres, injection molding, low tendency to warp, weather stabilizedInformation provided by LANXESS.
Mold Temperature 80.0 - 120 °C
176 - 248 °F
Injection Molding
LG Chemical LUPOY EF1006F PC, Halogen Free, Flame Retardant, High Heat Resistance
Description: Injection Molding, PC, Halogen Free Flame Retardant, High Heat ResistanceApplication: IT/OA Housing and Components (Adaptor)CAS: 103598-77-2Information provided by LG Chemical
Mold Temperature 80.0 - 120 °C
176 - 248 °F
ISO 294
Gromax BFG30-EN04B2 Nylon 6 36% Glass Filled (Conditioned)
Information provided by Gromax Enterprises Corp.
Mold Temperature 80.0 - 100 °C
176 - 212 °F
LATI Latilub 87/28-20T PC, PTFE Filled
Self-lubricating product based on Polycarbonate (PC). PTFE.Information provided by Lati Industria Termoplastici S.p.A.
Mold Temperature 80.0 - 100 °C
176 - 212 °F
LATI Latishield 66-10A G/15 PA66, Steel/Glass Fiber Reinforced
EMI shielding product based on Polyamide 66 (PA66). Steel fibers. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind..
Mold Temperature 80.0 - 100 °C
176 - 212 °F
Solvay TECHNYL® C 218 V 50 PA6, 50% glass fiber, Eh 0
Description: TECHNYL C 218 V50 is a polyamide 6 reinforced with 50% of glass fiber with excellent thermal stabilityColors: it is supplied in natural color and black color.Available in: Latin America..
Mold Temperature 80.0 - 95.0 °C
176 - 203 °F
Injection Molding
Styrolution Luran® S KR 2858 GS Colored 15% Glass Filled ASA
Description: Glass-reinforced grade with high stiffness and heat distortion resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
Mold Temperature 80.0 - 120 °C
176 - 248 °F
Surface
Solvay Technyl® A 216 V30 Nylon 66, 30% Glass Fiber, EH50
Polyamide PA66, reinforced with 30% of glass fiber, for injection molding.Technyl A 216 V30 is used in all sectors of industry, offering an excellent combination between thermal and mechanical prope..
Mold Temperature 80.0 °C
176 °F
Injection Molding; ISO 10724
Covestro Bayblend® T90 HT Polycarbonate + ABS
Injection molding gradehigh heat resistanceVicat/B 120 = 135 °Cball indentation temperature = 125 °Ceasy flowsuitable for supporting life componentsPreprocessingMax. Water content
Mold Temperature 80.0 - 120 °C
176 - 248 °F
Covestro Makrolon® 6265 Polycarbonate, Flame Retardant Grade
ISO 7391-PC,MFR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 19 cm3/10 minFlame retardantUL 94V-0/1.5 mmLow viscosityEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in opaque co..
Mold Temperature 80.0 - 120 °C
176 - 248 °F
Covestro Makrolon® LED2045 Polycarbonate
ISO 7391-PC,MRT,(,,)-24-9Global gradeMVR (250 °C/2.16 kg) 16.5 cm3/10minLight guidesPC with highest transmissionLow viscosityEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable ..
Mold Temperature 80.0 - 100 °C
176 - 212 °F
CP-Polymer-Technik Wellamid® 6600 CF20 HWCP 20% Carbon Fiber Nylon 66, Heat Stabilized, Conditioned
Information provided by CP-Polymer-Technik GmbH & Co. KG
Mold Temperature 80.0 °C
176 °F
optimum
DuPont Performance Polymers Crastin® T835FRUV NC010 PBT
Crastin® T835FRUV NC010 is a 5% glass fiber reinforced, toughened, flame retardant polybutylene terephthalate resin for injection molding. (precommercial code = Crastin® CE2402)Information provide..
Mold Temperature 80.0 - 100 °C
176 - 212 °F
Akro-Plastic Akromid® B3 GF 60 (2476) PA 6 Dry, 60% Glass Filled
AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur..
Mold Temperature 80.0 - 120 °C
176 - 248 °F
Celanese Thermx® CG043 NC010 PCT
Thermx® CG043 NC010 (formerly Thermx® CG043-0033L) is a 40% glass reinforced polycyclohexylenedimethylene terephthalate resin.Celenese acquired the Thermx product line from DuPont in 2010.
Mold Temperature 80.0 - 90.0 °C
176 - 194 °F
Injection-molding
BASF Ultramid® A3X2G7 35% Glass Filled PA66 (Dry)
Ultramid A3X2G7 is a 35% glass fiber reinforced injection molding PA66 grade with improved flame retardance and enhanced long-term stability. Flame retardant based on red phosphorus; very high stif..
Mold Temperature 80.0 - 90.0 °C
176 - 194 °F
Injection Molding
BASF Ultramid® B3M6 BK 23213 30% Mineral Filled PA6 (Conditioned)
Description: 30% Mineral-filled injection molding grade for high impact industrial items having very high dimensional stability, such as automobile wheel covers.Information provided by BASF
Mold Temperature 80.0 °C
176 °F
Optimal
BASF Ultramid® B3WG6 GP BK 23210 30% Glass Filled PA6 (Conditioned)
Description: 30% Glass fiber reinforced and heat aging resistant injection molding grade used e.g. for automobile manifold.Information provided by BASF
Mold Temperature 80.0 °C
176 °F
for test specimens; ISO 294
Lanxess Pocan® C 1206 000000 PET + PC
PET + PC, non-reinforced, injection molding, improved impact strengthInformation provided by LANXESS.
Mold Temperature 80.0 °C
176 °F
optimum
DuPont Performance Polymers Crastin® CE2055 BK580 PBT  (Unverified Data**)
Crastin® CE2055 is an unreinforced, low viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
Mold Temperature 80.0 - 110 °C
176 - 230 °F
Injection Molding
LG Chemical LUPOY SC1004ML PC, High Impact
Description: Injection Molding, PC, General Purpose, High Impact, Good Coloring, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 9046-16-6Information provided by LG Chemical..
Mold Temperature 80.0 - 100 °C
176 - 212 °F
Injection Molding
DuPont Performance Polymers Delrin® FG100AL NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® FG100AL is a high viscosity, lubricated acetal homopolymer resin, containing an advanced system of lubrication. It has been developed for consideration into applications such as parts for t..
Mold Temperature 80.0 - 120 °C
176 - 248 °F
ISO 294
Gromax CFG33-QS11N1 Nylon 6 33% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.
Mold Temperature 80.0 °C
176 °F
for shrinkage test, Optimal
BASF Ultradur® B 4300 G10 50% Glass Filled PBT
Description: Injection-molding grades containing 50% of glass fibers, for industrial parts, rigid, tough and dimensionally stable, for example for program switches, thermostat parts, small-motor hou..