Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.70 GPa | 682 ksi | STN EN ISO 178 |
Plastcom PLASTAMID® 66 GF 20 PA66 reinforced with glass fiber PA66 for injection molding, reinforced with 20% glass fiber, for moldings used in the automotive, electrical, building, engineering and hobby industry - holders of electric hand tools, hobby tools, .. |
|||
Flexural Modulus | 4.70 GPa | 682 ksi | |
Plastcom SLOVAMID 66 GF 15 T 6 TS PA66, 15% glass fibre, 6% talc FeaturesChemically reinforced with 15% glass fibre and 6% of talc, suitable for mouldings with high strength and toughness also at low temperatures. Used in the automotive, engineering and electrica.. |
|||
Flexural Modulus | 4.70 GPa | 682 ksi | |
Plastcom SLOVAMID 66 GF 20 HI PA66, 20% glass beads FeaturesChemically reinforced with 20% glass beeds, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry. I.. |
|||
Flexural Modulus | 4.70 GPa | 682 ksi | STN EN ISO 178 |
Plastcom SLOVAMID® 66 GF 20 HTS PA6 reinforced with glass fiber, heat stabilized, hydrolysis resistant PA66 for injection molding, reinforced with 20% glass fiber, heat stabilized, hydrolysis resistant, for moldings used in the automotive, electrical, building, engineering and hobby industry - holder.. |
|||
Flexural Modulus | 4.70 GPa | 682 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® C4215HF PC+ABS (Europe-Africa-Middle East) Cycoloy C4215HF is a 15% glass reinforced, non-FR PC+ABS grade with high heat resistance, excellent strength and rigidity with good cosmetic apprearance. It combines good processability with a low s.. |
|||
Flexural Modulus | 4.70 GPa @Temperature 23.0 °C |
682 ksi @Temperature 73.4 °F |
ISO 178 |
DuPont Performance Polymers Crastin® HR5315HF BK503 PBT
(Unverified Data**) Crastin® HR5315HF is a 15% glass reinforced PBT with high flow (HF), moderately toughened, hydrolysis resistant (HR) resin. Excellent balance of properties between terminal pullout and impact resis.. |
|||
Flexural Modulus | 4.70 GPa | 682 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycolac® CRT3370 ABS (Europe-Africa-Middle East) CYCOLAC CRT3370 is a 17% glass reinforced injection moulding grade of ABS. It exhibits high rigidity and excellent dimensional stability combined with medium/high heat performance and good flow char.. |
|||
Flexural Modulus | 4.70 GPa @Temperature 90.0 °C |
682 ksi @Temperature 194 °F |
ASTM D790 |
LATI LARIL 13-V1KC Mineral Filled Polyphenylene Oxide (PPOm) (UL94V-1)
(Unverified Data**) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |
|||
Flexural Modulus | <= 4.70 GPa | <= 682 ksi | |
Reliance Industries Polypropylene - Talc filled Information provided by Reliance Industries |
|||
Flexural Modulus | 4.70 GPa | 682 ksi | cond., 2 mm/min; ISO 178-A |
Lanxess Durethan® BKV 130 DUS008 901510 Nylon 6, Glass Fiber Reinforced, Impact Modified PA 6, 30% glass fibers, injection molding, impact modifiedInformation provided by LANXESS. |
|||
Flexural Modulus | 4.70 GPa | 682 ksi | ISO 178 |
Solvay TECHNYL® A 218 S40 Black 21 N PA66, 40% glass spheres, DRY Description: Polyamide 66, reinforced with 40% of glass spheres, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECHNYL ® A 218 S40 is used in all sectors of ind.. |
|||
Flexural Modulus | 4.70 GPa | 682 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL V03505 PPE+HIPS Noryl* V03505 is a 35% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Flexural Modulus | 4.70 GPa | 682 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL V03505 PPE+HIPS (Europe-Africa-Middle East) Noryl* V03505 is a 35% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Flexural Modulus | 4.70 GPa | 682 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL V03550 PPE+HIPS Noryl* V03550 is a 35% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Flexural Modulus | 4.70 GPa | 682 ksi | ISO 178 |
Solvay TECHNYL® B 216 V30 Black 3 N PA66, 30% glass fiber, Conditioned Description: Copolyamide 66/6, reinforced with 30% of glass fiber, for injection molding.Available in: Asia Pacific and EuropeProduct Applications: TECHNYL® B 216 V30 is used in all sectors of in.. |
|||
Flexural Modulus | 4.70 GPa | 682 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® 815F PBT+PET PBT+PET, 15% Glass, Mold Release, Heat Stabilized, For food contact applications |
|||
Flexural Modulus | 4.70 GPa | 682 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP MX06402H PP LNP* THERMOCOMP* MX06402H is a compound based on Polypropylene resin containing 20% Glass Fiber. Added features of this material include: Heat Stabilized, Low Extractable. |
|||
Flexural Modulus | 4.70 GPa | 682 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp PFB42ES PA 6 (Europe-Africa-Middle East) LNP* THERMOCOMP* PFB42ES is a compound based on PA6 resin containing Glass Fiber, Glass Bead. Added features include: Easy Molding, Heat Stabilized.This data was supplied by SABIC-IP for the Europe-.. |
|||
Flexural Modulus | 4.70 GPa | 682 ksi | ISO 178 |
Solvay TECHNYL® A 216 S40 PA66, 40% glass spheres, DRY Description: Polyamide 66, reinforced with 40% of glass spheres, for injection molding.Available in: EuropeProduct Applications: TECHNYL ® A 216 S40 is used in all sectors of industry, offering a.. |
|||
Flexural Modulus | 4.70 GPa | 682 ksi | ISO 178-93 |
Wellman Wellamid® MR340 42H-NBK1 Nylon 6, 34% Mineral Reinforced All information provided by Wellman Engineered Resins. |
|||
Flexural Modulus | 4.70 GPa | 682 ksi | ISO 178 |
Unitika TERRAMAC HV-6250H Polylactic Acid (PLA) Foam, Extrusion, blow, and foam sheet grades. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Flexural Modulus | 4.70 GPa | 682 ksi | ASTM D790 |
Unitika UM-8400-20 Characteristics: High dimensional accuracy (circularity and planarity) Large warping resistance Low linear expansion coefficientInformation provided by Unitika Ltd. |
|||
Flexural Modulus | 4.70 GPa | 682 ksi | 2 mm/min; ISO 178 |
Eurostar Staramide PFB42ES PA6, Glass Fiber/Bead Filled, Injection Molded Starflam PFB42ES is a Glass Bead and Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Modulus | 4.70 GPa | 682 ksi | 2 mm/min; ISO 178 |
Eurostar Staramide PX05046 PA6, Glass Bead/Fiber Filled, Injection Molded Staramide XP05046 is Glass Bead and Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Modulus | 4.70 GPa | 682 ksi | ISO Data |
BASF Ultramid® 7423-2 NF3001 13% Glass Filled PA66 (Dry) Ultramid 7423-2 NF3001 is an impact modified, 13% glass reinforced, heat stabilized injection molding PA6/6. |
|||
Flexural Modulus | 4.70 GPa | 682 ksi | ISO 178 |
BASF Ultramid® B3ZG6 BK 30564 30% Glass Filled PA6-1 (Conditioned) Description: Impact-modified and 30% glass fiber reinforced injection-molding grade for technical articles of very high stiffness and toughness, for instance, for vehicle airbag housings and suitcas.. |
|||
Flexural Modulus | 4.70 GPa | 682 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 636 Nylon 6/6, Glass/Mineral Reinforced, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company.40% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 4.70 GPa | 682 ksi | ISO 178 |
CENTROPLAST CENTROCARB GF Polycarbonate 30% glass fiber CENTROCARB GF is a transparent or semi-transparent plastic, reinforced for high strength and impact resistance. It has a high tensile modulus of elasticity and is well suited for structural element.. |
|||
Flexural Modulus | 4.70 GPa | 682 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 627 Nylon 6/6, Mineral Reinforced Data provided by the manufacturer, ComAlloy International Company.20% Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 4.70 GPa | 682 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp PFB42EU PA 6 (Europe-Africa-Middle East) LNP* THERMOCOMP* PFB42EU is a compound based on PA 6 resin containing Glass Fiber, Glass Bead. Added features include Easy Molding, Heat Stabilized.This data was supplied by SABIC-IP for the Europe-.. |