Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 32.0 kJ/m² @Temperature -30.0 °C |
15.2 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® LG9020 PC+ABS Low Gloss Cycoloy. Available only in natural, to be custom color concentrated and UV stabilized at the molding press. |
|||
Izod Impact, Notched (ISO) | 32.0 kJ/m² | 15.2 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Lexan® FXG1414T PC Copolymer PC-siloxane copolymer in special ""Diamond Sparkle"" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance. |
|||
Izod Impact, Notched (ISO) | 32.0 kJ/m² @Temperature -30.0 °C |
15.2 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® HFD1413 PC Copolymer 11 MFR LEXAN High Flow Ductile Copolymer |
|||
Izod Impact, Notched (ISO) | 32.0 kJ/m² @Temperature -30.0 °C |
15.2 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® HFD1413 PC Copolymer (Asia Pacific) 11 MFR LEXAN High Flow Ductile Copolymer |
|||
Izod Impact, Notched (ISO) | 32.0 kJ/m² | 15.2 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Lexan® FXG1414T PC Copolymer (Asia Pacific) PC-siloxane copolymer in special ""Diamond Sparkle"" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance. |
|||
Izod Impact, Notched (ISO) | 32.0 kJ/m² @Temperature -30.0 °C |
15.2 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® HFD1413 PC Copolymer (Europe-Africa-Middle East) 11 MFR LEXAN High Flow Ductile Copolymer |
|||
Izod Impact, Notched (ISO) | 32.0 kJ/m² @Temperature -30.0 °C |
15.2 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® HFD1433 PC Copolymer 11 MFR LEXAN High Flow Ductile Copolymer UV stabilized, available in transparent colors only |
|||
Izod Impact, Notched (ISO) | 32.0 kJ/m² @Temperature -30.0 °C |
15.2 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® HFD1433 PC Copolymer (Asia Pacific) 11 MFR LEXAN High Flow Ductile Copolymer UV stabilized |
|||
Izod Impact, Notched (ISO) | 32.0 kJ/m² | 15.2 ft-lb/in² | 80*10*4mm, Cut; ISO 180/1A |
SABIC Innovative Plastics SABIC PPCOMPOUND 9712 PP SABIC® PPcompound 9712 is a mineral filled, impact modified polypropylene TPO. This material combines high impact resistance, scratch resistance, and heat stability with interior automotive UV st.. |
|||
Izod Impact, Notched (ISO) | 32.0 kJ/m² @Temperature 23.0 °C |
15.2 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP Stat-loy A3000Z ABS LNP* Stat-loy* A3000Z is a compound based on Acrylonitrile Butadiene Styrene resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for t.. |
|||
Izod Impact, Notched (ISO) | 32.0 kJ/m² @Temperature 23.0 °C |
15.2 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP Stat-loy A3000Z ABS (Asia Pacific) LNP* Stat-loy* A3000Z is a compound based on Acrylonitrile Butadiene Styrene resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for t.. |
|||
Izod Impact, Notched (ISO) | 32.0 kJ/m² | 15.2 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP TH0300A PUR LNP THERMOCOMP* TH0300A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity. |
|||
Izod Impact, Notched (ISO) | 32.0 kJ/m² | 15.2 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP TH0300A PUR (Asia Pacific) LNP THERMOCOMP* TH0300A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity. |
|||
Izod Impact, Notched (ISO) | 32.0 kJ/m² | 15.2 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP VERTON RV0079 PA 66 (Asia Pacific) LNP VERTON* RV0079 is a compound based on Nylon 66 resin containing Flame Retardant, Long Glass Fiber, Long Glass. Added features of this material include: Easy Molding. |
|||
Izod Impact, Notched (ISO) | 32.0 kJ/m² | 15.2 ft-lb/in² | ISO 180/1A |
Borealis Daplen™ EG203AE Polypropylene Compound Elastomer and Mineral Modified Daplen EG203AE is a 20% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen EG203AE is a material with excellent impact /stiffness ratio. Thanks to its low .. |
|||
Izod Impact, Notched (ISO) | 32.0 kJ/m² @Temperature -50.0 °C |
15.2 ft-lb/in² @Temperature -58.0 °F |
|
Dow DOWLEX™ IP-2580 Linear Low Density Polyethylene Next Generation DOWLEX® IP-2580 resin is an improved processing linear low density polyethylene resin designed for excellent flow and stiffness with freezer grade impact properties. DOWLEX IP-2580 .. |
|||
Izod Impact, Notched (ISO) | 32.0 kJ/m² @Temperature -50.0 °C |
15.2 ft-lb/in² @Temperature -58.0 °F |
|
Dow LDPE 993I Low Density Polyethylene DOW LDPE 993I resin is a low slip, medium molecular weight distribution homopolymer designed to offer good gloss and rigidity with excellent flow characteristics. This resin has good processability .. |
|||
Izod Impact, Notched (ISO) | 32.0 kJ/m² | 15.2 ft-lb/in² | ISO 180/A |
BASF Ultramid® B3ZG6 30% Glass Filled PA6 (Conditioned) Ultramid B3ZG6 is an impact-modified, 30% glass fiber reinforced injection molding PA6 grade for industrial items having very high impact strength and rigidity. |
|||
Izod Impact, Notched (ISO) | 32.0 kJ/m² @Temperature 23.0 °C |
15.2 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
BASF Ultramid® B3ZG6 BK 30564 30% Glass Filled PA6-1 (Conditioned) Description: Impact-modified and 30% glass fiber reinforced injection-molding grade for technical articles of very high stiffness and toughness, for instance, for vehicle airbag housings and suitcas.. |
|||
Izod Impact, Notched (ISO) | 32.0 kJ/m² | 15.2 ft-lb/in² | Conditioned; ISO 180/1A |
Addiplast Addinyl PMD 20090 Nylon 6, 40% Glass Filled Glass fiber reinforced, high resistance to frictionInformation provided by Addiplast. |
|||
Izod Impact, Notched (ISO) | 32.0 kJ/m² @Temperature -30.0 °C |
15.2 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® HFD1433 PC Copolymer (Europe-Africa-Middle East) 11 MFR LEXAN High Flow Ductile Copolymer UV stabilized, available in transparent colors only |