Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0050 - 0.0070 cm/cm | 0.0050 - 0.0070 in/in | |
Nylene® Norpex® AX20MR , 20% Mineral Reinforced Polyphenylene Ether Description: Norpex® AX20MR is a 20% mineral reinforced Polyphenylene Ether. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Res.. |
|||
Linear Mold Shrinkage | 0.0050 cm/cm | 0.0050 in/in | ASTM D955 |
Nylene® PA6 Glass Filled 5213 HS Nylon 6 13% Glass Filled; Property data for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation. |
|||
Linear Mold Shrinkage | 0.0050 - 0.0070 cm/cm | 0.0050 - 0.0070 in/in | ISO 294-4 |
Premix Thermoplastics PRE-ELEC® ESD 7140 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 7140 is a static dissipative thermoplastic masterbatch based on ABS. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 7140 has been developed for.. |
|||
Linear Mold Shrinkage | 0.0050 - 0.0070 cm/cm | 0.0050 - 0.0070 in/in | Across Flow; ISO 2577 |
Polykemi AB SCANTEC PC 85FR Polycarbonate, Flame Retardant, Halogen Free Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0050 - 0.0070 cm/cm | 0.0050 - 0.0070 in/in | ASTM D955 |
Polymer Resources PC-FR2A-D-[color]-3 Polycarbonate, Flame Retardant, Medium Flow, UV-stabilized Polycarbonate, Flame Retardant, Medium Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Linear Mold Shrinkage | 0.0050 - 0.0070 cm/cm | 0.0050 - 0.0070 in/in | ASTM D955 |
Polymer Resources PPX-FR1-[color]EN Modified PPO, UL 94 V-0 with HDT of 190 F, Extrusion Grade Process: ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Linear Mold Shrinkage | 0.0050 - 0.0070 cm/cm | 0.0050 - 0.0070 in/in | ASTM D955 |
Polymer Resources PPX-FR3 Modified-PPO, V-1 Flame Retardant Modified-Polyphenylene Oxide, V-1 Flame Retardant, 265F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-.. |
|||
Linear Mold Shrinkage | 0.0050 - 0.0070 cm/cm | 0.0050 - 0.0070 in/in | ASTM D955 |
Ravago Manufacturing Americas Hylex® P1025FRVNH Polycarbonate Available in North America Features: Flame Retardant, Halogen Free and High Flow RoHS Compliant Form: PelletsInformation provided by Ravago |
|||
Linear Mold Shrinkage | 0.0050 - 0.0070 cm/cm @Thickness 3.17 mm |
0.0050 - 0.0070 in/in @Thickness 0.125 in |
ASTM D955 |
RTP Company RTP 400 HI TFE 10 Polystyrene (PS), PTFE Lubricated - High Impact |
|||
Linear Mold Shrinkage | 0.0050 cm/cm @Thickness 3.17 mm |
0.0050 in/in @Thickness 0.125 in |
ASTM D955 |
RTP Company RTP 900 MG 10 Polysulfone (PSU), Milled Glass |
|||
Linear Mold Shrinkage | 0.0050 - 0.0070 cm/cm | 0.0050 - 0.0070 in/in | ASTM D955 |
Polymer Resources PC-FR1-D-[color]-3 Polycarbonate, Improved Flame Retardant, Low Flow, UV-stabilized Polycarbonate, Improved Flame Retardant, Low Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples... |
|||
Linear Mold Shrinkage | 0.0050 - 0.0070 cm/cm | 0.0050 - 0.0070 in/in | ASTM D955 |
Polymer Resources PC-GP1-TFE10 Polycarbonate, 10% PTFE, Wear Resistant, Low Flow Polycarbonate, 10% PTFE, General Purpose, Wear Resistant, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sample.. |
|||
Linear Mold Shrinkage | 0.0050 - 0.015 cm/cm | 0.0050 - 0.015 in/in | FRISETTA Test Method |
Nilit FRIANYL A63 HH-FK 2020 Nylon 6.6 for injection molding, 20% glass fiber and 20% glass ball reinforced Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Linear Mold Shrinkage | 0.0050 - 0.0080 cm/cm @Thickness 1.59 mm |
0.0050 - 0.0080 in/in @Thickness 0.0625 in |
plaque |
Dow Pellethane® 2102-90AR Polyurethane Elastomer, Polyester Polycaprolactone Based
(discontinued **) PELLETHANE® 2102-90AR elastomer is a polyester polycaprolactone based polyurethane elastomer which combines excellent resistance to fuels and oils with enhanced mold release, low compression set, a.. |
|||
Linear Mold Shrinkage | 0.0050 - 0.0080 cm/cm | 0.0050 - 0.0080 in/in | 0.125 in; ASTM D955 |
Ravago Manufacturing Americas Hylon® N1013L Nylon 6/6 (DAM)
(discontinued **) Information provided by Ravago. |
|||
Linear Mold Shrinkage | 0.0050 - 0.0070 cm/cm @Temperature 23.0 °C |
0.0050 - 0.0070 in/in @Temperature 73.4 °F |
ASTM D955 |
Kingfa JH830T Flame Retardant PC Features:UL V-0 @ 2.4mmExcellent balance propertiesHigh stiffnessGood size stabilityGood surfaceTransparentApplications:Controller switchLamp-chimneyTelecommunicationHousehold appliance cabinetInfor.. |
|||
Linear Mold Shrinkage | 0.0050 cm/cm | 0.0050 in/in | ASTM D955 |
Global PBT-325 Polybutylene Terephthalate Alloy Information provided by Global Polymers Corporation. |
|||
Linear Mold Shrinkage | 0.0050 cm/cm | 0.0050 in/in | ASTM D955 |
LG Chemical LUPOY HF-5000 High Flow PC/ABS Alloy, Unreinforced Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Linear Mold Shrinkage | 0.0050 - 0.0080 cm/cm | 0.0050 - 0.0080 in/in | 0.125; ASTM D955 |
LTL Color Compounds ColorFast® FRPBT150 PBT, 13% Glass-Filled, Flame Retarded 13% glass-filled V-0 rated PBTAll information provided by LTL Color Compounders, Inc. |
|||
Linear Mold Shrinkage | 0.0050 - 0.0080 cm/cm | 0.0050 - 0.0080 in/in | ASTM D955 |
Mitsubishi Iupilon® E2000R 5 MFI Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Linear Mold Shrinkage | 0.0050 - 0.0070 cm/cm | 0.0050 - 0.0070 in/in | ISO 294 |
Styron Pulse® 2000EZ PC/ABS Engineering ResinInformation provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Linear Mold Shrinkage | 0.0050 cm/cm @Thickness 3.175 mm |
0.0050 in/in @Thickness 0.1250 in |
ASTM D955 |
A. Schulman SCHULADUR® B GF15 15% Glass Fiber Reinforced PET Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0050 - 0.0090 cm/cm @Thickness 3.17 mm |
0.0050 - 0.0090 in/in @Thickness 0.125 in |
ASTM D955 |
RTP Company RTP 201 D TFE 5 Nylon 6/12 (PA), Glass Fiber - PTFE Lubricated |
|||
Linear Mold Shrinkage | 0.0050 - 0.020 cm/cm | 0.0050 - 0.020 in/in | ASTM D955 |
Cheng Yu Plastic T883GV25 Flame Retardant PBT, 25% Glass Fiber |
|||
Linear Mold Shrinkage | 0.0050 - 0.0080 cm/cm | 0.0050 - 0.0080 in/in | ASTM D955 |
Diamond Polymers ABS/PC 9901 Description: Injection Molding Grade, Very High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Linear Mold Shrinkage | 0.0050 cm/cm | 0.0050 in/in | |
Dow Tyril® 1000B SAN TYRIL® 1000B SAN copolymer offers the best balance of physical properties of all TYRIL grades. It also provides excellent processability and chemical resistance, superior heat resistance, and good .. |
|||
Linear Mold Shrinkage | 0.0050 cm/cm | 0.0050 in/in | MD; ASTM D955 |
Aclo Accutech Polyethylene HD0234G10UVL High Density Glass Reinforced UV Stabilized |
|||
Linear Mold Shrinkage | 0.0050 - 0.0070 cm/cm | 0.0050 - 0.0070 in/in | ASTM D955 |
Asahi Kasei Xyron® 540Z Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Linear Mold Shrinkage | 0.0050 cm/cm @Thickness 3.17 mm |
0.0050 in/in @Thickness 0.125 in |
ASTM D955 |
RTP Company RTP 175 Polypropylene (PP), Glass Fiber & Glass Bead Reinforced - Chemically Coupled |
|||
Linear Mold Shrinkage | 0.0050 - 0.012 cm/cm | 0.0050 - 0.012 in/in | |
Lehmann & Voss LUVOCOM® 1-0865 Polyamide 66, with aramid reinforcement, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Low warpage.Improved heat resistance.Control disks, cams, sliding elements and other duty parts.. |